Formation of silicon carbide coatings by chemical vapor deposition (review)

Part 1
Sidorov D.V., Shavnev A.A., Melentev A.A.
Sidorov D.V., Shavnev A.A., Melentev A.A. Formation of silicon carbide coatings by chemical vapor deposition (review). Part 1 // Proceedings of VIAM. 2021. No. 6. DOI: 10.18577/2307-6046-2021-0-6-100-111. URL: https://www.viam-works.ru/en/journal/2021/6/10
Keywords
chemical vapor deposition, silicon carbide, coating, literature review, chemical reaction, reagent.
Abstract

The article provides an overview of the scientific and technical literature in the field of the formation of silicon carbide coatings by chemical vapor deposition (CVD). CVD is a complex process, approaches to which vary depending on the tasks being solved. Depending on the technological parameters, the initial reagents, the substrate for deposition, the type and design of the CVD reactors, it is possible to achieve both the deposition of pure silicon carbide and the co-deposition of silicon and/or carbon.

In the first part of the article, attention is paid to the study of CVD from the point of view of the mechanisms of chemical reactions, the design of the deposition apparatus, the substrates for deposition.

Reference list
  1. Kablov E.N., Echin A.B., Bondarenko Yu.A. History of development of directional crys-tallization technology and equipment for casting blades of gas turbine engines. Trudy VIAM, 2020, no. 3 (87), paper no. 01. Available at: http://www.viam-works.ru (accessed: April 1, 2020). DOI: 10.18577/2307-6046-2020-0-3-3-12.
  2. Kablov E.N., Semenova S.N., Suleymanov R.R., Chaykun A.M. Prospects for the use of ethylene-propylenediene rubber as part of cold resistant rubber. Trudy VIAM, 2019, no. 12 (84), paper no. 4. Available at: http://www.viam-works.ru (accessed: December 29, 2020).
  3. Kablov E.N., Valueva M.I., I.V. Zelenina, Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials. Trudy VIAM, 2020, no. 1, paper no. 07. Available at: http://www.viam-works.ru (accessed: December 29, 2020). DOI: 10.18577/2307-6046-2020-0-1-68-77.
  4. Matovic B., Yano T. Handbook of Advanced Ceramics. Oxford, 2013, pp. 225–244.
  5. Sidorov D.V., Storozhenko P.A., Shutova O.G., Kozhevnikov B.E. Obtaining alkylsilanes of high purity. Khimicheskaya tekhnologiya, 2006. No. 7, pp. 22-24.
  6. Sidorov D.V., Schavnev А.А., Solodkin P.V., Kirilin A.D. Quantum chemical calculation of intermolecular interaction methylsilane molecules during the pyrolysis process. Trudy VIAM, 2019, no. 11 (83), paper no. 5. Available at: http://www.viam-works.ru (accessed: January 4, 2021). DOI: 10.18577/2307-6046-2019-0-11-44-52.
  7. Choy K. Chemical vapour deposition of coatings. Progress in material science, 2003, vol. 48, pp. 57–170. DOI: 10.1016/S0079-6425(01)00009-3.
  8. Hishimone P., Nagai H., Sato M. Methods of Fabricating Thin Films for Energy Materials and Devices. Lithium-Ion Batteries – Thin Film for Energy Materials and Devices. Intechopen Limited. London, 2020, pp. 6. DOI: 10.5772/intechopen.85912.
  9. Wang L., Zhang W. Effect of free carbon on micro-mechanical properties of a chemically vapor T deposited SiC coating. Ceramics International. 2018, vol. 44, pp. 17118–17123.
  10. Yang L., Chen Z., Wang B. Chemical vapor deposition of SiC at different molar ratios of hydrogen to methyltrichlorosilane. Journal of Central South University of Technology. 2009, vol. 16, pp. 0730–0737. DOI: 10.1007/s11771-009-0121-4.
  11. Yang L., Zhang W. Kinetic and Microstructure of SiC Deposited from SiCl4–CH4–H2. Chinese Journal of Chemical Engineering. 2009, vol. 17, pp. 419–426. DOI: 10.1016/S1004-9541(08)60226-8.
  12. Zhang W., Huttinger G. CVD of SiC from Methyltrichlorosilane. Part I: Deposition Rates. Chemical Vapor Deposition. 2001, vol. 7, pp. 167–172.
  13. Zhang W., Huttinger G. CVD of SiC from Methyltrichlorosilane. Part II: Composition of the Gas Phase and the Deposit. Chemical Vapor Deposition. 2001, vol. 7, pp. 173–181.
  14. Reznik B., Gerthsen D., Zhang W., Huttinger G. Microstructure of SiC deposited from methyltrichlorosilane. Journal of the European Ceramic Society. 2003, vol. 23, pp. 1499–1508.
  15. Allendorf M., Mellus C. Theoretical Study of the Thermochemistry of Molecules in the Si–C–Cl–H System. Journal of Physical Chemistry. 1993, vol. 97, pp. 720–728.
  16. Deng J., Su K., Wang X. Thermodynamic properties of the most stable gaseous small silicon-carbon clusters in their ground states. The European Physical Journal D. 2008. Vol. 49, pp. 21–35.
  17. Mosebach H., Hopfe V., Erhard M., Meyer M. Monitoring of SiC Deposition in an Industrial CVI/CVD Reactor by In-Situ FTIR Spectroscopy. Journal de Physique IV Colloque. 1995, vol. 05, pp. 97–104.
  18. Jonas S., Ptak V., Sodowski W. FTIR In situ studies of the gas phase reactions in chemical vapor deposition of SiC. Journal of the Electrochemical Society. 1995, vol. 142, pp. 2357–2362.
  19. Papasouliotis G., Sotirchos S. Experimental study of atmospheric pressure chemical vapor deposition of silicon carbide from methyltrichlorosilane. Journal of Material Research. 1999, vol. 14, pp. 3397–3409.
  20. Nigam S., Chung H., Polyakov F. Growth kinetics study in halide chemical vapor deposition of SiC. Journal of Crystal Growth. 2005, vol. 284, pp. 112–122.
  21. Lu C., Cheng L., Zhao C. Kinetics of chemical vapor deposition of SiC from methyltrichlorosilane and hydrogen. Applied Surface Science. 2009, vol. 255, pp. 7495–7499.
  22. Chollon G., Langlais F., Placide M., Weisbecker P. Transient stages during the chemical vapour deposition of silicon carbide from CH3SiCl3/H2: impact on the physicochemical and interfacial properties of the coatings. Thin Solid Films. 2012, vol. 520, pp. 6075–6087.
  23. Lee Y., Choi D. The effect of diluent gases on the growth behavior of CVD SiC films with temperature. Journal of Materials Science. 2000, vol. 35, pp. 4519–4526.