Peculiarities of the development and use of the electroforming method for nickel and its alloys (review)

Tolmachev Y.V., Kravchenko D.V., Kozlov I.A., Gerasimov M.V., Nikiforov A.A.
Tolmachev Y.V., Kravchenko D.V., Kozlov I.A., Gerasimov M.V., Nikiforov A.A. Peculiarities of the development and use of the electroforming method for nickel and its alloys (review) // Proceedings of VIAM. 2022. No. 11. DOI: 10.18577/2307-6046-2022-0-11-103-118. URL: https://www.viam-works.ru/en/journal/2022/11/10
Keywords
electroplating, mandrel, nickel plating, sulfamate electrolyte, internal stress
Abstract

The paper examines modern directions of development and features of the electroforming method in relation to nickel and its alloys. An overview of the electroforming method is presented, indicating reference sources, features of the method used and various materials. The compositions of electrolytes for nickel electroforming and the physical properties of the coatings obtained from them are presented. The peculiarities of the influence of various additives in electrolytes on the quality and consumer properties of products were considered. Different types of mandrels and materials for their production are described. Their comparison is carried out; the positive and negative aspects of different types of mandrels are considered. Considerable attention is paid to the consideration of the effect of internal stresses on the properties of materials obtained by electroforming.

Reference list
  1. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technological development of Russia in the context of achieving national goals: problems and solutions. Innovatsii, 2020, vol. 6 (260), pp. 3–16.
  2. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  3. Salakhova R.K., Tikhoobrazov A.B. Thermal resistance of electrolytic chromium coatings. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 60–67. DOI: 10.18577/2071-9140-2019-0-2-60-67.
  4. Zakirova L.I., Laptev A.B. Properties of protective electroplating coatings for replacement of cadmium on steel fixing parts (review). Part 1. Morphology and corrosion resistance. Aviaсionnye materialy i tehnologii, 2020, no. 3 (60), pp. 37–46. DOI: 10.18577/2071-9140-2020-0-3-37-46.
  5. Buznik V.M., Kablov E.N. Arctic materials science. Tomsk: Tomsk State University, 2018, vol. 3, 44 c.
  6. Khmeleva K.M., Kozlov I.A., Nikitin Ya.Yu., Nikiforov A.A. Modern trends of protective galvanic coatings working at high temperatures (review). Trudy VIAM, 2020, no. 12 (94), paper no. 07. Available at: http://www.viam-works.ru (accessed: June 03, 2022). DOI: 10.18577/2307-6046-2020-0-12-75-86.
  7. Salakhova R.K., Tikhoobrazov A.B., Farafonov D.P., Smirnova T.B. Features of electrolytic deposition of abrasive-wear-resistant nickel-based coatings. Trudy VIAM, 2022, no. 2 (108), paper no. 08. Available at: http://www.viam-works.ru (accessed: June 03, 2022). DOI: 10.18577/2307-6046-2022-0-2-99-110.
  8. Di Bari G.A. Electroforming: Electroplating Engineering Handbook. Ed. L.J. Durney. 4th ed. New York: Van Nostrand Reinhold, 1984, pp. 474–490.
  9. Huang C.H., Wu H.M., Hon Y.H. High-Strength Electroformed Nickel. Plating and Surface Finishing, 1990, vol. 77, pp. 56–59.
  10. Safranek W.H. The Properties of Electrodeposited Metals and Alloys. A Handbook. Journal of The Electrochemical Society, 1975, vol. 122 (8), p. 270C. DOI: 10.1149/1.2134416.
  11. Wearmouth W.R., Belt K.C. Electroforming with Heat-Resistant Sulfur-Hardened Nickel. Plating and Surface Finishing, 1979, vol. 10, pp. 53–57.
  12. Dini J.W., Johnson H.R., Brooks J.A. Zinc in Sulfamate Nickel Deposits – Influence on Weldability of Electroforms. Metal Finishing, 1979, vol. 77, no. 2, pp. 99–101.
  13. Brooks J.A., Dini J.W., Johnson H.R. Effects of Impurities on the Weldability of Electroformed Nickel. US Sandia Laboratories, 1978, p. 36.
  14. Dini J.W., Johnson H.R. Some Property Data for Nickel-Cobalt Electrodeposits. Journal of Materials Science, 1976, vol. 11, no. 9, pp. 1779–1780.
  15. Wearmouth W.R., Belt K.C. Mechanical Properties and Electroforming Applications of Nickel-Cobalt Electrodeposits. Transactions of the Institute of Metal Finishing, 1974, vol. 52, no. 3, pp. 114–118.
  16. Snaith D.W., Groves P.D. Some Further Studies of the Mechanism of Cermet Electrodeposition. Transactions of the Institute of Metal Finishing, 1977, vol. 55, no. 3, pp. 136–140.
  17. Sykes J.M., Allner D.J. Mechanisms for the Formation of Electrodeposited Composite Coatings. Transactions of the Institute of Metal Finishing, 1974, vol. 52, p. 28.
  18. Malone G.A. Electrodeposition of Dispersion Strengthened Alloys. Symposium on Electrodeposited Metals for Selected Applications, Battelle Memorial Laboratories, 1991, vol. 78, pp. 58–62.
  19. Harris S.J., Boden P.J. Electroforming with Composite Materials. Electroplating Metal Finishing, 1973, vol. 26, no. 5, pp. 9–13.
  20. Bazzard R., Boden P.J. Codeposition of Chromium Particles in a Nickel Matrix. Transactions of the Institute of Metal Finishing, 1972, vol. 50, no. 2, pp. 63–69.
  21. Harris S.J., Baker A.A., Hall A.F., Bache R.J. Electroforming Filament Winding Process – Method of Producing Metal Matrix Composites. Transactions of the Institute of Metal Finishing, 1971, vol. 49, no. 5, pp. 205–213.
  22. Cooper G. Forming Processes for Metal Matrix Composites. Composites, 1970, vol. 1, no. 3, pp. 153–159.
  23. Wallace W.A., Greco V.P. Electroforming High-Strength Continuous Fiber-Reinforced Composites. Plating, 1970, vol. 57, no. 4, pp. 342–348.
  24. Dean A.V. Further Developments in the Use of Cast and Sprayed Backings on Electroformed Molds and Dies. Metallurgia, 1978, vol. 45, no. 5, pp. 243–248.
  25. Wearmouth W.R. Application of New Developments in Electroforming Technology in the Toolmaking Industry. Interfinish 76 – Proceedings of the Ninth World Conference on Metal Finishing. Amsterdam, 1976, pp. 1–21.
  26. Watson S.A. Recent Developments in Nickel Electroforming and Backing of Mold Cavities. Het Ingenieursblad, 1976, vol. 45, no. 9, pp. 279–287.
  27. Dean A.V., Wearmouth W.R. New Backing Techniques for Electroformed Molds and Dies. Electroplating & Metal Finishing, 1975, vol. 28, no. 12, pp. 18–23.
  28. Bertucio E.C. Electroforming with Collapsible Mandrels. Metal Finishing, 1966, vol. 64, pp. 61–66.
  29. Marti J.L. The Effects of Some Variables upon Internal Stress of Nickel as Deposited from Sulfamate Electrolytes. Plating, 1966, vol. 53, no. 1, pp. 61–71.
  30. Dini J.W., Johnson H.R., Saxton H.J. Influence of Sulfur Content on the Impact Strength of Electroformed Nickel. Electrodeposition Surface Treatment, 1974, vol. 2, no. 3, pp. 165–176.
  31. Whitehurst M.L. Strength and Ductility of Electroformed Nickel. Symposium on Electrodeposited Metals for Selected Applications. Columbus, 1972, pp. 53–64.
  32. Notley J.M. Corner Weakness in Nickel Electroforms. Transactions of the Institute of Metal Finishing, 1972, vol. 50, no. 1, pp. 6–10.
  33. MacInnis R.D., Gow K.V. Tensile Strength and Hardness of Electrodeposited Nickel-Iron Alloy Foil. Plating, 1971, vol. 58, no. 2, pp. 135–136.
  34. Hammond R.A.F. Nickel Plating from Sulphamate Solutions. Part 3 – Structure and Properties of Deposits from Conventional Solutions. Metal Finishing Journal, 1970, vol. 16, no. 188, pp. 234–243.
  35. Sample C.H., Knapp B.B. Physical and Mechanical Properties of Electroformed Nickel at Elevated and Subzero Temperatures. Special Technical Publication, 1962, no. 318, pp. 32–43. DOI: 10.1520/STP46002S.
  36. Zentner V., Brenner A., Jennings C.W. Physical Properties of Electrodeposited Metals. Part I – Nickel. American Society for Testing and Materials, 1952, vol. 39, no. 8, pp. 865–927.
  37. McGeough J.A., Rasmussen H. Analysis of Electroforming with Direct Current. Journal of Mechanical Engineering Science, 1977, vol. 19, no. 4, pp. 163–166.
  38. Dalby S., Nickelsen J., Alting L. Metal Distribution in Electroplating. Electroplating Metal Finishing, 1975, vol. 28, no. 10, pp. 18–23.
  39. Watson S.A. The Throwing Power of Nickel and Other Plating Solutions. Transactions of the Institute of Metal Finishing, 1960, vol. 37, pp. 28.
  40. Edwards R. Electroforming for Holographic Reproduction. Plating and Surface Finishing, 1988, vol. 75, no. 3, pp. 30–31.
  41. Legierse P.E.J. Electroformed Molds for Optical Readout Disks. Plating and Surface Finishing, 1984, vol. 71, no. 12, pp. 20–25.
  42. Legierse P.E.J. New Developments for Mastering and Electroforming Optical Disks. Plating and Surface Finishing, 1990, vol. 77, no. 1, pp. 48–50.
  43. Schmidt F.J., Hess I.J. Properties of Electroformed Aluminum. Plating, 1966, vol. 55, no. 2, pp. 229–234.
  44. Senderoff S. Electrodeposition of Refractory Metals. Metallurgical Review, 1966, vol. 11, pp. 97–112.
  45. Silman H. Electrodeposition from Molten Salts. Finishing Industry, 1980, vol. 4, no. 4, pp. 8–90.