Study of the effect of two types of fire retardants on the flammability of epoxy resin samples

Barbotko S.L., Bochenkov M.M., Volnyj O.S., Korobeinichev O.P., Shmakov A.G.
Barbotko S.L., Bochenkov M.M., Volnyj O.S., Korobeinichev O.P., Shmakov A.G. Study of the effect of two types of fire retardants on the flammability of epoxy resin samples // Proceedings of VIAM. 2021. No. 4. DOI: 10.18577/2307-6046-2021-0-4-132-140. URL: https://www.viam-works.ru/en/journal/2021/4/11
Keywords
UL 94, DOPO-THPO, fire safety, flammability, polymeric material, fire retardant, graphene, DOPO-THPO.
Abstract

Studies have been carried out to assess the effectiveness of fire retardants on the flammability of an epoxy composition – graphene and an organophosphorus compound DOPO-THPO. The concentrations of the added flame retardants were 2 and 4 % (mass). Flammability characteristics were determined using the method according to GOST 28157 (UL 94) with vertical and horizontal samples. It was found that the introduction of fire retardants reduces the flammability of the epoxy composition, but the introduction of even 4 % was insufficient to ensure self-extinguishing of the epoxy composition during vertical testing.

Reference list
  1. About fire safety: Feder. Law of December 21, 1994 No. 69-FZ (as amended on May 28, 2017 No. 100-FZ). Available at: https: //www.consultant.ru/document/cons_doc_LAW_5438 (accessed: February 09, 2021).
  2. State Standard 25076–81. Non-metallic materials for interior decoration of vehicles. Flammability determination method. Moscow: Publishing house of standards, 2003, 4 p.
  3. State Standard R 55183–2012. Locomotive-hauled passenger cars. Fire safety requirements. Moscow: Standartinform, 2013.16 p.
  4. Standards of airworthiness of transport category aircraft: AP-25. Ed. 5th as amended 1–8. Moscow: Aviaizdat, 2015, 288 p.
  5. Airworthiness Standards: Transport Category Airplanes: Part 25. Electronic Code of Federal Regulation. Title 14: Aeronautic and Space. Chapter 1. Subchapter C. Available at: https://www.ecfr.gov/cgi-bin/text-idx?SID=9091f0ebbfbf1539cdb87015908ad369&mc=true&node=pt14.1.25&rgn=div5 (accessed: December 01, 2020).
  6. International Code for Application of Fire Test Procedures, 2010 (2010 FTR Code, IMO resolution MSC.307 (88)). Saint Petersburg: TsNIIMF, 2011, 60 p.
  7. State Standard R ISO 14624-1-2010. Space systems. Safety and material compatibility. Part 1. Determination of upward flammability of materials. Moscow: Standartinform, 2011, 15 p.
  8. State Standard R ISO 14624-2–2010. Space systems. Safety and material compatibility. Part 2. Determination of flammability of insulation of electrical wires and auxiliary materials. Moscow: Standartinform, 2012, 18 p.
  9. State Standard R ISO 14624-4-2010. Space systems. Safety and material compatibility. Part 4. Determination of vertical flammability of materials in compressed oxygen or oxygen-enriched environment. Moscow: Standartinform, 2011.8 p.
  10. Van Krevelen D. W., Te Nijenhuis K. Properties of Polymers: Their Correlation with Chemical Structure; Their Numerical Estimation and Prediction From Additive Group Contributions. 4th Revised Edition. Elsevier Science & Technology, 2009, 1004 p.
  11. Kodolov V.I. Fire retardants for polymer materials. Moscow: Khimiya, 1980, 274 p.
  12. Barbotko S.L., Volny O.S., Kirienko O.A., Shurkova E.N. Assessment of fire safety of polymer materials for aviation purposes: state analysis, test methods, development prospects, methodological features. Ed. E.N. Kablov. Moscow: VIAM, 2018, 424 p.
  13. Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. Report XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2016, pp. 25–26.
  14. Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  15. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  16. Barbotko S.L. Ways of providing fire safety of aviation materials. Russian Journal of General Chemistry, 2011, vol. 81, no. 5, pp. 1068–1074.
  17. Flame Retardant Chemicals: Technologies and Global Markets. BCC Research, 2018. 128 p.
  18. Aseeva R.M., Zaikov G.E. Combustion of polymeric materials. Moscow: Khimiya, 1981. 280 p.
  19. Korobeinichev O.P., Trubachev S.A., Joshi A.K. et al. Experimental and numerical studies of downward flame spread over PMMA with and without addition of tri phenyl phosphate. Proceedings of the Combustion Institute. 2020. DOI: 10.1016/j.proci.2020.07.082. Available at: https://www.sciencedirect.com/science/article/abs/pii/S1540748920305320 (accessed: December 12, 2020).
  20. Jayarama K.J.V., Srivatsa K.S., Korobeinichev O.P., Vinu R. Detailed kinetic analysis of slow and fast pyrolysis of poly (methyl methacrylate)-Flame retardant mixtures. Thermochimica Acta, 2020, vol. 687. DOI: 10.1016/j.tca.2020.178545.
  21. Tuzhikov O.I., Khokhlova T.V., Bondarenko S.N. et al. Elastomers and plastics with low combustibility. Volgograd: Volgograd State Tech. University, 2005, 230 p.
  22. Polymer Green Flame Retardant. Ed. C.D. Papaspyrides, P. Kiliaris. Elsevier, 2014, 943 p.
  23. Chemical Weapons Convention Available at: http://www.opcw.org/sites/default/files/documents/CWC/CWC_ru.pdf (accessed: February 10, 2021).
  24. Serkova EA, Zastrogina O. B., Barbotko S. L. Study of the possibility of use of new environmentally friendly organophosphorus flame retardants in the composition of binders for interior fire safety materials. Trudy VIAM, 2019, no. 2 (74), paper no. 03. Available at: http://www.viam-works.ru (accessed: February 10, 2020). DOI: 10.18577/2307-6046-2019-0-2-24-34.
  25. Leonov D.V. Development of polyamide-6 functional purpose modified with oxidized graphite: thesis, Cand. Sc. (Tech.). Saratov: Saratov State Tech. University named Yu.A. Gagarin, 2018, 163 p.
  26. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  27. Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing - the basis of innovations. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  28. Graphene in the form of microparticles in powder. Available at: https://rusgraphene.ru/product-page/graphene-powder (accessed: February 10, 2021).
  29. Wang J., Ma C., Wang P. et al. Ultra-low phosphorus loading to achieve the superior flame retardancy of epoxy resin. Polymer Degradation and Stability, 2018, no. 149, pp. 119–128. DOI: 10.1016/j.polymdegradstab.2018.01.024.
  30. Barbotko S.L., Bochenkov M.M., Volnyj O.S., Korobeinichev O.P., Shmakov A.G. Evaluation of the effectiveness of the fire retardants, promising for the creation of new polymer composite materials intended for aviation techniques. Trudy VIAM, 2021, no. 2 (96), paper no. 03. Available at: http://www.viam-works.ru (accessed: February 24, 2021). DOI: 10.18577 / 2307-6046-2021-0-2-20-29.
  31. Yan W., Zhang M.-Q., Yu J. et al. Synergistic Flame-retardant Effect of Epoxy Resin Combined with Phenethyl-bridged DOPO Derivative and Graphene Nanosheets. Chinese Journal of Polymer Science, 2019, no. 37, pp. 79–88. DOI: 10.1007/s10118-019-2175-6.
  32. State Standard 28157–2018. Plastics. Methods for determination of resistance to combustion. Moscow: Standartinform, 2018, 11 p.
  33. Tests for Flammability of Plastic Materials for Parts in Devices and Appliances: UL 94. Underwriters Laboratories Inc., 2006, 54 p.