Carbon fiber based on a volume-reinforcing braided preform for an element of a propeller blade

Donetskiy K.I., Karavaev R.Y., Bystrikova D.V., Gracheva A.D.
Donetskiy K.I., Karavaev R.Y., Bystrikova D.V., Gracheva A.D. Carbon fiber based on a volume-reinforcing braided preform for an element of a propeller blade // Proceedings of VIAM. 2022. No. 12. DOI: 10.18577/2307-6046-2022-0-12-27-38. URL: https://www.viam-works.ru/en/journal/2022/12/3
Keywords
propeller, polymer composite materials, carbon fiber, pressure impregnation, epoxy hot melt binder, woven preforms, physical properties, performance properties
Abstract

Currently, one of the global trends in the development of aircraft engines is the replacement of metal alloys with composite materials, which makes it possible to achieve a significant reduction in the weight of products and improve their performance. The use of modern methods of modeling the process of impregnation of carbon filler allows to reduce the development time of both the material itself and the product based on it. It is necessary to apply a multilevel approach when developing materials of a new generation – material modeling at nano-, micro-, meso- and macrolevels, behavior of elementary samples, structural elements and products.

Reference list
  1. Carey J.P. Handbook of Advances in Braided Composite Materials: Theory, Production, Testing and Applications. Elsiever Ltd, 2016, 479 p.
  2. Development of a family of propellers with light high-life blades made of polymer composite materials for new generation turboprop aircraft: a report on the work of PJSC NPP Aerosila. 2018. Available at: http://aviationunion.ru (accessed: June 20, 2022).
  3. Calvert T. Braided Fabrics for Aircraft Interiors Use Carbon Reinforced PPS Tapes. 2009. Available at: https://www.reinforcedplastics.com/content/other/braided-fabrics-for-aircraft-interiors-use-carbon-reinforced-pps-tapes (accessed: May 28, 2022).
  4. A&P Technology, Bombardier Wing Flap. 2014. Available at: http://www.braider.com/Case-Studies/Bombardier-Wing-Flap.aspx (accessed: June 24, 2022).
  5. Donetskiy K.I., Bystrikova D.V., Karavaev R.Yu., Timoshkov P.N. Application of polymeric composite materials for creation of elements of transmissions of aviation engineering (review). Trudy VIAM, 2020, no. 3 (87), paper no. 09. Available at: http://www.viam-works.ru (accessed: May 19, 2020). DOI: 10.18577/2307-6046-2020-0-3-82-93.
  6. Ivey M., Carey J.P., Ayranci C. Manufacturing and characterization of braidtruded fiber reinforced polymer rebar. Polymer Compositе, 2018, vol. 39, pp. 337–350.
  7. Hajihosseini A., Ayranci C., Carey J.P.R. Simulation of the rapid curing process for braid reinforced frp rebar in braidtrusion process using a finite element analysis. Internatioanal SAMPE Technical Conference. Seattle; Washington, 2014, pp. 2–5.
  8. Del Rosso S., Iannucci L., Curtis P. Experimental Investigation of the Mechanical Properties of Dry Microbraids and Microbraid Reinforced Polymer Composites. Composite Structure, 2015, vol. 44, pp. 505–519.
  9. Gnädinger F., Karcher M., Henning F. Holistic and Consistent Design Process for Hollow Structures Based on Braided Textiles and RTM. Applied Composite Materials, 2013, vol. 21, pp. 1–16.
  10. Sun Y., Yang Y.H., He J.L. Study on Manufacture Technology and Mechanical Properties of Three Dimensional Braided Composite Support with Irregular Shape. Advanced Material Research, 2011, vol. 194–196, pp. 1417–1420.
  11. Branscomb D., Beale D., Broughton R.M. New Directions in Braiding. Journal of Engineered Fibers and Fabric, 2013, vol. 8, pp. 11–24.
  12. Okano M., Sugimoto K., Nakai A., Hamada H. Bending Properties of Braided Composite Tubes. Australasian Conference on Composite Materials (ACCM 4), 2014, pp. 218–222.
  13. Pototsky M.V., Nebelov E.V., Tkachenko D.P., Kirpichnikov A.P. An approach to the study of propeller blades of a turboprop engine damaged by foreign objects. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2012, vol. 17, no. 12, pp. 167–169.
  14. Melenka G.W., Pastore C.M., Kj F.K. et al. Advances in 2-D and 3-D braided composite material modeling. Edmonton, 2016, pp. 321–363.
  15. Kablov E.N. New Generation Materials and Technologies for Their Digital Processing. Herald of the Russian Academy of Sciences, 2020, vol. 90, no. 2, pp. 225–228.
  16. Donetskiy K.I., Karavayev R.Yu., Raskutin A.Ye., Dun V.A. Carbon fibers composite material on the basis of volume reinforcing triax braiding preformes. Trudy VIAM, 2019, no. 1 (73), paper no. 07. Available at: http://viam-works.ru (accessed: May 19, 202022). DOI: 10.18577/2307-6046-2019-0-1-55-63.
  17. Melenka G.W., Carey J.P., Hut A., Cheung B. Advanced testing of braided composite materials. Edmonton, 2016, pp. 155–204.
  18. Composite propeller blade (options) and method for its manufacture (options): pat. 2013109705 Rus. Federation; filed 04.03.13; publ. 20.05.14.
  19. Aircraft propeller blade: pat 2012131274 Rus. Federation; filed 20.12.10; publ. 20.11.14.
  20. Kablov E.N. The role of fundamental research in the creation of new generation materials. Reports of XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
  21. Advancements in Braided Materials Technology. 2015. Available at: http://www.braider.com/Resources/Papers-Articles/Automated-Manufacturing.aspx (accessed: May 19, 2022).
  22. Samipour S.A., Khaliulin V.I., Batrakov V.V. Development of the Technology of Manufacturing Aerospace Composite Tubular Elements by Radial Braiding. Journal of Machinery Manufacture and Reliability, 2018, vol. 47, no. 3, pp. 284–289.
  23. Ivey M., Carey J.P., Ayranci C. Ply mechanics for braided composite materials. Edmonton, 2017, pp. 259–306.
  24. Xu L., Kim S.J., Ong Ch.-H. Prediction of material properties of biaxial and triaxial braided textile composites. Journal of Composite Materials, 2012, vol. 46, pp. 2255–2270.
  25. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composite materials: textbook. Ed. E.N. Kablov. Moscow: NRC "Kurchatov Institute" – VIAM, 2021, 528 p.
  26. Donetskiy K.I., Usacheva M.N., Khrulkov A.V. Infusion methods for the manufacture of polymer composite materials (review). Part 1. Trudy VIAM, 2022, no. 6 (112). paper no. 06. Available at: http://www.viam-works.ru (accessed: May 19, 2022). DOI: 10118577/2307-6046-2022-0-6-58-67.
  27. Goncharov V.A., Usacheva M.N., Khrulkov A.V. Features of the structure and reinforcement transmission shafts made of polymer composite materials (review). Trudy VIAM, 2021, no. 1 (95), paper no. 9. Available at: http://www.viam-works.ru (accessed: May 19, 2022). DOI: 10.18577/2307-6046-2021-0-1-85-96.