Features of the development of technologies for the manufacture and removal of ceramic cores based on fused quartz for casting turbine blades from superalloys

Rassokhina L.I., Bityutskaya O.N., Gamazina M.V., Avdeev V.V.
Rassokhina L.I., Bityutskaya O.N., Gamazina M.V., Avdeev V.V. Features of the development of technologies for the manufacture and removal of ceramic cores based on fused quartz for casting turbine blades from superalloys // Proceedings of VIAM. 2022. No. 2. DOI: 10.18577/2307-6046-2022-0-2-3-12. URL: https://www.viam-works.ru/en/journal/2022/2/1
Keywords
ceramic cores, wax model with ceramic core, ceramic mold, casting of cooled turbine blade
Abstract

Technological parameters of removal of ceramic cores based on fused quartz from the inner cavity of turbine blade castings are selected and investigated. The results of studies of technological parameters of removal of ceramic cores based on fused quartz are presented, according to the results of which optimal technological parameters are selected and a technology for removing ceramic rods from fused quartz from the inner cavity of turbine blade castings is developed.

Reference list
  1. Cast blades of gas turbine engines: alloys, technologies, coatings. Ed. E.N. Kablov. 2nd ed. Moscow: Nauka, 2006, 632 p.
  2. Kablov E.N., Folomeikin Yu.I., Demonis I.M. Highly refractory ceramic molds and cores for casting cooled blades of gas turbine engines. Intern. scientific-practical conf. «Science and technology of silicate materials – present and future». St. Petersburg: Information of Education, 2003, vol. II. pp. 49–56.
  3. Belyakov A.V., Razumnova I.V., Demonis I.M., Folomeikin Yu.I. Easy-to-remove ceramic cores for investment casting of GTE blades. Steklo i keramika, 2012, no. 4, pp. 26–31.
  4. Landa M.I., Kopytov N.N. Influence of the grain composition of the powder composition on the properties of porous corundum ceramics of increased strength. Ogneupory, 1984, no. 4, pp. 21–25.
  5. Bakunov V.S., Balkevich V.L., Vlasov A.S. et al. Ceramics from high-refractory oxides. Moscow: Metallurgiya, 1977, 304 p.
  6. Strelov K.K. Structure and properties of refractories. Moscow: Metallurgy, 1982, 208 p.
  7. Folomeikin Yu.I. Formation of the structure of a porous highly refractory ceramic material with a granular structure. Steklo i keramika, 2015, no. 8, pp. 30–35.
  8. A mixture for the manufacture of foundry ceramic cores of hollow blades from heat-resistant alloys by investment casting: pat. 2691435 Rus. Federation; filed 23.07.18; publ. 13.06.19.
  9. Mixture for the manufacture of foundry ceramic rods: pat. 2273543 Rus. Federation; filed 01.09.04; publ. 10.04.06.
  10. Loshchinin Yu.V., Shorstov S.Yu., Kuzmina I.G. Research of influence of technology factors on thermal conductivity of ceramic casting molds. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 89–94. DOI: 10.18577 / 2071-9140-2019-0-2-89-94.
  11. Kablov E.N., Ospennikova O.G., Svetlov I.L. Highly efficient cooling of GTE hot section blades. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 3–14. DOI: 10.18577/2071-9140-2017-0-2-3-14.
  12. Zuev A.V., Loshchinin Yu.V., Barinov D.Ya., Marakhovskij P.S. Computational and experimental investigations of thermophysical properties. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 575–595. DOI: 10.18577/2071-9140-2017-0-S-575-595.
  13. Loshchinin Yu.V., Folomeikin Yu.I., Rykova T.P., Marakhovsky P.S., Pahomkin S.I. Thermophysical properties of ceramic materials of molds and rods for casting gas turbine engine blades from heat-resistant alloys. Materialovedenie, 2014, no. 3 (204). pp. 47–52.
  14. Ospennikova O.G., Rassokhina L.I., Bityutskaya O.N., Gamazina M.V. Optimization of technology for the manufacture of ceramic rods to improve the quality of cast blades of gas turbine engines. Novosti materialovedeniya. Nauka i tekhnologiya, 2017, no. 3–4, paper no. 04. Available at: http://www.materialsnews.ru (accessed: November 30, 2020).
  15. Ospennikova O.G., Rassohina L.I., Bitjuckaja O.N., Gamazina M.V. Development of technology for production of castings by the method of directional solidification of GTE blades made of alloys based on Nb–Si composite. Trudy VIAM, 2017, no. 4 (52), paper no. 01 Available at: http://www.viam-works.ru (accessed: November 30, 2020). DOI: 10.18577/2307-6046-2017-0-4-1-1.
  16. Rassokhina L.I., Bityutskaya O.N., Gamazina M.V., Avdeev V.V. Research of compositions of ceramic rods based on fused quartz and their manufacturing technology. Trudy VIAM, 2021, no. 1 (95), paper no. 04. Available at: http://www.viam-works.ru (accessed: December 11, 2021). DOI: 10.18577/2307-6046-2021-0-1-34-42.
  17. Folomeikin Yu.I., Kablov E.N., Demonis I.M. Highly refractory ceramics of rods and molds for casting blades with directional and single-crystal structures. Aviatsionnaya promyshlennost, 2000, no. 2, pp. 41–44.
  18. Method for removing ceramic material from casting parts: pat. 2557119 Rus. Federation; filed 12.03.14; publ. 20.07.15.
  19. Poklad V.A., Ospennikova O.G., Orlov M.R., Sudinin M.A. Technology for removal of ceramic rods from cooled blades of gas turbine engines. Aviatsionno-kosmicheskaya tekhnika i tekhnologiya, 2006, no. 9, pp. 24–30.
  20. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.