Research of possibility of application of fireproof paste for increase of fire safety of designs from polymeric composite materials

Venediktova M.A., Evdokimov A.A., Krasnov L.L., Petrova A.P.
Venediktova M.A., Evdokimov A.A., Krasnov L.L., Petrova A.P. Research of possibility of application of fireproof paste for increase of fire safety of designs from polymeric composite materials // Proceedings of VIAM. 2021. No. 9. DOI: 10.18577/2307-6046-2021-0-9-67-75. URL: https://www.viam-works.ru/en/journal/2021/9/7
Keywords
fireproof paste, polymeric composite materials, fire safety, carbon fiber-reinforced plastic, glass fibre plastics, thermal protection.
Abstract

Possibility of increase of fire safety of VPS-58 glass fibre plastics and carbon fiber-reinforced plastic the VKU-51 brands by putting fireproof swelling-up fireproof paste of the VZO-9kh brand is investigated. Complex researches of physicomechanical, fire and heatphysical properties of fireproof paste of the VZO-9kh brand are conducted. By results of researches it is established that fireproof paste of the VZO-9kh brand corresponds to qualifying standards and can be applied to increase of fire safety of designs from polymeric composite materials.

Reference list
  1. Doriomedov M.S. Russian and world market of polymer composites (review). Trudy VIAM, 2020, no. 6–7 (89), paper no. 04. Available at: http://www.viam-works.ru (accessed: June 1, 2021). DOI: 10.18577/2307-6046-2020-67-29-37.
  2. Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  3. Vlasenko F.S., Raskutin A.E. Applying FRP in building structures. Trudy VIAM, 2013, no. 8, paper no. 03. Available at: http://viam-works.ru (accessed: February 1, 2021).
  4. Evdokimov A.A., Imametdinov E.Sh., Malakhovskiy S.S. Strengthening concrete building structure via reinforcement external system from carbon plastic. Trudy VIAM, 2020, no. 10 (92), paper no. 08. Available at: http://www.viam-works.ru (accessed: February 1, 2021). DOI: 10.18577/2307-6046-2020-0-10-73-80.
  5. Rachel J. Deploying Carbon-Fiber-Reinforced Polymer Composites in Precast, Prestressed Concrete Bridges. PCI Journal, 2012, vol. 57, is. 2, p. 41.
  6. Lightweight Fiber Reinforced Polymer Composite Modular Panel: pat. 6591567 US; filed 10.12.01; publ. 15.07.03.
  7. Mishkin S.I., Raskutin A.E., Evdokimov A.A., Gulyaev I.N. Technologies and the main stages of construction of the arch bridge first in Russia from composite materials. Trudy VIAM, 2017, no. 6 (54), paper no. 05. Available at: http://www.viam-works.ru (accessed: June 1, 2021). DOI: 10.18577/2307-6046-2017-0-6-5-5.
  8. Kachura S.M., Postnov V.I. Perspective optical fiber sensors and their application (review). Trudy VIAM, 2019, no. 5 (77), paper no. 06. Available at: http://www.viam-works.ru (accessed: February 1, 2021). DOI: 10.18577/2307-6046-2019-0-5-52-61.
  9. Kurlepov D.V. The impact of high fire temperatures on building structures. Inzhenerno-stroitelny zhurnal, 2009, no. 4, pp. 41–43.
  10. Romanenkov I.G., Levutes F.A. Fireproof building structures. Moscow: Stroyzdat, 1991, 320 p.
  11. Lord E.S. Ways to protect building structures from fire impact. Molodoy ucheny, 2015, no. 24 (104), pp. 160–163. Available at: https://moluch.ru/Archive/104/24562/ (accessed: July 06, 2021).
  12. Gabdulin R.Sh. Effective methods of fire protection construction structures. Bezopasnost, 2011, no. 1, pp. 48–49.
  13. Pavlyuk B.Ph. The main directions in the field of development of polymeric functional materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
  14. Eliseev O.A., Naumov I.S., Smirnov D.N., Bryk Ya.A. Rubbers, sealants, fireproof and heat-shielding materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 437–451. DOI: 10.18577/2071-9140-2017-0-S-437-451.
  15. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  16. Kablov E.N. The role of chemistry in the creation of materials of a new generation for complex technical systems. XX Mendeleev Congress in general and applied chemistry. Ekaterinburg: URO RAS, 2016, pp. 25–26.
  17. Kablov E.N. Sixth technological way. Nauka i zhizn, 2010, no. 4, pp. 2–7.
  18. Krasnov L.L., Kirina Z.V. Materials that ensure the reliability of the structural elements in the conditions of fire. Vse materialy. Entsiklopedicheskiy spravochnik, 2012, no. 10, pp. 48–52.
  19. Pavlovich A.V., Vladovenkov V.V., Izyumsky V.N., Kilchitskaya S.L. Fire retardant sweeping coatings. Lakokrasochnaya promyshlennost, 2012, no. 5, pp. 22–27.
  20. Polymeric materials of reduced flammability: materials IV International. conf. Volgograd, 2000. 196 p.
  21. Nefedov N.I., Semenova L.V., Kuznecova V.A., Vereninova N.P. Paint coatings for protection of metallic and polymer composite materials against aging, corrosion and biodeterioration. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 393–404. DOI: 10.18577/2071-9140-2017-0-S-393-404.
  22. Kraschinnikova M.V. Fire-proofing materials based on organic-soluble film consumers. Lakokrasochnye materialy, 2006, no. 12, pp. 14–16.
  23. Barbotko S.L. Development of the fire safety test methods for aviation materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 516–526. DOI: 10.18577/2071-9140-2017-0-S-516-526.
  24. The norms of the airworthiness of the aircraft of the transport category: aviation regulations 25. 3rd ed. Moscow: Aviaisdat, 2009, 267 p.
  25. Barbotko S.L., Volny O.S., Kiriyenko O.A., Shurkova E.N. Evaluation of fire safety of polymeric materials of aviation destination: analysis of the state, methods of testing, development prospects, methodical features. Ed. E.N. Kablov. Moscow: VIAM, 2018, 424 p.