Fibrous composite materials with a metal matrix (review)

Zhabin A.N., Sidorov D.V., Nyafkin A.N.
Zhabin A.N., Sidorov D.V., Nyafkin A.N. Fibrous composite materials with a metal matrix (review) // Proceedings of VIAM. 2021. No. 6. DOI: 10.18577/2307-6046-2021-0-6-27-35. URL: https://www.viam-works.ru/en/journal/2021/6/3
Keywords
composite material, aluminum, titanium, carbon fibers, ceramic fibers, metal-intermetallic laminate.
Abstract

The article provides an overview of the literature in the field of composite materials (CM) based on metal matrices reinforced with carbon fibers. The main structural, physical and mechanical properties and morphology of such CMS are briefly described. The structure and properties of new CMS from multilayer metal-intermetallic multilayer laminates reinforced with carbon and ceramic fibers are also presented. Application of the method of ultrasonic consolidation for the manufacture of multilayer fibrous CMs based on metal-intermetallic laminates provides high adhesion of fibers with an intermetallic layer.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Composites: Today and Tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
  3. Kablov E.N., Chabina E.B., Morozov G.A., Muravskaya N.P. Conformity assessment of new materials using high-level CRM and MI. Kompetentnost, 2017, no. 2 (143), pp. 40–46.
  4. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  5. Akmeev A.R., Gulyaev I.N., Ilyichev A.V., Ivanov N.V Research of mechanical behav-ior of metal composite (aluminum and car-bon fiber-reinforced polymer) with an adap-tive reinforcement scheme. Aviacionnye materialy i tehnologii, 2017, no. 3 (48), pp. 43–49. DOI: 10.18577/2071-9140-2017-0-3-43-49.
  6. Yakovlev A.L., Nochovnaya N.A., Putyrskij S.V., Krohina V.A. Titanium-polymer laminated materials. Aviacionnye materialy i tehnologii, 2016, no. S2, pp. 56–62. DOI: 10.18577/2071-9140-2016-0-S2-56-62.
  7. Arislanov A.A., Goncharova L.J., Nochovnaya N.А., Goncharov V.A. Prospects for the use of titanium alloys in laminated composite materials. Trudy VIAM, 2015, no. 10, paper no. 04. Available at: http://www.viam-works.ru (accessed: February 26, 2021). DOI: 10.18577/2307-6046-2015-0-10-4-4.
  8. Valueva M.I., Zelenina I.V., Khaskov M.A., Gulyaev A.I. Preparation of carbon fibers to interphase coating deposition for ceramic matrix composites. Trudy VIAM, 2017, no. 10 (58), paper no. 09. Available at: http://www.viam-works.ru (accessed: March 3, 2021). DOI: 10.185577/2307-6046-2017-0-10-9-9.
  9. Mahaviradhan N., Sivaganesan S., Sravya N.P., Parthiban A. Experimental investigation on mechanical properties of carbon fiber reinforced aluminum metal matrix composite. Materials Today: Proceedings, 2021, vol. 39, part 1, pp. 743–747.
  10. Deshpande M., Gondil R., Rahul S.V.S. et al. Processing and characterization of carbon fiber reinforced aluminum 7075. Materials Today: Proceedings, 2018, vol. 5 (2), pp. 7115–7122.
  11. Deshpande M., Ramesh S. V. S., Gondil R. et al. Studies on 7075 aluminum alloy MMCs with milled carbon fibers as reinforcements. Transactions of the Indian Institute of Metals, 2018, vol. 71 (4), pp. 993–1002.
  12. Tamilarasan U., Karunamoorthy L., Palanikumar K. Mechanical properties evaluation of the carbon fiber reinforced aluminum sandwich composites. Materials Research, 2015, vol. 18 (5), pp. 1029–1037.
  13. Even C., Arvieu C., Quenisset J.M. Powder route processing of carbon fibers reinforced titanium matrix composites. Composites Science and Technology, 2008, vol. 68, pp. 1273–1281.
  14. Arvieu C., Manaud J.P., Quenisset J.M. Interaction between titanium and carbon at moderate temperatures. Journal of Alloys and Compounds, 2004, vol. 68, pp. 116–122.
  15. Sidorov D.V., Serpova V.M., Zavodov A.V., Shavnev A.A. Investigation of interphase interaction at the interface in the Ti – C system with domestic titanium alloys of classes α + β and pseudo-α. Fizika i khimiya obrabotki materialov, 2020, no. 5, pp. 75–81. DOI: 10.30791/0015-3214-2020-5-75-81.
  16. Jiao F., Liu M., Jiang F. et al. Continuous carbon fiber reinforced Ti / Al3Ti metal-intermetallic laminate (MIL) composites fabricated using ultrasonic consolidation assisted hot pressing sintering. Materials Science & Engineering A, 2019, vol. 765, pp. 1–21.
  17. Han Y., Lin C., Han X. et al. Fabrication, interfacial characterization and mechanical properties of continuous Al2O3 ceramic fiber reinforced Ti/Al3Ti metal-intermetallic laminated (CCFR-MIL) composite. Materials Science & Engineering A, 2017, vol. 688, pp. 338–345.
  18. Ji C., Wang B., Hu J. et al. Effect of different preparation methods on mechanical behaviors of carbon fiber-reinforced PEEK-Titanium hybrid laminates. Polymer Testing, 2020, vol. 85, pp. 1–10. DOI: 10.1016/j.polimertesting.2020.106462.
  19. Vecchio K.S., Jiang F. Fracture toughness of Ceramic-Fiber-Reinforced Metallic-Intermetallic-Laminate (CFR-MIL) composites. Materials Science & Engineering A, 2016, vol. 649, pp. 407–416.