Specificity of the formation of fiberglass based on PMR-polyimides
Kolpachkov E.D., Kurnosov A.O., Papina S.N., Petrova A.P. Specificity of the formation of fiberglass based on PMR-polyimides // Proceedings of VIAM. 2022. No. 7. DOI: 10.18577/2307-6046-2022-0-7- 37-49. URL: https://www.viam-works.ru/en/journal/2022/7/4
Keywords
melt-type polyimide binders, PMR-polyimides, polymer composite materials (PCM), glass-reinforced plastics, high-temperature PCM
Abstract
This paper presents the technological features of the processing of glass-reinforced plastics based on PMR-type polyimide binders. The main approaches to the manufacture of polymer composite materials (PCM) samples based on glass fillers and polyimide melt binders are demonstrated, taking into account their physicochemical features. It was shown that PCM based on melt-type polyimide binders can be processed according to different modes, providing different levels of characteristics.
Reference list
- Aldoshin S.M., Badamshina E.R., Kablov E.N. Polymer nanocomposites – a new generation of polymer materials with improved performance. Reports of Sci.-Tech. Sections I Intern. Forum on Nanotechnology "Rosnanotech 08". Moscow, 2008, pp. 385–387.
- Kablov E.N., Semenova L.V., Petrova G.N., Larionov S.A., Perfilova D.N. Polymer composite materials on a thermoplastic matrix. Izvestiya vysshikh uchebnykh zavedeniy. Ser.: Chemistry and chemical technology, 2016, vol. 59, no. 10, pp. 61–71.
- Kablov E.N. The role of fundamental research in the creation of new generation materials. Reports of XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
- Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and
- implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
- Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review).
- Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
- Guohua S., Xin Z., Dezhen W., Lianlong H. Research Progress in High-performance Polyimide Composites. China Plastics, 2021, vol. 35 (9), pp. 147–155. DOI: 10.19491/j.issn.1001-9278.2021.09.022.
- Gouzman I., Grossman E., Verker R. et al. Advances in Polyimide-Based Materials for Space Applications. Advanced materials, 2019, vol. 31 (18), art. 05. Available at: http://onlinelibrary.wiley.com (accessed: March 28, 2022). DOI: 10.1002/adma.201807738.
- Fernberg P., Gong G., Mannberg P. Processing and properties of new polyimide composites withhigh temperature ability. ECCM16 – 16th European Conference on Composite Materials (Seville, June 22–26, 2014). Available at: http://www.escm.eu.org/eccm16/assets/0600.pdf (accessed: November 17, 2021).
- Yang S.-Y., Ji M. Polyimide matrices for carbon fiber composites. Advanced Polyimide Materials. Synthesis, Characterization and Applications. Elsevier 2018, pp. 93–136. DOI: 10.1016/B978-0-12-812640-0.00003-2.
- Boychuk A.S., Generalov A.S., Dikov I.A. FRP parts and structures testing by phased array technique. Aviacionnye materialy i tehnologii, 2017, no. 1 (46), pp. 45–50. DOI: 10.18577/2071-9140-2017-0-1-45-50.
- Kondrashov S.V., Shashkeev K.A., Petrova G.N., Mekalina I.V. Constructional polymer composites with functional properties. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 405–419. DOI: 10.18577/2071-9140-2017-0-S-405-419.
- Zhelezina G.F., Solovyeva N.A., Makrushin K.V., Rysin L.S. Polymer composite materials for manufacturing engine air particle separation of advanced helicopter engine. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 58–63. DOI: 10.18577/2071-9140-2018-0-1-58-63.
- Mikhailin Yu.A. Heat-resistant polymers and polymer materials based on them. Polimernye materialy, 2005, no. 8, pp. 23–26.
- Aleksandrov N.A., Malysheva G.V., Nelyub V.A. Investigation of fracture surfaces of carbon fiber plastics made using melt and mortar technologies. Vse materialy. Entsiklopedicheskiĭ spravochnik, 2011, no. 3, p. 7.
- Zharinov M.A., Shimkin A.A., Akhmadiyeva K.R., Zelenina I.V. Features and properties of solvent-free PMR-type polyimide resin. Trudy VIAM, 2018, no. 12 (72), paper no. 05. Available at: http://www.viam-works.ru (accessed: March 28, 2022). DOI: 10.18577/2307-6046-2018-0-12-46-53.