Features of the magnetic state in amorphous RE–TM and RE–TM–B magnets (review)

Morgunov R.B., Korolev D.V., Valeev R.A., Piskorsky V.P.
Morgunov R.B., Korolev D.V., Valeev R.A., Piskorsky V.P. Features of the magnetic state in amorphous RE–TM and RE–TM–B magnets (review) // Proceedings of VIAM. 2021. No. 9. DOI: 10.18577/2307-6046-2021-0-9-43-58. URL: https://www.viam-works.ru/en/journal/2021/9/5
Keywords
magnetism, magnetic anisotropy, amorphous magnets, spin-reorientation transition.
Abstract

Provides an overview of the magnetism features of amorphous magnets of the RE–TM and RE–TM–B alloys (RE – rare earth metal, TM – transition metal, B – boron). Magnetic states in amorphous alloys, the effect of the single-ionic anisotropy of heavy rare-earth metals on local disorder and spin frustrations in an amorphous body, and some spin-reorientation transitions observed in such compounds are presented. It is shown that the identification of the spin-glass state can be achieved by detecting specific features on the field and temperature dependences of the magnetic moment and magnetic susceptibility of the sample.

Reference list
  1. Moorjani K., Coey J.M.D. Magnetic Glasses. Amsterdam: Elsevier, 1984. 536 p.
  2. O’Handley R.C. Physics of ferromagnetic amorphous alloys. Journal of Applied Physics, 1987, vol. 62. DOI: 10.1063/1.339065.
  3. Andreenko A.S., Nikitin S.A. Magnetic properties of amorphous alloys of rare earth metals with transition 3D metals. Uspekhi fizicheskikh nauk, 1997, vol. 167, pp. 606–622.
  4. Rao K.V. Spin-Glass-Ferromagnetic «Phase» Transitions in Amorphous Soft Magnetic Systems. Physica Scripta, 1982, vol. 25, no. 6A, p. 742.
  5. Imry Y., Ma Sh.-K. Random-Field Instability of the Ordered State of Continuous Symmetry. Physical Review Letter, 1975, vol. 35, p. 1399.
  6. Chudnovsky E.M., Saslow W.M., Serota R.A. Ordering in ferromagnets with random anisotropy. Physical Review B, 1986, vol. 33, p. 251.
  7. Filippi J., Amaral V.S., Barbara B. High-field magnetization curve of random-anisotropy amorphous magnets: Observation of a crossover and link to structural short-range order. Physical Review B, 1991, vol. 44, p. 2842.
  8. Barbara B., Dieny B., Filippi J. Rotational and transverse dynamics of some random anisotropy magnets. Journal of Applied Physics, 1990, vol. 67. DOI: 10.1063/1.345958.
  9. Sellmyer D.J., O’Shea M.J. Random anisotropy, exchange fluctuations and phase transitions in rare earth glasses. Journal of the Less-Common Metals, 1983, vol. 94, pp. 59–68.
  10. Sellmyer D.J., Nafis S. Phase transition in the random anisotropy system: α-DyFeB. Journal of Magnetism and Magnetic Materials, 1986, vol. 54–57, pp. 1173–1176.
  11. Zolotukhin I.V., Kalinin Yu.E. Amorphous metal alloys. Uspekhi fizicheskikh nauk, 1990, vol. 160, pp. 75–110.
  12. Handrich K. A Simple Model for Amorphous and Liquid Ferromagnets. Physica Status Solidi B. 1969, vol. 32, art. k55. DOI: 10.1002/pssb.19690320166.
  13. Koplak O.V., Kunitsyna E.I., Valeev R.A., Korolev D.V., Piskorskii V.P., Morgunov R.B. Ferromagnetic microwires α-Fe/(PrDy)(FeCo)B for micromanipulators and polymer composites. Trudy VIAM, 2019, no. 11 (83), paper no. 7. Available at: http://www.viam-works.ru (accessed: May 8, 2021). DOI: 10.18577/2307-6046-2019-0-11-60-67.
  14. Morgunov R.B., Koplak O.V., Talantsev A.D., Korolev D.V., Piskorskij V.P., Valeev R.A. The phenomenology of the magnetic hysteresis loops in multilayer microwires α-Fe/DyPrFeCoB. Trudy VIAM, 2019, no. 7 (79), paper no. 08. Available at: http://www.viam-works.ru (accessed: May 8, 2021). DOI: 10.18577/2307-6046-2019-0-7-67-75.
  15. Messmer R. Local electronic structure of amorphous metal alloys using cluster models. Evidence for specific metalloid-metal interactions. Physical Review B, 1981, vol. 23, pp. 1616.
  16. Korenblit E.Ya., Shender E.F. Spin glasses. Izvestiya vuzov, ser.: Physics, 1984, no. 10, pp. 23–45.
  17. Rezchikova I.I., Moiseeva N.S., Korolev D.V., Morgunov R.B., Piskorskii V.P. Spontaneous magnetization loss dynamics of (Pr, Dy)–(Fe, Co)–B magnets. Technical Physics. The Russian Journal of Applied Physics, 2020, vol. 65, no. 3, pp. 377–381.
  18. Koplak O.V., Kunitsyna E.I., Valeev R.A., Korolev D.V., Piskorskii V.P., Morgunov R.B. Ferromagnetic microwires α-Fe/(PrDy)(FeCo)B for micromanipulators and polymer composites. Trudy VIAM, 2019, no. 11 (83), paper no. 7. Available at: http://www.viam-works.ru (accessed: April 12, 2021). DOI: 10.18577/2307-6046-2019-0-11-60-67.
  19. Morgunov R.B., Piskorskiy V.P., Valeev R.A., Korolev D.V. The thermal stability of rare-earth magnets supported by means of the magnetocaloric effect. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 88–94. DOI: 10.18577/2071-9140-2019-0-1-88-94.
  20. Kablov E.N., Piskorsky V.P., Valeev R.A., Melnikov S.A., Buzenkov A.V. Comparison of the effect of additives based on REM intermetallics on the properties of sintered magnets from the base alloy Nd – Fe – Ti – Cu – B. Metaliy, 2015, no. 1, pp. 73–75.
  21. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  22. Nikitin S.A., Zolotukhin I.V., Solovev A.S. et al. Observation of giant magnetostriction in amorphous terbiumcobalt alloys. Fizika Tverdogo Tela, 1987, vol. 29, is. 5, pp. 1526–1529.
  23. Sayko G.V., Utochkin S.N., Zvezdin A.K. Spin-reorientation phase transitions in thin films of RE–TM amorphous alloys. Journal of Magnetism and Magnetic Materials, 1992, no. 113, pp. 194–200.
  24. De Almeidai J.R.L., Thoules D.J. Stability of the Sherrington-Kirkpatrick solution of a spin glass model. Journal Physical A, 1987, vol. 11, no. 5, pp. 983–990.
  25. Sherrington D., Kirpatrick S. Solvable Model of a Spin-Glass. Physical Review Letter, 1975, vol. 35, p. 1792.
  26. Dieny B., Barbara B. Critical Properties of a Random-Anisotropy System. Physical Review Letter, 1986, vol. 57, p. 1169.
  27. Saito Т., Matsumaru Y., Shinagawa K., Tsushima T. Critical behavior of transverse and longitudinal ac susceptibilities in a random anisotropy magnet α-Dy16Fe84. Journal of Magnetism and Magnetic Materials, 1994, vol. 130, p. 347.
  28. Chudnovsky E.M., Saslow W.M., Serota R.A. Ordering in ferromagnets with random anisotropy. Physical Review B, 1986, vol. 33, pp. 251–261. DOI: 10.1103/physrevb.33.251.
  29. Saito T., Miyano H., Shinagawa K., Tsushima T. Effect of coherent anisotropy on the H-T phase diagram of random anisotropy magnets of amorphous DyGdFe. Journal of Magnetism and Magnetic Materials, 1995, vol. 140, pp. 1757.
  30. Dieny B., Barbara B., Fillion G. et al. Hysteresis loop and torque experiments on a random anisotropy system. Journal of Physique, 1987, vol. 48, pp. 1741.
  31. Katori H.A., Ito A. Experimental Study of the de Almeida-Thouless Line by Using Typical Ising Spin-Glass FexMn1-xTiO3 with x = 0.41, 0.50, 0.55, and 0.57. Journal Physical Society Japan, 1994, vol. 63, pp. 3122–3128.
  32. Imai K., Masago E., Saito T. et al. Crossover from Heisenberg to Ising spin-glass-like magnetic properties in random anisotropy magnets amorphous Dy16MxFe84(1–x) (M = Cu, A1, Cu, and Al). Journal of Magnetism and Magnetic Materials, 1998, vol. 99, pp. 177–181.
  33. Singh R.R.P., Young A.P. De Almeida–Thouless instability in short-range Ising spin glasses. Physical Review E, 2017, vol. 96, pp. 012127.