Determination of stickiness of prepregs on the basis of carbon fillers the sounding method

Mishkin S.I., Klimenko O.N., Kutsevich K.E.
Mishkin S.I., Klimenko O.N., Kutsevich K.E. Determination of stickiness of prepregs on the basis of carbon fillers the sounding method // Proceedings of VIAM. 2022. No. 3. DOI: 10.18577/2307-6046-2022-0-3-35-43. URL: https://www.viam-works.ru/en/journal/2022/3/4
Keywords
stickiness, polymer composite material, the modifier, adhesion, viability of prepreg, prepreg storage life, carbon prepreg, epoxy binder, the sounding method, automated laying
Abstract

Results of work on determination of stickiness of the carbon prepregs developed in Research Center Kurchatovsky institut – VIAM are given. The method and the equipment for determination of stickiness of prepregs is described. The comparative analysis of stickiness of prepregs on different epoxy binders and structures of carbon fillers is carried out. The interrelation between stickiness and short-term impact of temperature on technological properties of semi-finished products is shown. Stickiness of the prepregs used for manufacturing of aviation products, using the automated laying is investigated.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Materials of new generation and digital technologies of their processing. Vestnik Rossiyskoy akademii nauk. 2020, vol. 90, no. 4, pp. 331–334.
  3. Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  4. Kablov E.N. Marketing of materials science, aircraft building and industry: present and future. Direktor po marketingu i sbytu, 2017, no. 5–6, pp. 40–44.
  5. Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. Abstracts of the XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2016, pp. 25–26.
  6. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  7. Kinlok E. Adhesion and adhesives, science and technology. Moscow: Mir, 1991, 484 p.
  8. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021. no. 1 (62). paper no. 03. Available at: https://journal.viam.ru (accessed: February 19, 2021). DOI: 10.18577/2713-0193-2021-0-1-22-23.
  9. Duchk V., Pisanova E., Zhandarov S., Lauke B. Adhesion and adhesive strength in polymeric fibrous composites. Mekhanika kompozitnykh materialov, 1998, vol. 34, no. 5, pp. 431–446.
  10. Postnov V.I., Nikitin K.E., Petukhov V.I., Burkhan O.L., Orzaev V.G. Method and device for determining the stickiness of prepregs. Aviacionnye materialy i tehnologii, 2009, no. 3, pp. 29–33.
  11. Timoshkov P.N., Usacheva M.N., Khrulkov A.V. Stickiness and possibility of using prepregs for automated technologies (review). Trudy VIAM, 2018, no. 8 (68), paper no. 04. Availableat: http://www.viam-works.ru (accessed: November 15, 2021). DOI: 10.18577/2307-6046-2018-0-8-38-46.
  12. Banks R., Mouritz A.P., John S. et al. Development of a new structural prepreg: characterization of handling, drape and tack properties. Composite Structures, 2004, vol. 66, pp. 169–174. DOI: 10/1016.j.compstruct.2004.04.034.
  13. ASTM D2979-01. Standard Test Method for Pressure-Sensitive Tack of Adhesives Using an Inverted Probe Machine, 2001, pp. 1–3.
  14. ASTM D3167. Standard Test Method for Floating Roller Peel Resistance of Adhesives, 2017, pp. 1–6.
  15. Lizunov D.A. Development of high-strength carbon plastics based on epoxy-containing oligomers: thesis, Cand. Sc. (Chem.). Moscow: RKhTU im. D.I. Mendeleeva, 2014, 237 p.
  16. Bogdanova Yu.G. Adhesion and its role in ensuring the strength of polymer composites: textbook. Moscow: Lomonosov Moscow State University, 2010, 68 p.
  17. Orlov E.V., Gusev Yu.A., Khrulkov A.V., Korotkov I.A. Comparative analysis of stickiness determination methods of prepreg. Trudy VIAM, 2016, no. 7, paper no. 09. Available at: http://www.viam-works.ru (accessed: November 12, 2021). DOI: 10.18577/2307-6046-2016-0-7-9-9.
  18. Budelmann D., Detampel H., Schmidt C., Meiners D. Interaction of process parameters and material properties with regard to prepreg tack in automated lay-up and draping process. Composites. Part A: applied science and manufacturing, 2019, vol. 117, pp. 308–316.
  19. Kutsevich K.E., Tyumeneva T.Yu., Petrova A.P. Influence of fillers on properties of adhesive prepregs and PCM on their basis. Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 51–55. DOI: 10.18577/2071-9140-2017-0-4-51-55.
  20. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  21. Gunyayeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.