Growth of carbon fiber production technologies (review)

Kolobkov A.S.
Kolobkov A.S. Growth of carbon fiber production technologies (review) // Proceedings of VIAM. 2022. No. 8. DOI: 10.18577/2307-6046-2022-0-8-123-131. URL: https://www.viam-works.ru/en/journal/2022/8/10
Keywords
carbon, carbon fiber, polyacrylonitrile, fiber molding, strength, technology development, carbon nanotubes, electroforming
Abstract

Currently, interest in carbon fibers and polymer composite materials based on them, which are promising materials, is quite high. The article discusses the emergence of carbon fiber technology and its development. Technologies for obtaining a precursor from polyacrylonitrile, from which carbon fibers are produced, are described. The main directions of their improvement are shown, as well as possible ways of developing carbon-based fibers and their main manufacturers.

Reference list
  1. Kablov E.N., Valueva M.I., I.V. Zelenina, Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials. Trudy VIAM, 2020, no. 1, paper no. 07. Available at: http://www.viam-works.ru (accessed: June 1, 2022). DOI: 10.18577/2307-6046-2020-0-1-68-77.
  2. Kablov E.N. Materials of a new generation and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  3. Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3,
  4. pp 97–105.
  5. Sorokin A.E., Ivanov M.S., Sagomonova V.A. Thermoplastic polymer composite materials based on polyetheretherketones of various manufacturers. Aviation materials and technologies, 2022, no. 1 (66), paper no. 04. Available at: http://www.journal.viam.ru (accessed: June 1, 2022). DOI: 10.18577/2071-9140-2022-0-1-41-50.
  6. Gunyaeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
  7. Sidorina A.I. Multiaxial carbon fabrics in the products of aviation technology (review). Aviation materials and technologies, 2021, no. 3 (64), paper no. 10. Available at: http://www.journal.viam.ru (accessed: June 1, 2022). DOI: 10.18577/2713-0193-2021-0-3-105-116.
  8. Kutsevich K.E., Dementeva L.A., Lukina N.F., Tyumeneva T.Yu. Adhesive prepregs as promising materials for parts and assemblies from polymeric composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 379–387. DOI: 10.18577/2071-9140-2017-0-S-379-387.
  9. Bacon R. Growth, structure, and properties of graphite whiskers. Zhurnal fizicheskoy khimii, 1960, p. 283–290.
  10. Radushkevich L.V., Lukyanovich V.M. On the structure of carbon formed during the thermal decomposition of carbon monoxide on an iron contact. Journal of Physical Chemistry, 1952, vol. 26, no. 1, pp. 88–95.
  11. Oberlin A., Endo M., Koyama T. Filamentous growth of carbon through benzene decomposition. Journal of crystal growth, 1976, vol. 1, no. 32 (3), p. 335.
  12. Kolobkov A.S. S-shaped curve of development of technology for the production of carbon fibers. Kompozitnyy mir, 2018, no. 3 (78), pp. 24–25.
  13. Gladunova I.O., Lysenko A.A. The market of polymer composite materials. Trends and prospects. Vestnik Sankt-Peterburgskogo gosudarstvennogo universiteta tekhnologii i dizajna. Ser. 1: Natural and technical sciences, 2021, no. 2, pp 96–100.
  14. Wang Y., Tong Y., Zhang B. et al. Formation of surface morphology in polyacrylonitrile (PAN) fibers during wet-spinning. Journal of Engineered Fibers and Fabrics, 2018, no. 13, pp. 52–55.
  15. Udakhe J. Melt Processing of Polyacrylonitrile (PAN) Polymers. Journal of the Textile Association, 2011, no. 71, pp. 233–241.
  16. Reneker D.H., Yarin A.L. Electrospinning jets and polymer nanofibers. Polymer, 2008, no. 13, pp. 425.
  17. Zussman E., Chen X., Ding W. et al. Mechanical and structural characterization of electrospun PAN-derived carbon nanofibers. Carbon, 2005, no. 43, pp. 2175–2185.
  18. Zhou Z., Lai C., Zhang L. Development of carbon nanofibers from aligned electrospun polyacrylonitrile nanofiber bundles and characterization of their microstructural, electrical, and mechanical properties. Polymer, 2009, no. 50, pp. 2999–3006.
  19. Arshad S.N., Naraghi M., Chasiotis I. Strong carbon nanofibers from electrospun Polyacrylonitrile. Carbon, 2011, vol. 1, no. 49 (5), pp. 1710–1719.
  20. Rogalski J.J., Bastiaansen C.W., Peijs T. Rotary jet spinning review – a potential high yield future for polymer nanofibers. Nanocomposites, 2017, vol. 2, no. 3 (4), pp. 97–121.
  21. Oberlin A., Endo M., Koyama T. Filamentous growth of carbon through benzene decomposition. Journal of crystal growth, 1976, vol. 1, no. 32 (3), pp. 335.
  22. Hayashi Y., Chiba Y., Inoue H. et al. A review of dry spun carbon nanotube yarns and their potential applications in energy and mechanical devices. Journal of Fiber Science and Technology, 2020, no. 76 (2), pp. 72–78.
  23. Zhang M., Atkinson K.R., Baughman R.H. Multifunctional carbon nanotube yarns by downsizing an ancient technology. Science, 2004, no. 306 (5700), pp. 1358–1361.