Investigation of the effect of the final curing temperatures on the complex of properties of carbon-glass hybrid materials
Kolpachkov E.D., Kurnosov A.O., Marachovskiy P.C., Petrova A.P. Investigation of the effect of the final curing temperatures on the complex of properties of carbon-glass hybrid materials // Proceedings of VIAM. 2021. No. 6. DOI: 10.18577/2307-6046-2021-0-6-66-73. URL: https://www.viam-works.ru/en/journal/2021/6/7
Keywords
thermosetting binder, polymer composite materials, product aviation purpose, glass-carbon composite material, hybrid composite materials.
Abstract
Presents the results of a study of the effect of the final curing temperatures on the complex of properties of the developed epoxy binder grade VSE-65 and glass-fiber-reinforced plastic based on it. It was found that with a decrease in the final curing temperature, the residual heat effect increases and, in turn, a decrease in the conversion of epoxy groups occurs. Presents the results of a comparative analysis of VKG-6 glass-carbon plastic samples prepared by vacuum infusion and pressure impregnation. Based on the results of the analysis, it has been established that the technologies make it possible to realize the required level of physical and mechanical properties.
Reference list
- Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
- Kablov E.N. Modern materials – the basis of innovative modernization of Russia. Metally Evrazii, 2012, no. 3, pp. 10–15.
- Kablov E.N. Trends and guidelines for innovative development in Russia: collection of inform. materials. 3rd ed., rev. and add. Moscow: VIAM, 2015, 720 p.
- Satdinov R.A., Istyagin S.E., Veshkin E.A. Analysis of the temperature-time parameters mode curing PCM with specified characteristics. Trudy VIAM, 2017, no. 3, paper no. 9. Available at: http://www.viam-works.ru (accessed: April 16, 2021). DOI: 10.18577/2307-6046-2017-0-3-9-9.
- Dushin M.I., Hrulkov A.V., Muhametov R.R. A choice of technological parameters of autoclave formation of details from polymeric composite materials. Aviacionnye materialy i tehnologii, 2011, no. 3, pp.20–26.
- Zagora A.G., Kondrashov S.V., Antyufeeva N.V., Pykhtin A.A. Research of influence of technological modes of production of epoxy nanocomposites with carbon nanotubes on their heat resistance. Trudy VIAM, 2019, no. 1 (73), paper no. 08. Available at: http://www.viam-works.ru (accessed: April 16, 2021). DOI: 10.18577/2307-6046-2019-0-1-64-73.
- Melnikov D.A., Khaskov M.A., Guseva M.A., Antyufeeva N.V. To the question of the development of pressing mode for laminated PCMs based on prepregs. Trudy VIAM, 2018, no. 2, paper no. 09. Available at: http://www.viam-works.ru (accessed: April 16, 2021). DOI: 10.18577/2307-6046-2018-0-2-9-9.
- Kogan D.I., Dushin M.I., Borshchev A.N., Veshkin E.A., Abramov P.A., Makrushin K.V. Properties of structural carbon-fiber reinforced plastics made by impregnation under vacuum. Izvestiya Samarskogo nauchnogo tsentra RAN, 2012, vol. 14, no. 4 (2), pp. 762–766.
- Antyufeeva N.V., Komarova O.A., Pavlovskij K.A., Aleksashin V.M. Practice of the calorimetric control reactionary ability prepreg KMU-11tr. Trudy VIAM, 2014, no. 2, paper no. 06. Available at: http://viam-works.ru (accessed: April 16, 2021). DOI: 10.18577/2307-6046-2014-0-2-6-6.
- Ustinova A.M., Oleinikova E.V., Lipskaya V.A. et al. Fast-curing epoxy binder. Plasticheskiye massy, 1983, no. 3, pp. 34–42.
- Khaskov M.A., Melnikov D.A., Kotova E.V. Selection of temperature-time modes of curing epoxy binders taking into account the scale factor. Klei. Germetiki. Tekhnologii, 2017, no. 10, p. 24.
- Dmitriev O.S., Kirillov V.N., Zuev A.V., Cherepakhina A.A. Influence of the type of filler on the optimal modes of solidification of thick-walled PCM. Klei. Germetiki. Tekhnologii, 2011, no. 11, p. 27.
- Veshkin E.A. Features of out-of-autoclave forming of poor-porous PCM. Trudy VIAM, 2016, no. 2 (38), paper no. 07. Available at: http://www.viam-works.ru (accessed: April 16, 2021). DOI: 10.1857/2307-6046-2016-0-2-7-7.
- Kolpachkov E.D., Kurnosov A.O., Petrova A.P., Raskutin A.E. Hybrid composite materials for aviation based on fibrous fillers (review). Voprosy materialovedeniya, 2020, no. 1 (101), pp. 126–138.
- Kolpachkov ED, Gurevich Ya.M., Kurnosov A.O., Marakhovsky PS, Petrova A.P. Investigation of the characteristics of glass-carbon plastics based on binders with a low curing temperature. Vse materialy. Entsiklopedicheskiy spravochnik, 2021, no. 6, pp. 41–45.