Determination of rare earth metals in aluminum alloys by atomic emission spectrometry with inductively coupled plasma
Karachevtsev F.N., Dvoretskov R.M., Nikolaev E.V. Determination of rare earth metals in aluminum alloys by atomic emission spectrometry with inductively coupled plasma // Proceedings of VIAM. 2022. No. 4. DOI: 10.18577/2307-6046-2022-0-4-96-107. URL: https://www.viam-works.ru/en/journal/2022/4/10
Keywords
measurement technique, aluminum alloys, atomic emission spectrometry, inductively coupled plasma, scandium, yttrium, cerium, lanthanum, neodymium, praseodymium
Abstract
A method is proposed for the determination of scandium, yttrium, cerium, lanthanum, neodymium, and praseodymium by inductively coupled plasma atomic emission spectrometry in aluminum alloys. Analytical REM lines free from significant spectral overlaps are selected. The selection of the sample preparation method was carried out, namely, dissolution in a mixture of hydrochloric and nitric acids. The accuracy indicator of the developed technique is not more than 4% rel. for the content of rare-earth metals from 0.05 to 6 wt. %, which fully ensures the control of the content of rare-earth metals in products made of aluminum alloys.
Reference list
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Aluminum alloys. History of aviation materials science. VIAM – 80 years: years and people. Ed. E.N. Kablov. Moscow: VIAM, 2012, pp. 143–156.
- Kablov E.N. Aerospace materials science. Vse materialy. Entsiklopedicheskiy spravochnik, 2008, no. 3, pp. 2–14.
- Korgin A.V., Romanets V.A., Ermakov V.A., Zeid Kilani L.Z. Perspectives and problems of using aluminum alloys in the construction of bridges in the Russian Federation // Vestnik BSTU im. V.G. Shukhova, 2018, no. 9, pp. 42–48.
- Kablov E.N., Ospennikova O.G., Vershkov A.V. Rare metals and rare-earth elements are materials for modern and future high technologies. Aviacionnye materialy i tehnologii, 2013, no. S2, pp. 3–10.
- Lukin V.I., Skupov A.A., Panteleev M.D., Ioda E.N. Influence of scandium additives on the weldability of aluminum alloys of the Al–Mg system // Svarka i diagnostika, 2016, no. 1, pp. 13–15.
- Ryabov D.K., Kolobnev N.I., Kochubej A.Ya., Zavodov A.V. Changing of mechanical properties of 1913 alloy sheets after scandium addition. Aviacionnye materialy i tehnologii, 2014, no. 4, pp. 3–8.
- Shchetinina N.D., Kuznetsova P.E., Dynin N.V., Selivanov A.A. Aluminum alloys with additions of Sc and Zr IN additive manufacturing (review). Aviation materials and technologies, 2021, no. 3 (64), paper no. 03. Available at: http://www.journal.viam.ru (accessed: December 27, 2021). DOI: 10.18577/2713-0193-2021-0-3-19-34.
- Antipov V.V. Strategy of development of titanium, magnesium, beryllium and aluminum alloys. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 157–167.
- Skupov A.A., Panteleev M.D., Ioda E.N., Movenko D.A. The efficiency of rare earth metals for filler materials alloying. Aviacionnye materialy i tehnologii, 2017, no. 3 (48), pp. 14–19. DOI: 10.18577/2071-9140-2017-0-3-14-19.
- Savitsky V.M., Terekhova V.F., Burov I.V. et al. Alloys of rare earth metals. Moscow: Publishing House of the Academy of Sciences of the USSR, 1962, 266 p.
- Savitsky V.M., Terekhova V.F., Markova I.A., Torchinov R.S. Rare earth metals, alloys and compounds. Moscow: Nauka, 1973, 356 p.
- Rokhlin L.L., Dobatkina T.V., Eskin D.G. et al. Physico-chemical studies of new aluminum and magnesium alloys. Institutu metallurgii i materialovedeniya im. A.A. Baykov 60 years old: collection. Ed. N.P. Lyakishev. Moscow: ELIS, 1998, pp. 235–242.
- Smirnov A.A., Budinovskij S.A., Matveev P.V., Chubarov D.A. The development of thermal barrier coatings for turbine blades of single-crystal nickel alloys VZhM4, VZhM5U. Trudy VIAM, 2016, no. 1 (37), paper no. 3. Available at: http://www.viam-works.ru (accessed: December 27, 2021). DOI: 10.18577/2307-6046-2016-0-1-17-24.
- State Standard 11739.25–90. Alloys aluminum casting and deformable. Scandium determination method. Moscow: Publishing house of standards, 1990, 7 p.
- State Standard 11739.22–90. Alloys aluminum casting and deformable. Method for the determination of rare earth elements and yttrium. Moscow: Publishing house of standards, 1990, 7 p.
- Ryabchikov D.I., Ryabukhin V.A. Analytical chemistry of rare earth elements and yttrium. Moscow: Nauka, 1966, 380 p.
- State Standard 7727–81. Aluminum alloys. Methods of spectral analysis. Moscow: Publishing house of standards, 2002, 26 p.
- Karpov Yu.A., Baranovskaya V.B. Analytical control is an integral part of material diagnostics. Zavodskaya laboratoriya. Diagnostika materialov, 2017, vol. 83, no. 1-I, pp. 5–12.
- Zagvozdkina T.N., Karachevtsev F.N., Dvoretskov R.M., Yakimova M.S. Determination of silicon content in aluminium alloys by ICP-AES method in combination with microwave pre-treatment. Trudy VIAM, 2014, no. 12, paper no. 10. Available at: http://www.viam-works.ru (accessed: December 27, 2021). DOI: 10.18577/2307-6046-2014-0-12-10-10.
- Karachevtsev F.N., Dvoretskov R.M., Zagvozdkina T.N., Slavin А.V. Determination of titanium and zirconium in aluminum alloys by atomic emission spectrometry with inductively coupled plasma. Trudy VIAM, 2021, no. 10 (104), paper no. 11. Available at: http://www.viam-works.ru (accessed: December 27, 2021). DOI: 10.18577/2307-6046-2021-0-10-108-116.
- Molchan N.V., Konkevich V.Yu., Fertikov V.I. Control of structural changes in aluminum alloy 1379p, obtained by granular technology, by atomic emission spectroscopy // Zavodskaya laboratoriya. Diagnostika materialov, 2017, vol. 83, no. 2, pp. 42–45.
- Karpov Yu.A., Baranovskaya V.B. Problems of standardization of methods of chemical analysis in metallurgy. Zavodskaya laboratoriya. Diagnostika materialov, 2019, vol. 85, no. 1–2, pp. 5–14.
- Karpov Yu.A. Analytical control of metallurgical production. Moscow: Metallurgy, 1995, pp. 97–107.
- Otto M. Modern methods of analytical chemistry: in 2 vols. Moscow: Technosfera, 2003, vol. 1, 416 p.
- Dvoretskov R.M., Uridia Z.P., Karachevtsev F.N., Zagvozdkina T.N. Determination of the chemical composition of magnesium alloys by the atomic emission spectrometry with inductively coupled plasma. Trudy VIAM, 2019, no. 12 (84), paper no. 10. Available at: http://www.viam-works.ru (accessed: December 27, 2021). DOI: 10.18577/2307-6046-2019-0-12-88-98.
- RMG 61-2010. State system for ensuring the uniformity of measurements. Indicators of accuracy, correctness, precision of methods of quantitative chemical analysis. Assessment methods. Moscow: Publishing house of standards, 2010, 41 p.