Domestic thermoplastic carbon plastic based on polyetheretherketone

Ivanov M.S., Sagomonova V.A., Morozova V.S.
Ivanov M.S., Sagomonova V.A., Morozova V.S. Domestic thermoplastic carbon plastic based on polyetheretherketone // Proceedings of VIAM. 2022. No. 12. DOI: 10.18577/2307-6046-2022-0-12-49-62. URL: https://www.viam-works.ru/en/journal/2022/12/5
Keywords
polyetheretherketone, carbon fabric, thermoplastic composite material, thermoforming, carbon plastic, prepreg
Abstract

The analysis of information sources in area of thermoplastic composite materials on the basis of polyetheretherketone (PEEK) for aerospace application is carried out. Requirements are formulated and the main results on development of prepreg and thermoplastic carbon plastic the VKU-65 brands on the basis of domestic woven carbon filler and PEEK binding are provided. Processes of manufacturing of prepreg and thermoplastic carbon plastic are described, research of their main properties is conducted. The refining technology of thermoplastic carbon plastic is developed by thermoforming method.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Komarov G.A. The state, prospects and problems of the use of PKM in technology. Polimernye materialy, 2009, no. 2, pp. 5–9.
  3. Kerber M.L., Vinogradov V.M., Golovkin G.S. et al. Polymer composite materials: structure, properties, technology. St. Petersburg: Professiya, 2011, pp. 32–33.
  4. Petrova G.N., Bader E.Ya. Structural materials based on reinforced thermoplasts. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 30–40.
  5. Kraev I.D., Shuldeshov E.M., Platonov M.M., Yurkov G.Yu. Composite materials combining acoustic and radio shielding properties. Aviacionnye materialy i tehnologii, 2016, no. 4 (45), pp. 60–67. DOI: 10.18577/2071-9140-2016-0-4-60-67.
  6. Gunyaev G.M., Chursova L.V., Komarova O.A., Gunyaeva A.G. Constructional carbon the plastics modified by nanoparticles. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 277–286.
  7. Golovkin G.S. The regulation of the mechanical properties of PCM by the methods of targeted formation of the interference zone. Polimernye materialy, 2009, no. 11, pp. 26–28.
  8. Gunyaeva A.G., Veshkin E.A., Antyufeeva N.V., Panafidnikova A.N., Efimik V.A. Research of influence of the condensation moisture on carbon fiber plastic prepreg on the basis of solution epoxy binder and PСM on its basis. Trudy VIAM, 2019, no. 9 (81), paper no. 09. Available at: http://www.viam-works.ru (accessed: May 20, 2022). DOI: 10.18577/2307-6046-2019-0-9-80-88.
  9. Kirin B.S., Kuznetsova K.R., Petrova G.N., Sorokin A.E. Comparative analysis of properties of polyetheretherketones of domestic and foreign production. Trudy VIAM, 2018, no. 5 (65), paper no. 05. Available at: http://www.viam-works.ru (accessed: May 20, 2022). DOI: 10.18577/2307-6046-2018-0-5-34-43.
  10. Sorokin A.E., Bejder E.Ya., Izotova T.F., Nikolaev E.V., Shvedkova A.K. Investigation of carbon fiber reinforced plastic on polyphenylenesulfide resin after accelerated and natural climatic test. Aviacionnye materialy i tehnologii, 2016, no. 3 (42), pp. 66–72. DOI: 10.18577/2071-9140-2016-0-3-66-72.
  11. Petrova G.N., Larionov S.A., Sorokin A.E., Sapego Yu.A. Modern ways of processing of thermoplastics. Trudy VIAM, 2017, no. 11 (59), paper no. 07. Available at: http://www.viam-works.ru (accessed: May 20, 2022). DOI: 10.18577/2307-6046-2017-0-11-7-7.
  12. Timoshkov P.N., Usacheva M.N., Khrulkov A.V. Stickiness and possibility of using prepregs for automated technologies (review). Trudy VIAM, 2018, no. 8 (68), paper no. 04. Available at: http://www.viam-works.ru (accessed: May 20, 2022). DOI: 10.18577/2307-6046-2018-0-8-38-46.
  13. Mikhailin Yu.A. Thermal-resistant polymers and polymer materials based on them. St. Petersburg: Professiya, 2006, 346 p.
  14. Kablov E.N. Trends and guidelines of innovative development of Russia: collection scientific-inform. materials. 3rd ed. Moscow: VIAM, 2015, 720 p.
  15. Kablov E.N. What to make the future from? The materials of the new generation, the technology of their creation and processing are the basis of innovation. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  16. Nikolaev A.F. Heat-resistant polymers. Leningrad: Lensovet LTI, 1988, pp. 3–11.
  17. Golovkin G.S. Technological properties of thermoplastic binders for reinforced plastics. Plasticheskie massy, 2005, no. 1, pp. 35–40.
  18. Mazhirin P.Yu. Polyphenylene sulfide in aircraft industry. Polimernye materialy, 2003, no. 2, pp. 22–24.
  19. Li J. Effect of Silane Couning Agent on the Tensile Properties of Carbon Fiber-Reinforced Thermoplastic Polyimide. Composites. A: Polymer-Plastics Technology and Engineering, 2010, vol. 49, pp. 337–340.
  20. Trostyanskaya E.B., Stepanova M.I., Rosokhin G.I. Heat-resistant linear polymers. Rostov-on-Don: RGASKhM, 2002, pp. 3–22.
  21. Kablov E.N. Russia needs new generation materials. Redkiye zemli, 2014, no. 3, pp. 8–13.
  22. Buznik V.M., Kablov E.N. Arctic Materials Science: Current State and Prospects. Herald of the Russian Academy of Sciences, 2017, vol. 87, no. 5, pp. 397–408.
  23. Lazareva T.K., Ermakin S.N., Kostyagina V.A. Problems of creating composite materials based on structural thermoplasts. Uspekhi v khimii i khimicheskoy tekhnologii, 2010, vol. 24, no. 4, pp. 58–63.
  24. Kablov E.N. Airospace materials science. Vse materialy. Entsiklopedicheskiy spravochnik, 2008, no. 3, pp. 2–14.
  25. Jones Fr. A Review of Interphase Formation and Design in Fibre-Reinforced Composites. Journal of Adhesion Science and Technology, 2010, vol. 24, no. 1, pp. 171–202.
  26. Drzal Lt., Raghavedran Vk. Adhesion of Thermoplastic Matrices to Carbon Fibers: Effect of Polymer Molecular Weight and Fiber Surface Chemistry. Journal of Thermoplastic Composite Materials, 2003, vol. 16, pp. 21–30.
  27. Thostenson E.T., Chou T.-W. Aligned Multi-Walled Carbon Nanotube-Reinforced Composites: Processing and Mechanical Characterization. Journal of Physics. D: Applied Physics, 2002, vol. 35, pp. L77–L80.
  28. Chuang L., Chu N.-J. Effect of Polyamic Acids on Interface SHEAR Strength In Carbon Fiber/Aromatic Thermopoplastics. Journal of Applied Polymer Science, 1990, vol. 41, pp. 373–382.
  29. Datasheet Setex-1200. Available at: www.toraytac.com (accessed: May 05, 2022).
  30. Datasheet Tenax®-E TPCL Peek-HTA40. Available at: www.teijincarbon.com (accessed: May 05, 2022).
  31. Sorokin A.E., Ivanov M.S., Sagomonova V.A. Thermoplastic polymer composite materials based on polyetheretherketones of various manufacturers. Aviation materials and technologies, 2022, no. 1 (66), paper no. 04. Available at: http://www.journal.viam.ru (accessed: May 20, 2022). DOI: 10.18577/2071-9140-2022-0-1-41-50.
  32. Kirin B.S., Sorokin A.E., Boychuk A.S. Carbon fiber reinforced thermoplastic on the basis of polyetheretherketones. Trudy VIAM, 2020, no. 4–5 (88), paper no. 03. Available at: http://www.viam-works.ru (accessed: May 05, 2022). DOI: 10.18577/2307-6046-2020-0-45-22-31.
  33. A Kind of Method of Carbon Fiber Surface Modification: pat. CN108642882A, no. CN201810435940; filed 09.05.18; publ. 12.10.18.
  34. The method of manufacturing carbon fiber based on woven carbon filler and thermoplastic binding: pat. 2765042 Rus. Federation, no. 2020135999; filed 02.11.20; publ. 25.01.22.