Deformation treatment of hard-to-deform Ni–Ti–Nb and Ni–Ti–Nb–Zr shape memory alloys
Skugorev A.V., Kapitanenko D.V. Deformation treatment of hard-to-deform Ni–Ti–Nb and Ni–Ti–Nb–Zr shape memory alloys // Proceedings of VIAM. 2022. No. 1. DOI: 10.18577/2307-6046-2022-0-1-14-25. URL: https://www.viam-works.ru/en/journal/2022/1/2
Keywords
shape memory alloys, hot deformation, pressing, drawing, mechanical properties, thermomechanical couplings
Abstract
The work is devoted to the study of the processes of hot and cold plastic deformation of hard-to-deform shape memory alloys of the Ni–Ti–Nb and Ni–Ti–Nb–Zr systems. The optimal modes of deformation treatment of these alloys, which ensure the production of semi-finished products without surface defects, have been determined. Investigations of the mechanical properties of hot-deformed and cold-deformed semi-finished products from alloys of the Ni–Ti–Nb and Ni–Ti–Nb–Zr systems have been carried out. It is shown that the selected treatment modes of these alloys provide a high level of mechanical properties of materials.
Reference list
- Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing - the basis of innovation. Krylya Rodiny, 2016, no. 5, pp. 8–18.
- Kablov E.N. Marketing of materials science, aircraft construction and industry: present and future. Direktor po marketingu i sbytu, 2017, no. 5-6, pp. 40–44.
- Shcherbakov A.I., Mosolov A.N., Kalitsev V.A. Production of beryllium-containing steel 32Kh13N6K3M2BDLT-VI (VNS32-VI). Materialovedenie, 2017, no. 4, pp. 17–21.
- Denisova V.S., Malinina G.A., Vlasova O.V., Vinogradova A.Yu. The influence of silicon tetraboride additives on properties of heat-resistant coatings for nickel alloys protection. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 68–73. DOI: 10.18577/2071-9140-2019-0-2-68-73.
- Rosenenkova V.A., Solntsev S.S., Mironova N.A., Gavrilov S.V. Glass-ceramic composite protective technological coatings for thermomechanical processing of intermetallic alloys. Steklo i keramika, 2016, no. 10, pp. 32–36.
- Solntsev S.S., Denisova V.S. Reaction-hardened composite coatings and glass. Steklo i keramika, 2019, no. 4, pp. 9–14.
- Ponomarenko D.A., Letnikov M.N., Skugorev A.V., Sidorov S.A. The use of specialized isothermal presses for forging blanks of turbine disks from hard-to-deform heat-resistant alloys. Kuznechno-shtampovochnoye proizvodstvo. Obrabotka materialov davleniyem, 2018, no. 3, pp. 19–25.
- Bakradze M.M., Lomberg B.S., Sidorov S.A., Bubnov M.V. Method of large-sized deformed turbine discs manufacturing from EK151-ID industrial ingots with limited diameter (320 mm). Trudy VIAM, 2017, no. 6 (54), paper no. 02. Available at: http://www.viam-works.ru (accessed: August 18, 2021). DOI: 10.18577/2307-6046-2017-0-6-2-2.
- Moiseev N.V., Nekrasov B.R., Letnikova E.Yu., Vydumkina S.V. Stamping materials for high-temperature isothermal deformation in air. Kuznechno-shtampovochnoye proizvodstvo. Obrabotka materialov davleniyem, 2017, no. 7, pp. 25–30.
- Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G. The metallurgical fundamentals for high quality maintenance of single crystal heat-resistant nickel alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 55–71. DOI: 10.18577/2071-9140-2017-0-S-55-71.
- Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G., Rigin V.E. Resource-saving technologies for the smelting of promising casting and wrought superheat-resistant alloys taking into account the processing of all types of waste. Elektrometallurgiya, 2016, no. 9, pp. 30–41.
- Sidorov V.V., Min P.G., Kablov D.E. Desulfurization of monocrystalline heat-resistant nickel alloys during melting in vacuum. Metallurg, 2017, no. 5, pp. 57–62.
- Sidorov V.V., Kablov D.E., Min P.G., Vadeev V.E. Refining of complex alloyed nickel alloy ZhS32-VI from silicon and phosphorus impurities by means of unidirectional solidification of the melt at low speeds of movement of the crystallization front. Tekhnologiya metallov, 2016, no. 3, pp. 2–7.
- Shpagin A.S., Kucheryaev V.V., Bubnov M.V. Computer simulation of thermomechanical processing of heat-resistant nickel alloys VZh175 and EP742. Trudy VIAM, 2019, No. 8 (80), paper no. 04. Available at: http://www.viam-works.ru (accessed: August 18, 2021). DOI: 10.18577/2307-6046-2019-0-8-27-35.
- Bakradze M.M., Skugorev A.V., Kucheryayev V.V., Bubnov M.V. Computer modeling of technological metal forming processes as effective instrument for development of new technologies. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 175–185. DOI: 10.18577/2071-9140-2017-0-S-175-185.
- Gladkov Yu.A., Kanevsky S.S. Modeling of extrusion of aluminum profiles in the new version of the QForm Extrusion VX program: a joint deformation problem. Kuznechno-shtampovochnoye proizvodstvo. Obrabotka materialov davleniyem, 2016, no. 11, pp. 41–48.
- Borovkov D.V. Structure, martensitic transformations and functional properties of shape memory alloys based on Ti – Ni – Nb with wide martensitic hysteresis: thesis, Cand. tech. sciences. Moscow, 2006, 122 p.