Uncertainty of the measurements results of the chemical composition and its methods assessment
Karachevtsev F.N., Letov A.F., Slavin A.V. Uncertainty of the measurements results of the chemical composition and its methods assessment // Proceedings of VIAM. 2021. No. 8. DOI: 10.18577/2307-6046-2021-0-8-84-91. URL: https://www.viam-works.ru/en/journal/2021/8/10
Keywords
metrology, uncertainty, error, reproducibility, repeatability, standard uncertainty, expanded uncertainty.
Abstract
An explanation of the difference between the uncertainty and the error of the measurement results, which is in the approach to their assessment, is given. The standard and expanded uncertainty are estimated taking into account the uncertainty at each operation to transfer the size of a physical quantity from a standard (standard sample) to a measuring instrument and during measurements. The error is estimated based on the variance of the final measurement. Methods for evaluating the uncertainty of measurement results are given depending on regulatory documents, metrological characteristics, measurement methods, such as indicators and limits of repeatability and reproducibility.
Reference list
- Dvorkin V.I., Boldyrev I.V. The concept of uncertainty and its use in laboratory practice. Factory laboratory. Zavodskaya laboratoriya. Diagnostika materialov, 2006, vol. 72, no. 4, pp. 55–61.
- Kuznetsov V.P. Comparative analysis of measurement error and uncertainty. Izmeritelnaya tekhnika, 2003, no. 8, pp. 21–27.
- State Standard R ISO 5725-1–2002. Accuracy (correctness and precision) of measurement methods and results. Basic provisions and definitions. Moscow: Publishing house of standards, 2002, 32 p.
- State Standard ISO/IEC 17025–2019. Interstate standard. General requirements for the competence of testing and calibration laboratories. Moscow: Standartinform, 2019. 26 p.
- Recommendations for Interstate Standardization 43-2001. Application of the "Guide to the Expression of Uncertainty in Measurement". Moscow: Publishing house of standards, 2003. 24 p.
- Metrology guidelines 50.2.038–2004. Direct single measurements. Estimation of errors and uncertainty of the measurement result. Moscow: Standartinform, 2005, 7 p.
- Kablov E.N., Chabina E.B., Morozov G.A., Muravskaya N.P. Conformity assessment of new materials using high-level CRM and MI. Kompetentnost, 2017, no. 2, pp. 40–46.
- Lutsenko A.N., Perov N.S., Chabina E.B. The new stages of development of Testing Center. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 460–468. DOI: 10.18577/2071-9140-2017-0-S-460-468.
- Karpov Yu.A., Baranovskaya V.B. Analytical control is an integral part of materials diagnostics. Zavodskaya laboratoriya. Diagnostika materialov, 2017, vol. 83, no. 1-I, pp. 5–12.
- Bazyleva O.A., Ospennikova O.G., Arginbaeva E.G., Letnikova E.Yu., Shestakov A.V. Development trends of nickel-based intermetallic alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 104–115. DOI: 10.18577/2071-9140-2017-0-S-104-115.
- Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G. The metallurgical fundamentals for high quality maintenance of single crystal heat-resistant nickel alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 55–71. DOI: 10.18577/2071-9140-2017-0-S-55-71.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- State Standard 8.563–2009. Measurement techniques (methods). Moscow: Publishing house of standards, 2009, 32 p.
- Dvoretskov R.M., Baranovskaya V.B., Karachevtsev F.N., Letov A.F. Determination of rare earth metals in magnesium alloys by inductively coupled plasma atomic emission spectrometry. Izmeritelnaya tekhnika, 2019, no. 4, pp. 62–66.
- Dvoretskov R.M., Petrov PS, Orlov G.V., Karachevtsev F.N., Letov A.F. Standard samples of new grades of heat-resistant nickel alloys and their application for spectral analysis. Zavodskaya laboratoriya. Diagnostika materialov, 2018, vol. 84, no. 11, pp. 15–22.
- Alekseev A.V., Yakimovich P.V., Kvachenok I.K. Determination of impurities in nickel by ICP-MS. Trudy VIAM, 2020, no. 2 (86), paper no. 11. Available at: http://www.viam-works.ru (accessed: June 21, 2021). DOI: 10.18577/2307-6046-2020-0-2-101-108.
- State Standard 7728–79. Magnesium alloys. Spectral analysis methods. Moscow: Publishing house of standards, 1998, 12 p.