Methods additive manufacturing of magnesium alloys (review)
Tokarev M.S., Trofimov N.V., Leonov A.A., Alikhanyan A.A. Methods additive manufacturing of magnesium alloys (review) // Proceedings of VIAM. 2021. No. 6. DOI: 10.18577/2307-6046-2021-0-6-3-16. URL: https://www.viam-works.ru/en/journal/2021/6/1
Keywords
additive manufacturing, magnesium, magnesium alloys, magnesium alloy production, additive manufacturing methods, deposition, 3D printing, selective melting, laser melting, inkjet printing, mechanical properties.
Abstract
The development of industrial production in the modern world cannot do without the use of new technologies. This article discusses various methods for the additive manufacturing of magnesium alloy parts. There are several alternative methods for producing parts, such as selective laser fusion, direct laser deposition and arc welding. Depending on the additive manufacturing method, finished parts will differ in structure, phase composition and mechanical properties. The article presents a comparison of traditional and additive manufacturing methods for parts.
Reference list
- Kablov E.N. The dominant feature of the national technology initiative. Problems of accelerating the development of additive technologies in Russia. Metally Evrazii, 2017, no. 3, pp. 2–6.
- Kablov E.N. Present and future of additive technologies. Metally Evrazii, 2017, no. 1, pp. 2–6.
- Kablov E.N., Akinina M.V., Volkova E.F., Mostyaev I.V., Leonov A.A. The research of aspects of phase composition and fine structure of magnesium alloy ML9 in the as-cast and heat-treated conditions. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 17–24. DOI: 10.18577/2071-9140-2020-0-2-17-24.
- Leonov A.A., Trofimov N.V., Duyunova V.A., Uritia Z.P. Trends in the development of cast magnesium alloys with an increased ignition temperature (review). Trudy VIAM, 2021, no. 2 (96), paper no. 1. Available at: http://www.viam-works.ru (accessed: April 5, 2021). DOI: 10.18577/2307-6046-2021-0-2-3-9.
- Volkova E.F., Mostyaev I.V., Akinina M.V. Comparative analysis of mechanical properties anisotropy and microstructure of semi-finished products from high-strength magnesium alloys with REE. Trudy VIAM, 2018, no. 5 (65), paper no. 4. Available at: http://www.viam-works.ru (accessed: March 25, 2021). DOI: 10.18577/2307-6046-2018-0-5-24-33.
- Duyunova V.A., Molodtsov S.V., Leonov A.A., Trapeznikov A.V. Application of computer modeling methods in the manufacture of complex-contoured shaped casting. Trudy VIAM, 2019, no. 11 (83), paper no. 1. Available at: http://www.viam-works.ru (accessed: April 7, 2021). DOI: 10.18577/2307-6046-2019-0-11-3-11.
- Knyazev A.E., Vostrikov A.V. Sieving of powders additive and powder manufactu-rings (review). Trudy VIAM, 2020, no. 11 (93), paper no. 2. Available at: http://www.viam-works.ru (accessed: April 8, 2021). DOI: 10.18577/2307-6046-2020-0-11-11-20.
- Egorkin V.S., Gnedenkov S.V., Sinebryukhov S.L. et al. Increasing thickness and protective properties of PEO-coatings on aluminum alloy. Surface and Coatings Technology, 2018, vol. 334, pp. 29–42.
- Mohedano M., Blawert C., Zheludkevich M.L. Cerium-based sealing of PEO coated AM50 magnesium alloy. Surface and Coatings Technology, 2015, vol. 269, pp. 145–154.
- Sinebryukhov S.L., Gnedenkov A.S., Mashtalyar D.V., Gnedenkov S.V. PEOcoating/substrate interface investigation by localised electrochemical impedance spectroscopy. Surface and Coatings Technology, 2010, vol. 205, pp. 1697–1701.
- Gnedenkov A.S., Sinebryukhov S.L., Mashtalyar D.V., Gnedenkov S.V. Microscale morphology and properties of the PEO-coating surface. Physics Procedia, 2012, vol. 23, pp. 98–101.
- Gnedenkov A.S., Sinebryukhov S.L., Mashtalyar D.V., Gnedenkov S.V. Protective properties of inhibitor-containing composite coatings on a Mg alloy. Corrosion Science, 2016, vol. 102, pp. 348–354.
- Zhang Y., Blawert C., Tang S. et al. Influence of surface pre-treatment on the deposition and corrosion properties of hydrophobic coatings on a magnesium alloy. Corrosion Science, 2016, vol. 112, pp. 483–494.
- Li Z., Jing X., Yuan Y., Zhang M. Composite coatings on a Mg-Li alloy prepared by combined plasma electrolytic oxidation and solegel techniques. Corrosion Science, 2012, vol. 63, pp. 358–366.
- Cui X., Lin X., Liu C. et al. Fabrication and corrosion resistance of a hydrophobic micro-arc oxidation coating on AZ31 Mg alloy. Corrosion Science, 2015, vol. 90, pp. 402–412.
- Zhao J., Xie X., Zhang C. Effect of the graphene oxide additive on the corrosion resistance of the plasma electrolytic oxidation coating of the AZ31 magnesium alloy. Corrosion Science, 2017, vol. 114, pp. 146–155.
- Guo X., Du K., Guo Q. et al. Experimental study of corrosion protection of a three-layer film on AZ31B Mg alloy. Corrosion Science, 2012, vol. 65, pp. 367–375.
- Kruth J., Mercelis P., Van Vaerenbergh J. et al. Binding mechanisms in selective laser sintering and selective laser melting. Rapid Prototyping Journal, 2005, vol. 11, pp. 26–36.
- Wei K., Wang Z., Zeng X. Influence of element vaporization on formability, composition, microstructure, and mechanical performance of the selective laser melted Mg–Zn–Zr components. Materials Letters, 2015, vol. 156, pp. 187–190.
- Vyasaraj M., Gururaj P., Manoj G., Selective Laser Melting of Magnesium and Magnesium Alloy Powders: a Review. Metals, 2017, vol. 7, pp. 1–35.
- Bar F., Berger L., Jauer L. et al. Laser additive manufacturing of biodegradable magnesium alloy WE43: a detailed microstructure analysis. Acta Biomaterialia, 2019, vol. 98, pp. 36–49.
- Gnedenkov S.V., Sinebryukhov S.L. Magnesium fabricated using additive technology: Specificity of corrosion and protection. Journal of Alloys and Compounds, 2019, vol. 808, pp. 151629.
- Arrabal R., Mota J., Criado A. et al. Assessment of duplex coating combining plasma electrolytic oxidation and polymer layer on AZ31 magnesium alloy. Surface and Coatings Technology, 2012, vol. 206, pp. 4692–4703.
- Song B., Dong S., Zhang B. et al. Effects of processing parameters on microstructure and mechanical property of selective laser melted Ti6Al4V. Materials Letters, 2012, vol. 35, pp. 120–125.
- ASTM F2792–12a. Standard Terminology for Additive Manufacturing. West Conshohocken, 2013, pp. 1–3.
- Takagi H., Sasahara H., Abe T., Sannomiya H. et al. Material-property evaluation of magnesium alloys fabricated using wire-and-arcbased additive manufacturing. Additive Manufacturing, 2018, vol. 24, pp. 498–507.
- Vorndran E., Moseke C., Gbureck U. 3D printing of ceramic implants. MRS Bulletin, 2015, vol. 40, pp. 127–136.
- Meininger S., Moseke C., Spatz K. et al. Effect of strontium substitution on the material properties and osteogenic potential of 3D powder printed magnesium phosphate scaffolds. Materials Letters, 2019, vol. 98, pp. 1145–1158.
- Ji B., Junqi S.,Shengsun H. et al. Microstructure and mechanical properties of AZ91 Mg alloy fabricated by cold metal transfer additive manufacturing. Materials Letters, 2020, vol. 276, pp. 128185.
- Yangyang G., Houhong P., Lingbao R., Gaofeng Q. Microstructure and mechanical properties of wire arc additively manufactured AZ80M magnesium alloy. Materials Letters, 2019, vol. 247, pp. 4–6.