Mechanical properties of polymer composite materials based on knitted fillers with modified structure (review)

Ponomarenko L.A.
Ponomarenko L.A. Mechanical properties of polymer composite materials based on knitted fillers with modified structure (review) // Proceedings of VIAM. 2022. No. 12. DOI: 10.18577/2307-6046-2022-0-12-76-86. URL: https://www.viam-works.ru/en/journal/2022/12/7
Keywords
mechanical properties, cross-knitted, flat-knitted knitted filler for polymer composite material, non-knitted fibers, press and floating loops, eraser
Abstract

The mechanical properties of polymer composite materials (PCM) based on knitted fillers with a modified structure are considered. The specific features of the structure of fillers and the nature of their influence on the mechanical properties of the filler and PCM are described. Particular attention is paid to knitwear with additional non-knitted carbon fibers and the properties of PCM based on it. For such materials, the tensile strength is in the range from 767 to 1157 MPa, which is comparable to the values of this characteristic of carbon fiber reinforced plastics based on unidirectional fillers.

Reference list
  1. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  2. Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
  3. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  4. Kablov E.N., Kulagina G.S., Zhelezina G.F., Lonskii S.L., Kurshev E.V. Microstructure research of the unidirectional organoplastic based on Rusar-NT aramid fibers and epoxy-polysulfone binder. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 19–26. DOI: 10.18577/2071-9140-2020-0-4-19-26.
  5. Kurnosov A.O., Vavilova M.I., Melnikov D.A. Manufacturing technologies of glass fillers and study of effects of finishing material on physical and mechanical properties of fiberglass plastics. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 64–70. DOI: 10.18577/2071-9140-2018-0-1-64-70.
  6. Belinis P.G., Donetskiy K.I., Lukyanenko Yu.V., Rogozhnikov V.N., Mayer Yu., Bystrikova D.V. Volume reinforcing solid-woven preforms for manufacturing of polymer composite materials (review). Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 18–26. DOI: 10.18577/2071-9140-2019-0-4-18-26.
  7. Cuong N.K., Yamane H., Maekawa Z. Mechanical properties of knitted fabric reinforced polypropylene composites. Advanced Composite Materials, 2000, vol. 9, pp. 25–35. DOI: 10.1163/156855100300132947.
  8. Qi Y., Li J., Liu L. Tensile properties of multilayer-connected biaxial weft knitted fabric reinforced composites for carbon fibers. Materials & Design (1980–2015), 2014, vol. 54, pp. 678–685. DOI: 10.1016/j.matdes.2013.08.051.
  9. Li D.-S., Xia Y., Zhou Q. et al. Experimental study on the mechanical behavior and failure mechanism of 3d MWK carbon/epoxy composites under quasi-static loading. Polymer Composites, 2016, vol. 37, is. 12, pp. 3486–3498. DOI: 10.1002/pc.23548.
  10. Li D.-S., Zhao C., Jiang L., Jiang N. Experimental study on the bending properties and failure mechanism of 3D integrated woven spacer composites at room and cryogenic temperature. Composite Structures, 2014, vol. 111, pp. 56–65. DOI: 10.1016/j.compstruct.2013.12.026.
  11. Jiang D., Hu X., Lin Zh. et al. Mechanical properties and crystallization behaviors of oriented electrospun nanofibers of zein/poly(ε-caprolactone) composites. Polymer Composites, 2018, vol. 39, pp. 2151–2159. DOI: 10.1002/pc.24180.
  12. Leong K.H., Ramakrishna S., Huang Z.M., Bibo G.A. The potential of knitting for engineering composites – a review. Composites. Part A: Applied Science and Manufacturing, 2000, vol. 31, is. 3, pp. 197–220. DOI: 10.1016/S1359-835X(99)00067-6.
  13. Kim K.-Y., Curiskis J. I., Ye L., Fu Sh.-Y. Mode-I interlaminar fracture behaviour of weft-knitted fabric reinforced composites. Composites. Part A: Applied Science and Manufacturing, 2005, vol. 36, is. 7, pp. 954–964. DOI: 10.1016/j.compositesa.2004.12.004.
  14. Hasanalizadeh F., Dabiryan H., Sadighi M. Low-velocity impact behavior of weft-knitted spaсer fabrics reinforced composites based on energy absorption. 17th World Textile Conference (AUTEX 2018). IOP Conf. Series: Materials science and Engineering, 2017, vol. 254, art. 042014. DOI: 10.1088/1757-899X/254/4/042014.
  15. Ponomarenko L.A. About ways of structure modification of a knitted fillers for polymeric composite materials (review). Trudy VIAM, 2018, no. 3 (109), paper no. 09. Available at: http://www.viam-works.ru (accessed: June 02, 2022). DOI: 10.18577/2307-6046-2022-0-3-54-63.
  16. Dalidovich A.S. Fundamentals of the theory of knitting. Moscow: Light industry, 1970, 432 p.
  17. Truevtsev A.V., Tsobkallo E.S., Moskalyuk O.A. Quasi-continuous reinforcement of the composite with knitwear. Tekhnologiya legkoy promyshlennosti, 2016, no. 1, pp. 64–67.
  18. Balea L., Dusserre G., Bernhart G. Mechanical behaviour of plain-knit reinforced injected composites: effect of inlay yarns and fiber type. Composites. Part: B, 2014, no. 56, pp. 20–29. DOI: 10.1016/j/compositesb.2013.07.028.
  19. Dusserre G., Balea L., Bernhart G. Elastic properties prediction of a knitted composite with inlaid yarns subjected to stretching: A coupled semi-analytical model. Composites. Part A: Applied science and manufacturing, 2014, no. 64, pp. 185–193. DOI: 10.1016/j.compositesa.2014.05.007.
  20. De Araujo M., Fangueiro R., Hu H. Weft-knitted structures for Industrial applications. Advances in Knitting Technology, Woodhead Publishing Ltd, 2011, pp. 136–170. DOI: 10.1533/9780857090621.2.136.
  21. Zilio L., Dias M., Santos T. et al. Characterization and statistical analysis of the mechanical behavior of knitted structures used to reinforce composities: yarn compositions and float stitches. Journal of materials research and technology, 2020, no. 9 (4), pp. 8323–8336. DOI: 10.1016/j.jmrt.2020.05.089.
  22. Hu J.L., Jiang Y.M., Ko K.F. Modeling uniaxial tensile properties of multiaxial warp knitted fabric. Textile Research Journal, 1998, vol. 68, pp. 828–834. DOI: 10.1177/004051759806801107.
  23. Vuure A.W., Ko K.F., Beevers C. Net-shape knitting for complex composite performs. Textile Research Journal, 2003, vol. 73, pp. 1–10. DOI: 10.1177/004051750307300101.
  24. Pei X., Shang B., Chen L. et al. Compression properties of multilayer-connected biaxial weft knitted carbon fiber fabric reinforced composites. Composites. Part. B, 2016, vol. 91, pp. 296–305. DOI: 10/1016/j/compositesb.2015.12.041.
  25. Gunes K.S., Ince M.E., Icoglu H.I. Compressibility of weft knitted reinforcement fabrics from glass yarn. 18th World Textile Conference (AUTEX 2018). IOP Conf. Series: Materials Science and Engineering, 2018, no. 460, pp. 1–6. DOI: 10.1088/1757-899X/460/1/012029.
  26. Ishmael N., Fernando A. Textile tehnologies for the manufacture of three-dimensional textile preforms. Research Journal of Textile and Apparel, 2017, vol. 21, no. 4, pp. 342–362. DOI: 10.1108/RJTA-06-2017-0034.
  27. Bezsmertna V., Mazna O., Kohanyiy V. et al. Multifunctional polymer-based composite materials with weft-knitted carbon fibrous fillers. MATEC Web of Conferences, 2019, no. 304, art. 01012. DOI: 10.1051/matecconf/201930401012.
  28. Xue D., Hu H. Mechanical properties of biaxial weft-knitted flax composities. Materials and design, 2012, no. 46, pp. 264–269. DOI: 10.1016/j.matdes.2012.10.019.
  29. Demirkan O., Hamada Y., Kosui T., Nakai A. Effect of stitch yarn on tensile properties of biaxial weft knitted thermoplastic composites. ECCM 15th European Conference on Composite Materials, Venice, 2012, pp. 1–5.
  30. Molosnov K.A. Development of knitted fabrics for reinforcing composite materials: thesis, Cand. Sc. (Tech.). St. Petersburg, 2013, 17 p.
  31. Truevtsev A.V., Tsobkallo E.S., Moskalyuk O.A. Polymer composite materials with knitted filler. Modern trends in the development of chemistry and technology of polymeric materials: abstracts of the IV Intern. scientific conf. St. Petersburg, 2018, pp. 57–59.
  32. Bazanova E.A., Truevtsev A.V. On the possibility of using knitwear as a filler for composites. Molodye uchenye – razvitiyu natsional'noy tekhnologicheskoy initsiativy (POISK), 2020, no. 1, pp. 21–23.
  33. Composite Materials for Aircraft Structures. ALAA Education series. Ed. A. Baker, S. Dutton, D. Kelly. Second Edition. Blacksburg, 2004, 540 p.