Study of the main properties of glass fiber laminates for printed circuit boards and assessment of the influence of climatic influences on the indicators of their dielectric constant

Mishurov K.S., Payarel S.M., Kurnosov A.O., Sokolov I.I., Egorov A.V.
Mishurov K.S., Payarel S.M., Kurnosov A.O., Sokolov I.I., Egorov A.V. Study of the main properties of glass fiber laminates for printed circuit boards and assessment of the influence of climatic influences on the indicators of their dielectric constant // Proceedings of VIAM. 2021. No. 6. DOI: 10.18577/2307-6046-2021-0-6-74-81. URL: https://www.viam-works.ru/en/journal/2021/6/8
Keywords
glass fiber laminates, fiberglass, dielectric, printed circuit board, polymer matrix, composite material.
Abstract

In this paper, the main properties of glass fiber laminates – dielectric composite materials for printed circuit boards are considered: glass transition temperature, temperature coefficient of linear expansion, ultimate strength in bending, water resistance. The influence of climatic influences (increased ambient temperature, low ambient temperature, increased air humidity, the effect of temperature changes, the effect of salt fog) on the dielectric constant of glass fiber laminates has been evaluated.

Reference list
  1. Pirogova E.V. Design and technology of printed circuit boards. Moscow: FORUM-INFRA-M, 2005, 560 p.
  2. Medvedev A.M., Mozharov V.A., Mylov G.V. Printed circuit boards. The current state of basic materials. Pechatnyy montazh, 2011, no. 5 (34). S. 148-149.
  3. Sarychev I.A., Serkova E.A., Khmelnitsky V.V., Zastrogin O.B. Thermosetting binders for aircraft floor panel materials (review). Trudy VIAM, 2019, no. 7 (79), paper no. 03. Available at: http://www.viam-works.ru (accessed: March 1, 2021). DOI: 10.18577/2307-6049-2019-0-7-26-33.
  4. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  5. Mishkin S.I., Malakhovskiy S.S. Fast curing resins and prepregs: receiving, properties and areas of application (review). Trudy VIAM, 2019, no. 5 (77), paper no. 04. Available at: http://viam-works.ru (accessed: March 1, 2021). DOI: 10.18577/2307-6046-2019-0-5-32-40.
  6. Kurnosov A.O., Vavilova M.I., Melnikov D.A. Manufacturing technologies of glass fillers and study of effects of finishing material on physical and mechanical properties of fiberglass plastics. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 64–70. DOI: 10.18577/2071-9140-2018-0-1-64-70.
  7. Medvedev A.P. Printed circuit boards. Constructions and materials. Moscow: Tekhnosfera, 2005, 304 p.
  8. Medvedev A.M. Materials for flexible printed circuit boards. Tekhnologii v elektronnoy promyshlennosti, 2011, no. 3, pp. 12–19.
  9. Kablov E.N., Startsev O.V. The basic and applied research in the field of corrosion and ageing of materials in natural environments (review). Aviacionnye materialy i tehnologii, 2015, no. 4 (37), pp. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
  10. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Climatic aging of composite materials for aviation purposes. III. Significant factors of aging. Deformatsiya i razrusheniye materialov, 2011, no. 1, pp. 34–40.
  11. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Climatic aging of composite materials for aviation purposes. I. Mechanisms of aging. Deformatsiya i razrusheniye materialov, 2010, no. 11, pp. 19–27.
  12. Kirillov V.N., Startsev O.V., Efimov V.A. Climatic firmness and damageability of polymeric composite materials, problems and solutions. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 412–423.
  13. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Climatic aging of composite materials for aviation purposes. II. Relaxation of the initial structural nonequilibrium and the gradient of properties over thickness. Deformatsiya i razrusheniye materialov, 2010, no. 12, pp. 40–46.
  14. Kablov E.N., Grashchenkov D.V., Erasov V.S., Anchevsky I.E., Ilyin V.V., Walter R.S. Stand for testing at the climatic station GTSKI large-sized structures made of PCM. Reports of IX Intern. scientific. conf. on hydroaviation "Gidroaviasalon-2012". Gelendzhik, 2012, pp. 122–123.
  15. Shirokov V.V., Romanov A.M. Waveguide method research of honeycomb glass fibre plastics dielectric characteristics. Aviacionnye materialy i tehnologii, 2013, no. 4, pp. 62–68.