Features of electrolytic deposition of abrasive-wear-resistant nickel-based coatings

Salakhova R.K., Tihobrazov A.B., Farafonov D.P., Smirnova T.B.
Salakhova R.K., Tihobrazov A.B., Farafonov D.P., Smirnova T.B. Features of electrolytic deposition of abrasive-wear-resistant nickel-based coatings // Proceedings of VIAM. 2022. No. 2. DOI: 10.18577/2307-6046-2022-0-2-99-110. URL: https://www.viam-works.ru/en/journal/2022/2/8
Keywords
nickel plating, abrasive microparticles, zirconium dioxide, wear resistance, aluminizing, thermal cyclic resistance, penetration test
Abstract

An electrolytic method of deposition of composite abrasive-wear-resistant coatings based on nickel containing microparticles of zirconium dioxide with a dispersion of 120–200 microns in a metal matrix is proposed. A device for the application of a nickel abrasive-wear-resistant coating and a technological process diagram have been developed, which ensures uniform introduction of particles into the coating with the formation of the so-called «abrasive knife». The results of a metallographic study of the structure, micro-х-ray spectral analysis of a nickel matrix and tests of the coating for thermal cyclic resistance and penetration (abrasion of the sealing material) are presented.

Reference list
  1. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  2. Kablov E.N. Materials are the basis of any business. Delovaya Slava Rossii, 2013, no. 2, pp. 4–9.
  3. Kablov E.N., Muboyadzhyan S.A. Heat-shielding coatings for high-pressure turbine blades of advanced gas turbine engines. Metaly, 2012, no. 1, pp. 5–13.
  4. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  5. Bondarenko Yu.A. Trends in the development of high-temperature metal materials and technologies in the production of modern aircraft gas turbine engines. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 3–11. DOI: 10.18577/2071-9140-2019-0-2-3-11.
  6. Farafonov D.P., Migunov V.P., Sarayev A.A., Leshchev N.E. Abradability and erosion resistance of seals in turbine engine air-gas channel. Trudy VIAM, 2018, no. 8 (68), paper no. 7. Available at: http://www.viam-works.ru (accessed: November 10, 2021). DOI: 10.18577/2307-6046-2018-0-8-70-80.
  7. Ivakhnenko Yu.A., Baruzdin B.V., Varrik N.M., Maksimov V.G. High-temperature fibrous sealing materials. Aviacionnye materialy i tehnologii, 2017, No. S, pp. 272–289. DOI: 10.18577/2071-9140-2017-0-S-272-289.
  8. Farafonov D.P., Leshchev N.E., Afanasiev-Khody- kin A.N., Artemenko N.I. Abrasive wear-resistant seal materials of the gas turbine engine flow section. Aviacionnye materialy i tehnologii, 2019, No. 3 (56), pp. 67–74. DOI: 10.18577/2071-9140-2019-0-3-67-74.
  9. Balashova Yu.A., Grashchenkov D.V., Shavnev A.A., Babashov V.G. High-temperature heat-shielding ceramic and metal-ceramic composite materials for a new generation of aircraft. Vestnik kontserna VKO «Almaz-Antey», 2020, no. 2 (33). pp. 83–92.
  10. Barvinok V.A., Shitarev I.A., Bogdanovich V.I., Dokukina I.A. and others. Triggered, wear-resistant and heat-shielding coatings for parts of the gas path of the turbine, compressor and combustion chamber of the gas turbine engine. Vestnik Samarskogo gosudarstvennogo aerokosmicheskogo universiteta, 2009, no. 3 (19). pp. 11–28.
  11. Salakhova R.K., Semenychev V.V., Tyurikov E.V. Technological features of deposition of composite-cluster galvanic coatings based on nickel and chromium (III). Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk, 2013, vol. 15, no. 6, pp. 82–87.
  12. Salakhova R.K., Semenychev V.V., Tikhobrazov A.B. Study of galvanic composite coatings by metal-physical methods. Galvanotekhnika i obrabotka poverkhnosti, 2013, vol. 21, no. 3, pp. 45–49.
  13. Khaibieva V.Sh., Fomina G.G., Saifullin R.S. et al. Investigation of the influence of ZrO2 of various dispersions on the electrodeposition of nickel coatings and their properties. Vestnik tekhnologicheskogo universiteta, 2016, vol. 19, no. 9, pp. 129–131.
  14. Tseluykin V.N. Composite electrochemical coatings: obtaining, structure, properties. Fizikokhimiya poverkhnosti i zashchita materialov, 2009, vol. 45, no. 3, pp. 287–301.
  15. Tseluykin V.N., Yakovlev A.V. On electrochemical deposition and properties of nickel-based composite coatings. Fizikokhimiya poverkhnosti i zashchita materialov, 2020, vol. 56, no. 2, pp. 197–201.
  16. Gorohova E.O., Kulebyakin A.V., Lomonova E.E. Synthesis, structure and properties of zirconium dioxide crystals doped with Yb3+ ions. Uspekhi v khimii i khimicheskoy tekhnologii, 2016, vol. 30, no. 3, pp. 123–125.
  17. Kuznetsova L.I., Obukhova A.V., Bondarenko G.N., Fetisova O.Yu. Structural properties and state of the surface layer of zirconium dioxide modified with Me3+ cations. Zhurnal fizicheskoy khimii, 2018, vol. 92, no. 9, pp. 1470–1477.
  18. Devoino O.G., Okovity V.V. Plasma heat-shielding coatings based on zirconium dioxide with increased thermal stability. Nauka i tekhnika, 2015, no. 1, pp. 35–39.
  19. Abrasive ceramic matrix turbine blade tip and method for forming: pat. 5952110 US; filed 12.24.96; publ. 09.14.99.
  20. Gas-turbine engine sealing device (versions), gas-turbine engine blade and gas-turbine engine sharp edge: pat. 2229031RU; filed 11.24.98; publ. 05.20.04.
  21. Salakhova R.K., Tikhoobrazov A.B. Thermal resistance of electrolytic chromium coatings. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 60–67. DOI: 10.18577/2071-9140-2019-0-2-60-67.