Influence of structure of polymeric matrix on structure and property priming coverings
Kuznetsova V.A., Zheleznyak V.G., Lonskii S.L., Kovrizhkina N.A., Silaeva A.A. Influence of structure of polymeric matrix on structure and property priming coverings // Proceedings of VIAM. 2021. No. 8. DOI: 10.18577/2307-6046-2021-0-8-50-58. URL: https://www.viam-works.ru/en/journal/2021/8/6
Keywords
primer coatings, adhesion, tensile strength, impact strength, water absorption, scanning electron microscopy, phase structure.
Abstract
Adhesion, physicomechanical properties, and also kinetics of water absorption of priming coatings on basis the E-41 epoxy resin modified by liquid Thiokol 1 and by Laproxide AF, and also their phase structure are investigated. As hardeners of primer compositions organic silicon ammine ASOT-2 and low-molecular polyamide PO-200 has been used. It is shown that use of the reactive modifier Laproxide AF and hardener ASOT-2 in the epoxy and thiokol film-formers allows to receive priming coating with uniform finely divided phase structure with low porosity and high water resistance.
Reference list
- Kablov E.N. Aviation materials science: results and prospects. Izvestiya Rossijskoy akademii nauk, 2002, vol. 72, no. 1, pp.3–12.
- Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. Reports of the XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2016, pp.25–26.
- Zhitomirskiy G.I. Aircraft design. Moscow: Mashinostroenie, 1991, 400 p.
- Lutsenko A.N., Slavin A.V., Erasov V.S., Khvackij K.K. Strength tests and researches of aviation materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 527–546. DOI: 10.18577/2071-9140-2017-0-S-527-546.
- Kablov E.N., Startsev O.V., Medvedev I.M. Review of international experience on corrosion and corrosion protection. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
- Kozlova A.A., Kuznetsova V.A., Kozlov I.A., Naprienko S.A., Silaeva A.A. The effect of prolonged heating on the properties of protective coatings for aluminum alloy system Al–Si–Mg. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 74–80. DOI: 10.18577/2071-9140-2019-0-2-74-80.
- Fomina M.A., Karimova S.A. Analysis of the corrosion state of materials of the airframe of aircraft of the "Su" type after long-term operation. Corrosion: materials, protection. 2014, no. 9, pp.20–24.
- Pavlyuk B.Ph. The main directions in the field of development of polymeric functional materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
- Zheleznyak V.G. Modern paint and varnish materials for use in aviation equipment products. Trudy VIAM, 2019, no. 5 (77), paper no. 07. Available at: http://www.viam-works.ru. (accessed: January 18, 2021). DOI: 10.18577/2307-6046-2019-0-5-62-67.
- Kondrashov E.K., Kuznetsova V.A., Semenova L.V., Lebedeva T.A., Malova N.Ye. Development of aviation paints and varnishes. Vse materialy. Entsyklopedicheskiy spravochnik, 2012, no. 5, pp. 49–54.
- Kuznecova V.A., Kuznecov G.V. Development trends in the field of fuel resistant paintwork coatings for protection of integral fuel tanks of aircrafts (review). Trudy VIAM, 2014, no. 11, paper no. 08. Available at: http://www.viam works.ru (accessed: January 25, 2021). DOI: 10.18577/2307-6046-2014-0-11-8-8.
- Drinberg A.S., Itsko E.F., Kalinskaya T.V. Anti-corrosion primers. Saint Petersburg, 2006, 168 p.
- Kuznetsova V.A., Deev I.S., Zheleznyak V.G., Silaeva A.A. Anti wear coating with quasicrystal filler. Trudy VIAM, 2018, no. 3 (63), paper no. 08. Available at: http://www.viam-works.ru (accessed: January 25, 2021). DOI: 10.18577/2307-6046-2018-0-3-68-76.
- Kurbatov V.G., Ilyin A.A., Indeikin E.A. Anticorrosive pigments and fillers with a polyaniline sheath. Lakokrasochnye materialy i ikh primenenie, 2012, no. 11, pp. 49–52.
- Kurbatov V.G., Kochkina N.V., Indeikin E.A. The use of shell pigments in the composition of polymeric anticorrosive materials. Uspekhi v khimii i khimicheskoy tekhnologii, 2014, vol. XXVIII, no. 3, pp. 92–96.
- Problems of protective coatings (review). Lakokrasochnye materialy i ikh primenenie, 2013, no. 9, pp. 33–35.
- Rosenfeld I.L., Rutinstein F.I., Zhigalova K.A. Protection of metals from corrosion by paint and varnish coatings. Moscow: Khimiya, 1987. 224 p.
- Sosnina S.A., Kuleshova I.D. Regulation of the interaction of components in filled paint and varnish compositions. Lakokrasochnye materialy i ikh primenenie, 2011, no. 1, pp. 60–62.
- Korobschikova T.S., Orlova N.A. Modeling of mechanical properties of paint and varnish material filled with wollastonite. Lakokrasochnye materialy i ikh primenenie, 2011, no. 1–2, pp. 62–64.
- Semenova L.V., Nefedov N.I. Application of modified epoxy primers in the painting systems. Aviacionnye materialy i tehnologii, 2014, no. 3, pp. 38–44. DOI: 10.18577/2071-9140-2014-0-3-38-44.
- Chalykh A.E., Kochnova Z.A., Lark E.S. Compatibility and diffusion in epoxy oligomer – liquid carboxylate rubbers systems. Vysoko molekulyarnye soedineniya, series A, 2001, vol. 43, no. 12, pp. 2147–2155.
- Chalykh A.E. Diffusion in polymer systems. Moscow: Chemistry, 1987, pp.252–266.
- Kablov V.F. System technology of rubber-oligomeric compositions. Collection of articles X Intern. conf. on chemistry and physical chemistry of polymers. Volgograd: Volgograd State Tech. University, 2009, pp. 162–191.
- Lipatov Yu.S. Interfacial phenomena in polymers. Kiev: Naukova Dumka, 1980. 260 p.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.