Production of spherical granules of a high-temperature metal composite material based on molybdenum

Bobrovkiy A.P., Efimochkin I.Yu., Bolshakova A.N., Khudnev A.A.
Bobrovkiy A.P., Efimochkin I.Yu., Bolshakova A.N., Khudnev A.A. Production of spherical granules of a high-temperature metal composite material based on molybdenum // Proceedings of VIAM. 2022. No. 1. DOI: 10.18577/2307-6046-2022-0-1-44-52. URL: https://www.viam-works.ru/en/journal/2022/1/5
Keywords
metal composite materials, mechanical alloying, powder metallurgy, spheroidization, agglomeration, additive technologies
Abstract

Discusses the process of obtaining spherical granules of a metal composite material based on molybdenum with an initial fraction of 40‒63 microns. The results obtained during the research showed the fundamental possibility of spheroidization of granules of high-temperature metal composite materials based on refractory metals reinforced with particles of ceramic compounds. However, the need for a more thorough study and selection of spheroidization modes to minimize the formation of satellites on granules during processing in an electric arc discharge plasma is revealed.

Reference list
  1. Kashin D.S., Dergacheva P.E., Stekhov P.A. Heat resistant slurry coatings (review). Trudy VIAM, 2018, no. 5 (65), paper no. 08. Available at: http://www.viam-works.ru (accessed: August 12, 2021). DOI: 10.18577/2307-6046-2018-0-5-64-75.
  2. Trofimenko N.N., Efimochkin I.Yu., Bolshakova A.N. Problems of creation and prospects for the use of heat-resistant high-entropy alloys. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 3–8. DOI: 10.18577/2071-9140-2018-0-2-3-8.
  3. Grashchenkov D.V., Efimochkin I.Yu., Bolshakova A.N. High-temperature metal-matrix composite materials reinforced with particles and fibers of refractory compounds. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 318–328. DOI: 10.18577/2071-9140-2017-0-S-318-328.
  4. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  5. Svetlov I.L. High-temperature Nb – Si-composites. Materialovedenie, 2010, no. 9, pp. 29–38.
  6. Svetlov I.L. High-temperature Nb – Si-composites (end). Materialovedenie, 2010, no. 10, pp. 18–27.
  7. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7-8, pp. 54–58.
  8. Kablov E.N. New generation materials – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  9. Bondarenko Yu.A. Trends in the development of high-temperature metal materials and technologies in the production of modern aircraft gas turbine engines. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 3–11. DOI: 10.18577/2071-9140-2019-0-2-3-11.
  10. Ershova I.O., Fedotenkova O.B. Powder composite materials based on molybdenum. Problemy chernoy metallurgii i materialovedeniya, 2015, no. 1, pp. 93–98.
  11. Titov D.D., Kargin Yu.F., Lysenkov A.C. et al. Influence of WSi2 content and magnesium aluminosilicate additives on oxidation and strength properties of MoSi2–WSi2 composites. Materialovedenie, 2012, no. 7, pp. 45–49.
  12. Klimkina A.A. Study of the structure and properties of molybdenum alloys obtained by the methods of additive technologies. XLVII Gagarin readings: collection of articles. Proceedings of Mezhdunar. youth scientific. conf. Moscow, 2021, p. 81.
  13. Dubinkin D.M., Ismailova Sh.Ya., Iskandarova E.I., Usachenko O.I. Current state, development paths, areas of application of selective laser sintering (SLS). Innovations in information technologies, mechanical engineering and motor transport: materials III Intern. scientific-practical conf. Kemerovo: Kuzbass state tech. un-t them T.F. Gorbachev, 2019, pp. 174–177.
  14. Zalessky V.G., Pobol I.L., Bakinovsky A.A., Gubko A.D. Obtaining metal products using electron-beam additive technologies. Izvestiya Natsionalnoy akademii nauk Belarusi, A series of physical and technical sciences, 2018, vol. 63, no. 2, pp. 169–180.
  15. Rodionov A.I., Efimochkin I.Yu., Samokhin A.V., Sinayskiy M.A. The influence of the spheroidization process on the fractional composition and morphology of alloy VKNA-4u in a particle-reinforced sheath Al2O3–Y2O3. Trudy VIAM, 2019, no. 11 (83), paper no. 02. Available at: http://www.viam-works.ru (accessed: August 12, 2021). DOI: 10.18577/2307-6046-2019-0-11-12-21.