Methods of chemical modification of epoxy oligomers (review)

Zagora A.G., Tkachuk A.I., Terekhov I.V., Mukhametov R.R.
Zagora A.G., Tkachuk A.I., Terekhov I.V., Mukhametov R.R. Methods of chemical modification of epoxy oligomers (review) // Proceedings of VIAM. 2021. No. 7. DOI: 10.18577/2307-6046-2021-0-7-73-85. URL: https://www.viam-works.ru/en/journal/2021/7/8
Keywords
PCM, epoxy oligomer, modification, reactive diluents, bismaleimides.
Abstract

This paper is devoted to one of the most pressing problems of modern non – metallic materials science-chemical modification of thermosetting systems based on epoxy oligomers with active diluents and bismaleimides: polymer binders for reinforced plastics, adhesives, compounds, sealants, and protective paint coatings. Based on the analysis of domestic and foreign scientific literature, as well as patents for inventions, a conclusion was made about the prospects for further research in this direction. The use of these types of modifiers can increase the chemical resistance, crack resistance, strength, impact strength, heat resistance and other valuable properties of polymer composite materials (PCM) based on an epoxy polymer matrix.

Reference list
  1. Kablov E.N., Valueva M.I., Zelenina I.V., Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials. Trudy VIAM, 2021, no. 1 (95), paper no. 7. Available at: http://www.viam-works.ru (accessed: June 29, 2021). DOI: 10.18577/2307-6046-2020-0-1-68-77.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N., Solovyanchik L.V., Kondrashov S.V., Yurkov G.Yu., Buznik V.M. et al. Electrically conductive hydrophobic polymer composite materials based on oxidized carbon nanotubes modified with tetrafluoroethylene telomers. Rossiyskie nanotekhnologii, 2016, vol. 11, no. 11–12. S. 91–97.
  4. Pavlyuk B.Ph. The main directions in the field of development of polymeric functional materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
  5. Mukhametov R.R., Petrova A.P. Properties of epoxy polymer binders and their processing into polymer composite materials. News of Materials Science. Science and technology. Novosti materialovedeniya. Nauka i tekhnika, 2018, no. 3-4 (30), paper no. 06. Available at: http://www.mterialsnews.ru (accessed: June 1, 2021).
  6. Muhametov R.R., Petrova A.P., Ponomarenko S.A., Dolgova E.V., Pavlyuk B.F. Properties of binder EDT-69N and polymer composites on its basis. Trudy VIAM, 2018, no. 4 (64), paper no. 04. Available at: http//www.viam-works.ru (accessed: June 1, 2021). DOI: 10.18577/2307-6046-2018-0-4-28-37.
  7. Tkachuk A.I., Gurevich Ya.M., Guseva M.A., Mishurov K.S. Technological and operational characteristics and fields of application of the epoxy binder VSE-1212, processed using prepreg technology. Klei. Germetiki. Tekhnologii, 2018, no. 4, pp. 29–34.
  8. Terekhov I.V., Shlenskiy V.A., Kurshev E.V., Lonskiy S.L., Dyatlov V.A. Researches of factors affecting the formation of epoxy-containing microcapsules for the self-healing compositions. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 27–34. DOI: 10.18577/2071-9140-2018-0-3-27-34.
  9. Panina N.N., Chursova L.V., Babin A.N., Grebeneva T.A., Gurevich Ya.M. The main methods of modifying epoxy polymer materials in Russia. Vse materialy. Entsiklopedicheskiy spravochnik, 2014, no. 9, pp. 10–17.
  10. Babaevsky P.G., Kulik S.G. Crack Resistance of Cured Polymer Compositions. Moscow: Khimiya, 1991.336 p.
  11. Chebotareva E.G., Ogrel L.Yu. Modern trends in the modification of epoxy polymers. Fundamentalnye issledovaniya, 2008, no. 4, pp. 102–104.
  12. Kochergin Yu.S., Grigorenko T.I. Influence of liquid reactive rubbers on wear resistance of epoxy adhesive compositions. Klei. Germetiki. Tekhnologii, 2013, no. 11, pp. 22–28.
  13. Nasonov F.A., Aleksashin V.M., Melnikov D.A., Bukharov S.B. Investigation of the modification of an epoxy binder and carbon fiber-reinforced plastic based on it with zinc stearate. Klei. Germetiki. Tekhnologii, 2018, no. 9, pp. 24–31.
  14. Anikhovskaya L.I., Batizat D.V., Baturina E.I., Leshchun E.V., Sakharov A.M. Non-combustible film glue and adhesive prepreg based on it. Klei. Germetiki. Tekhnologii, 2013, no. 6, pp. 2–5.
  15. Tatarintseva O.S., Zimin D.E., Samoilenko V.V. Influence of modification on technological and mechanical properties of an epoxyanhydride binder. Mekhanika kompozitsionnykh materialov i konstruktsiy, 2015, vol. 21, no. 4, pp. 489–500.
  16. Akopova T.A., Olikhova Yu.V., Osipchik V.S. Study of the curing process of epoxy-amine binders modified with epoxy-containing silsesquioxane by thermoanalytical methods. Klei. Germetiki. Tekhnologii, 2014, no. 11, pp. 22–26.
  17. Rakhmatullina A.P., Satbaeva N.S., Cherezova E.N. Modification of epoxy compositions with an oligomer based on polyethylene terephthalate destructate. Klei. Germetiki. Tekhnologii, 2018, no. 3, pp. 18–21.
  18. Golovkov P.V., Korotkova N.P., Potapochkina I.I. Influence of the type of active diluent on the protective properties of epoxy coatings. Lakokrasochnyye materialy i ikh primenenie, 2008, no. 6, pp. 18–21.
  19. Akulinicheva A.A., Korotkova N.P., Styunina A.O. The choice of a monofunctional active diluent for modifying the properties of the epoxy system. Lakokrasochnyye materialy i ikh primenenie, 2020, no. 4, pp. 38–40.
  20. Makhin M.N., Terekhov A.V., Dmitriev G.S. et al. Composite materials: properties of a polymer matrix based on epoxy resin and mono-epoxy diluent-p-tert-butylphenol glycidyl ether. Zhurnal prikladnoy khimii, 2018, vol. 91, no. 5, p. 749–754.
  21. Zarubina A.Yu., Kozhevnikov V.S., Trofimov A.N. et al. The influence of an active diluent on the rheokinetics of a heat-resistant binder based on a polyfunctional epoxy oligomer. Vestnik MITKHT im. M.V. Lomonosova, 2013, vol. 8, no. 4, pp. 99–102.
  22. Trofimov AN, Apeksimov NV, Simonov-Emelyanov ID, Prokhorova Yu.S. Influence of diluents on the kinetics of volumetric shrinkage and stresses during curing of epoxydian oligomers. Tonkie khimicheskiye tekhnologii, 2016, vol. 11, no. 6, pp. 103–107.
  23. Pakhomov K.S., Zarubina A.Yu., Antipov Yu.V., Simonov-Emelyanov I.D. Influence of modifiers on rheokinetics of curing of chlorine-containing epoxy binders. Plasticheskiye massy, 2012, no. 5, pp. 19–22.
  24. Gorbatkina Yu.A., Ivanova-Mumzhieva V.G., Kuperman A.M. Adhesion of modified epoxy matrices to reinforcing fibers. Vysokomolekulyarnyye soyedineniya, series A, 2016, vol. 58, no. 5, pp. 439–447.
  25. Nizina T.A., Selyaev V.P., Startsev O.V., Molokov M.V., Nizin D.R. Using the method of dynamic mechanical analysis to determine the characteristic temperature of the α′-transition of polymer composite materials based on low-viscosity epoxy binders. Polimery v stroitelstve, 2015, no. 1 (3). S. 55–68.
  26. Potapochkina I.I., Korotkova N.P., Tarasov V.N., Lebedev V.S. Modifiers of epoxy resins produced by NPP «Makromer». Klei. Germetiki. Tekhnologii, 2006, no. 7, pp. 14–17.
  27. Tuisov A.G., Belousov A.M., Bystrova O.V. Investigation of the effect of modifying an epoxy binder for fiberglass with an active diluent laproxide 301G and laproxide 603. Plasticheskiye massy, 2008, no. 6, pp. 29–31.
  28. Khozin V.G. Reinforcement of epoxy polymers. Kazan: Dom pechati, 2004, 446 p.
  29. Epoxy resin composition: pat. 10655005 USA, no. 15/560773; filed 22.03.16; publ. 19.05.20.
  30. Li Y., Li B., Chen W. A study on the reactive diluent for the solvent-free epoxy anticorrosive coating. Journal of Chemical and Pharmaceutical Research, 2014, vol. 6, no. 7, pp. 2466–2469.
  31. Shen L., Wang Y., Zhao Q. et al. Influence of a long-side-chain-containing reactive diluent on the structure and mechanical properties of UV-cured films. Polymer International, 2016, vol. 65, pp. 1150–1156. DOI: 10.1002/pi.5163.
  32. Multilayer structural adhesive film: pat. 10632707 USA, no. 15/774621; filed 14.11.16; publ. 28.04.20.
  33. Two-component mortar compound and use thereof: pat. 10633286 USA, no. 16/326386; filed 20.07.17; publ. 28.04.20.
  34. Marcos da Silva W., Ribeiro H., Cardoso Neves J. et al. Improved impact strength of epoxy by the addition of functionalized multiwalled carbon nanotubes and reactive diluent. Journal of Applied Polymer Science, 2015. DOI: 10.1002/APP.42587.
  35. Ali M., Hammami A. Experimental Modeling of the Cure Behavior of a Formulated Blend of DGEBA Epoxy and C12-C14 Glycidyl Ether as a Reactive Diluent. Polymer Composites, 2005. DOI: 10.1002/pc.20131.
  36. Flores H.A., Ayude M.A., Riccardi C.C., Fasce L.A. Influence of a Reactive Diluent on Curing Kinetics, Internal Curing Process, and Mechanical Performance of Filament Wound Glass Fiber-Reinforced Epoxy Composite Pipes. Polymer Engineering and Science, 2018. DOI: 10.1002/pen.24911.
  37. Cicala G., Recca G., Carciotto S., Restuccia C.L. Development of Epoxy/Hyperbranched Blends for Resin Transfer Molding and Vacuum Assisted Resin Transfer Molding Applications: Effect of a Reactive Diluent. Polymer Engineering and Science, 2009, vol. 49, no. 3, pp. 577–584. DOI: 10.1002/pen.21282.
  38. Epoxy composition for the manufacture of products from polymer composite materials by vacuum infusion: pat. 2488612 Rus. Federation, no. 2012115497/04; filed 18.04.12; publ. 27.07.13.
  39. Epoxy composition for the manufacture of products from polymer composite materials by vacuum infusion: pat. 2606443 Rus. Federation, no. 2015143321; filed 13.10.15; publ. 10.01.17.
  40. Heat-resistant epoxy binder for the manufacture of products by impregnation under pressure: pat. 2590563 Rus. Federation, no. 2015115289/05; filed 23.04.15; publ. 10.07.16
  41. Epoxy adhesive composition: pat. 2184131 Rus. Federation, no. 2000107500/04; filed 27.03.00; publ. 27.06.02.
  42. Compound for antifriction coatings: pat. 2621115 Rus. Federation, no. 2016133878; filed 18.08.16; publ. 31.05.17.
  43. Epoxy adhesive: pat. 2520479 Rus. Federation, no. 2012153357/05; filed 10.12.12; publ. 27.06.14.
  44. Electrical insulating filling and impregnating compound: pat. 2672094 Rus. Federation, no. 2017144361; filed 18.12.17; publ. 12.11.18.
  45. Highly filled compound for the manufacture of ferromagnetic cores: pat. 2680999 Rus. Federation, no. 2017144397; filed 18.12.17; publ. 01.03.19.
  46. A method of obtaining anti-adhesive coatings: pat. 2490292 Rus. Federation, no. 2011151675/05; filed 16.12.11; publ. 20.08.13.
  47. A method of obtaining antifriction materials for binary surfaces: pat. 2487904 Rus. Federation, no. 2012104096/05; filed 06.02.12; publ. 20.07.13.
  48. Glue composition (its variants): pat. 2174139 Rus. Federation, no. 2000132253/04; filed 22.12.00; publ. 27.09.01.
  49. Vibration-absorbing epoxy composition: pat. 2507228 Rus. Federation, no. 2012130493/05; filed 17.07.12; publ. 20.02.14.
  50. Adhesive composition: pat. 2285027 Rus. Federation, no. 2005118802/04; filed 17.06.05; publ. 10.10.06.
  51. Polymer composition: pat. 2507227 Rus. Federation, no. 2011132574/05; filed 03.08.11; publ. 20.02.14.
  52. Method of strengthening power structures: pat. 2516185 Rus. Federation, no. 2011153594/02; filed 28.12.11; publ. 20.05.14.
  53. Highly filled composite structural material: pat. 2657060 Rus. Federation, no. 2016125606; filed 27.06.16; publ. 08.06.18.
  54. Polymer composition: pat. 2506291 Rus. Federation, no. 2011153590/04; filed 28.12.11; publ. 10.02.14.
  55. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM. Aviacionnye materialy i tekhnologii, 2011, no. 2, pp. 38–42.
  56. Vavilova M.I., Sokolov I.I., Akhmadieva K.R., Yamshchikova G.A. Polymer composite materials with low porosity obtained by the technology of impregnation with a film binder. Voprosy materialovedeniya, 2017, no. 1 (89). S. 140-146.
  57. Mosiyuk V.N., Tomchani O.V. Evaluation of properties of glass-fibre-reinforced plastics based on epoxybisma-leimide resin, produced by different non-autoclave mol-ding techniques. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 47–52. DOI: 10.18577 / 2071-9140-2019-0-2-47-52.
  58. Mikhailin Yu.A. Heat-resistant polymers and polymer materials. Moscow: Professiya, 2006.624 p.
  59. Bismaleimide-epoxy compositions and prepregs: pat. 4510272 USA, no. 475836; filed 16.03.83; publ. 09.04.85.
  60. Rao B.S. Novel bismaleimides via epoxy-carboxy addition reaction: synthesis characterization and thermal stability. Journal Polymer Science, 1988, no. 1, pp. 3–10.
  61. Yerlikaya Z., Erinc N.К., Oktem Z. et al. Chain-extended bismaleimides. II. A study of chain-extended bismaleimides as matrix elements in carbon fiber composites. Journal of Applied Polymer Science, 1996, vol. 59, no. 3, pp. 537–542.
  62. Mikhaylin Yu.A., Minchenko I.P. Maleimide binders (review). Plasticheskiye massy, 1992, no. 5, pp. 56–64.
  63. Jena R.K., Yue C.Y., Sk M.M., Ghosh K.A. Novel high performance bismaleimide/diallyl bisphenol A (BMI/DBA) – epoxy interpenetrating network resin for rigid riser application. RSC Advances, 2015, no. 5 (97), pp. 79888–79897.
  64. Xiong X., Chen P., Zhang J. et al. Preparation and Properties of High Performance Phthalide-Containing Bismaleimide Modified Epoxy Matrices. Journal of Applied Polymer Science, 2011, vol. 121, pp. 3122–3130. DOI: 10.1002/app.33588.
  65. Xiong X., Chen P., Zhu N. et al. Synthesis and Properties of a Novel Bismaleimide Resin Containing 1,3,4-Oxadiazole Moiety and the Blend Systems Thereof With Epoxy Resin. Polymer Engineering and Science, 2011, vol. 51, no. 8, pp. 1599–1606. DOI: 10.1002/pen.21942.
  66. Suresh Kumar R., Alagar M. Studies on Mechanical, Thermal, and Morphology of Diglycidylether-Terminated Polydimethylsiloxane-Modified Epoxy-Bismaleimide Matrices. Journal of Applied Polymer Science, 2006, vol. 101, pp. 668–674. DOI: 10.1002/app.23799.
  67. Mahesh K.P.O., Alagar M., Jothibasu S. A Comparative Study on the Preparation and Characterization of Aromatic and Aliphatic Bismaleimides-Modified Polyurethane-Epoxy Interpenetrating Polymer Network Matrices. Journal of Applied Polymer Science, 2006, vol. 99, pp. 3592–3602. DOI: 10.1002/app.22982.
  68. Ambika Devi K., Bibin J., Reghunadhan Nair C.P., Ninan K.N. Syntactic Foam Composites of Epoxy-Allyl Phenol-Bismaleimide Ternary Blend Processing and Properties. Journal of Applied Polymer Science, 2007, vol. 105, pp. 3715–3722. DOI: 10.1002/app.26316.
  69. Shenoy M.A., Patil M., Shetty A. Modification of Epoxy Resin by Addition of Bismaleimide and Diallyl Phthalate. Polymer Engineering and Science, 2007, vol. 47, no. 11, pp. 1881–1888. DOI: 10.1002/pen.20901.
  70. Yuan L., Liang G., Gu A. Novel fiber reinforced bismaleimide/diallyl bisphenol A/microcapsules composites. Polymers for Advanced Technologies, 2011, vol. 22, pp. 2264–2272. DOI: 10.1002/pat.1755.
  71. Zhou B.X., Huang Y.J., Zhang X.H. et al. Thermal Properties of an Epoxy Cresol-Formaldehyde Novolac/Diaminodiphenyl Sulfone System Modified by Bismaleimide Containing Tetramethylbiphenyl and Aromatic Ether Structures. Polymer Engineering and Science, 2009, vol. 49, no. 8, pp. 1525–1532. DOI: 10.1002/pen.21381.
  72. The composition of the epoxy-bismaleimide binder for prepregs (options), a method for producing epoxy-bismaleimide binder (options), prepreg and product: pat. 2335514 Rus. Federation, no. 2006147031/04; filed 27.12.06; publ. 10.10.08.
  73. Composition of epoxy-bismaleimide binder for prepregs, prepreg and product: pat. 2427598 Rus. Federation, no. 2009139831/05; filed 15.12.14; publ. 20.06.16.
  74. Composition of epoxy-bismaleimide resin and method for its production: pat. 2587169 Rus. Federation, no. 2014150885/05; filed 15.12.14; publ. 20.06.16.