Laser technology to remove paint coatings in the process of repair and maintenance of aircraft (review)

Ospennikova O.G., Kozlova A.A., Kozlov I.A.
Ospennikova O.G., Kozlova A.A., Kozlov I.A. Laser technology to remove paint coatings in the process of repair and maintenance of aircraft (review) // Proceedings of VIAM. 2021. No. 4. DOI: 10.18577/2307-6046-2021-0-4-110-123. URL: https://www.viam-works.ru/en/journal/2021/4/9
Keywords
laser, surface cleaning, coating removal, paint coatings, repairing, CO2-laser, Nd:YAG laser, laser cleaning.
Abstract

A number of domestic and foreign publications devoted to research on the possibility of using laser surface treatment technologies for cleaning from dirt, removing paint coatings and preparing the metal surface for subsequent technological operations are considered. The most striking examples of the use of technologies in the foreign aviation industry are given and the high readiness of their implementation in practice is noted. Theoretical information about laser technology is presented and the most progressive directions are highlighted.

Reference list
  1. Kablov E.N. Corrosion or life. Nauka i zhizn, 2012, no. 11, pp. 16–21.
  2. Franchuk G.M., Savchenko V.I. Experience of using aerosol gas-dynamic flows in technological cleaning processes. Kiev: Znanie, 1988, 16 p.
  3. Technology of paints and varnishes: collection of scientific articles. Moscow: LKM-press, 2009, p. 63.
  4. Stoye D., Freytag V. Paints, coatings and solvents. Saint Petersburg: Professiya, 2007, 528 p.
  5. Itsko E.F., Drinberg A.S. Removal of paint and varnish coatings. Moscow: LKM-press, 2010, 116 p.
  6. Agarwala V.S., Rajeshwar K. Paint and coating removal technologies: Past, present and future. NACE – International Corrosion Conference Series. Houston, 2001, paper no. NACE-01577.
  7. Maeno T., Mori K., Ogihara T., Fujita T. Removal of thin oxide scale by ultrasonic cleaning with diluted hydrochloric acid in hot stamping of bare 22MnB5 sheet using resistance heating. Procedia Manufacturing, 2019, vol. 29, pp. 225–231.
  8. Kablov E.N., Semenova L.V., Eskov A.A., Lebedeva T.A. Complex systems of paint and varnish coatings for the protection of metal polymer composite materials, as well as their contact compounds from aggressive factors. Lakokrasochnye materialy i ikh primenenie, 2016, no. 6, pp. 32–35.
  9. Kablov E.N. Innovative development is the most important priority of the state. Metally Evrazii, 2010, no. 2, pp. 6–11.
  10. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  11. Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing – the basis of innovations. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  12. Kablov E.N. The sixth technological order. Science and Life. 2010, no. 4, pp. 2–7.
  13. Shcherbakov I.A. Laser. Great Russian Encyclopedia. Available at: https://bigenc.ru/physics/text/ 4341828 (accessed: January 22, 2021).
  14. Schawlow A.L. Lasers. Science, 1965, vol. 149, no. 3679, pp. 13–22.
  15. Bo Y., Geng A., Xu Z. High average power Q-switched quasi-continue-wave Nd: YAG laser. Acta Physica Sinica, 2006, vol. 55, no. 3, pp. 1171–1175.
  16. Furuta K., Kojima T., Fujikawa S. Diode-pumped 1 kW Q-switched Nd: YAG rod laser with high peak power and high beam quality. Applied Optics, 2005, vol. 44, no. 19, pp. 4119–4122.
  17. Roberts D.E. Pulsed laser coating removal by detachment and ejection. Applied Physics, 2004, vol. 79, no. 4, pp. 1067–1070.
  18. Method of removing rust from metallic objects: pat. US 4368080; filed 10.27.80; publ. 11.01.83.
  19. Method of laser surface cleaning: pat. RU 2538161C2; filed 28.12.12; publ. 10.01.15.
  20. Method of surface cleaning and device for its implementation: pat. RU 2297886; filed 06.06.05; publ. 27.04.07.
  21. Method for cleaning the surface of materials and a device for its implementation: pat. RU 2037342C1; filed 17.09.90; publ. 19.06.95.
  22. Method of surface laser treatment and device for its implementation: pat. RU 2445175C1; filed 28.06.10; publ. 20.03.12.
  23. Method for laser cleaning of metals: pat. RU 2619692C1; filed 24.05.16; publ. 17.05.17.
  24. Method of laser surface cleaning: pat. RU 2668619C1; filed 14.08.17; publ. 10.02.18.
  25. Shastin V.I., Belunnik A.I., Lotsmanov G.S. Removal of paint and varnish coatings by laser radiation. Proceedings of the meeting "Laser technological installations and prospects for their application at the enterprises of the industry". Moscow: NIAT, 1986, p. 3.
  26. Shastin V.I. Removal of highly resistant paint and varnish coatings using laser radiation. Lakokrasochnye materialy i ikh primenenie, 2015, no. 8, pp. 42–46.
  27. Kuang Z., Guo W., Li J. et al. Nanosecond fiber laser paint stripping with suppression of flames and sparks. Journal of Materials Processing Technology, 2019, vol. 266, pp. 474–483.
  28. Jasim H.A., Demir A.G., Previtali B., Taha Z.A. Process development and monitoring in stripping of a highly transparent polymeric paint with ns-pulsed fiber laser. Optics and Laser Technology, 2017, vol. 93, pp. 60–66.
  29. Madhukar Y.K., Mullick S., Shukla D.K. et al. Effect of laser operating mode in paint removal with a fiber laser. Applied Surface Science, 2013, vol. 264, pp. 892–901.
  30. Schmidt M. J. J., Li L., Spencer J. T. An investigation into the feasibility and characteristics of using a 2.5 kW high power diode laser for paint stripping. Journal of Materials Processing Technology, 2003, vol. 138, is. 1-3, pp. 109–115.
  31. Samokhvalov A.A. Laser cleaning of the surface of industrial objects from paint and varnish coatings and contamination: thesis, Cand. Sc. (Tech.). Saint Petersburg, 2013, 107 p.
  32. Smirnov V.N. Development of technology for processing aircraft engine parts. Lazernye tekhnologii, 2016. Available at: http://laser.com.ru/refinement_aviation.html (accessed: January 24, 2021).
  33. Smirnov V.N. Mobile laser modules: solving problems of repair and restoration work in the field conditions of engines. Lazernye tekhnologii, 2016. Available at: http://laser.com.ru/article_mlm.html (accessed: January 24, 2021).
  34. Smirnov V.N. Anti-corrosion treatment of engines. Lazernye tekhnologii, 2016. Available at: http://laser.com.ru/anti.html (accessed: January 24, 2021).
  35. Panych D.S. Application of laser-plasma treatment to remove the corrosion layer in machines and metal structures. Evraziyskiy nauchny zhurnal, 2016, no. 9, pp. 197–199.
  36. Verger R. How to most effectively remove paint from a jet fighter. Pokrytiya segodnya, 2021. Available at: http://coatings-today.com/articles/view/69 (accessed: January 22, 2021).
  37. Schlett J. Laser paint removal takes off in aerospace. Vision Spectra, 2016. Available at: https://www.photonics.com/Articles/Laser_Paint_Removal_Takes_Off_in_Aerospace/a61353 (accessed: January 22, 2021).
  38. Muboyadzhan S.A., Alexandrov D.A., Gorlov D.S. Ion-plasma nanolayer erosion-resistant coatings based on metal carbides and nitrides. Metally, 2010, no. 5, pp. 39–51.
  39. Aleksandrov D.A. The research of wear-resistant coatings based on multicomponent titanium nitrides Trudy VIAM, 2020, no. 4-5 (88), paper no. 07 Available at: http://www.viam-works.ru (accessed: February 01, 2021). DOI: 10.18577/2307-6046-2020-0-45-62-69.
  40. Aleksandrov D.A., Muboyadzhyan S.A., Zhuravleva P.L., Gorlov D.S. Investigation of the effect of surface preparation and ion-assisted deposition on the structure and properties of erosion-resistant ion-plasma coating. Trudy VIAM, 2018, no. 10 (70), paper no. 08. Available at: http://www.viam-works.ru (accessed: February 01, 2021). DOI: 10.18577/2307-6046-2018-0-10-62-73.
  41. Muboyadzhyan S.A., Aleksandrov D.A., Gorlov D.S., Egorova L.P., Bulavinceva E.E. Protective and strengthening ion-plasma coverings for blades and other responsible details of the GTE compressor. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 71–81.
  42. Kablov E.N., Muboyadzhyan S.A. Erosion-resistant coatings for compressor blades of gas turbine engines. Elektrometallurgiya, 2016, no. 10, pp. 23–38.
  43. Nochovnaya N.A., Nikitin Ya.Yu., Grigorenko V.B., Kozlov I.A. Changes in the surface properties of titanium alloy VT20 in the chemical removal of operational carbon pollution. Trudy VIAM, 2017, no. 10 (58), paper no. 05. Available at: http://www.viam-works.ru (accessed: February 01, 2021). DOI: 10.18577/2307-6046-2017-0-10-5-5.
  44. Nochovnaya N.A., Nikitin Ya.Yu. The current state of the question in the field of cleaning of the compressor GTE from operational pollution (review). Trudy VIAM, 2017, no. 3, paper no. 05. Available at: http://www.viam-works.ru (accessed: February 01, 2021). DOI: 10.18577 / 2307-6046-2017-0-3-5-5.
  45. Plankovsky S.I., Golovin I.I., Sirenko F.F. Analysis of existing methods for cleaning the surface of turbine blades in gas turbine engines. Aviatsionno-kosmicheskaya tekhnika i tekhnologiya, 2013, no. 6, pp. 8–14.
  46. Plankovsky S.I., Tsegelnik E.V., Golovin I.I., Melnichuk P.I. Prospects for laser cleaning in the repair of gas turbine engines. Aviatsionno-kosmicheskaya tekhnika i tekhnologiya, 2015, no. 10 (127), pp. 54–57.
  47. Method for cleaning and stripping a gas turbine engine blade by means of a pulsed laser: pat. RU 2604406C2; filed 02.05.12; publ. 10.12.16.
  48. Turner M.W., Crouse P.L., Li L., Smith A.J.E. Investigation into CO2 laser cleaning of titanium alloys for gas-turbine component manufacture. Applied Surface Science, 2006, vol. 252, is. 13, pp. 4798–4802.
  49. State Standard EN 4678–2016. Aerospace series. Welded and brazed products for aerospace structures. Connections of metallic materials, made laser welded. Quality of welded products (as amended). Mosocow: Standartinform, 2017, 38 p.
  50. Li X., Zhang Q., Zhou X. et al. The influence of nanosecond laser pulse energy density for paint removal. Optik, 2018, vol. 156, pp. 841–846.
  51. Veiko V.P., Smirnov V.N., Chirkov A.M., Shakhno E.A. Laser cleaning in mechanical engineering and instrument making. Saint Petersburg: NIU ITMO, 2013, 103 p.
  52. Veiko V.P., Mutin T.Yu., Smirnov V.N. et al. Laser cleaning of metal surfaces: physical processes and application. Izvestiya vysshikh uchebnykh zavedeniy. Priborostroyenie, 2008, vol. 51, no. 4, pp. 30–36.
  53. Levin A. The Quantum Beacon: The History of One of the Most Important Inventions of the 20th Century – the Laser. Populyarnaya mekhanika, 2019. Available at: https://www.popmech.ru/technologies/5466-kvantovyy-svetoch-istoriya-odnogo-iz-samykh-vazhnykh-izobreteniy-xx-veka-lazera (accessed: Febryary 02, 2021).
  54. Schweizer G., Werner L. Industrial 2 kW TEA CO2 laser for paint stripping of aircraft. Proceedings of SPIE, 1994, vol. 2502, pp. 57–62.
  55. Liu K., Garmire E. Paint removal using lasers. Applied Optics, 1995, vol. 34, pp. 4409–4415.
  56. Prinsloo F.J., Heerden S.P.V., Ronander E., Botha L.R. Efficient TEA CO2 laser based coating removal system. Proceedings of SPIE, 2007, vol. 6346, pp. 1–8.
  57. Tsunemi A., Hagiwara K., Saito N., Nagasaka K., Miyamoto Y., Suto O. Complete removal of paint from metal surface by ablation with a TEA CO2 laser. Applied Physics A, 1996, vol. 63, pp. 435–439.
  58. Chen G.X., Kwee T.J., Tan K.P., Choo Y.S., Hong M.H. Laser cleaning of steel for paint removal. Applied Physics A, 2010, vol. 101, pp. 249–253.
  59. Forbes A., Du Preez N.C., Belyi V., Botha L.R. Paint stripping with high power flattened Gaussian beams. Proceedings of SPIE, 2009, vol. 7430, pp. 1–5.
  60. Pantelakis S.G., Kermanidis T.B., Haidemenopoulos G.N. Mechanical 2024 Al alloy specimen behavior subjected to paint stripping by laser radiation and plasma etching. Theoretical and Applied Fracture Mechanics, 1996, vol. 25, pp. 139–146.
  61. Arabgari S., Aghaie M., Radmard S., Nabavi S.H. Thin-disk laser resonator design: The dioptric power variation of thin-disk and the beam quality factor. Optik, 2019, vol. 185, pp. 868–874.
  62. Shayganmanesh M., Beirami R. Evaluation of thermal effects on the beam quality of disk laser with unstable resonator. Optics communications, 2017, vol. 38315, pp. 92–100.
  63. Gavili A., Shayganmanesh M. Thin disk laser with unstable resonator and reduced output coupler. Optics & Laser Technology, 2018, vol. 101, pp. 349–357.
  64. Larionov M. Thin disk lasers. Encyclopedia of modern optics. Second edition. Oxford: Academic Press, 2018, vol. 2, pp. 407–414.
  65. Apollonov V.V. Disk lasers: advantages and prospects. Ekspertny soyuz. Available at: http: //laser.rf/2017/09/15/5383 (accessed: January 28, 2021).
  66. Routering M. Targeted paint removal with a powerful Nd: YAG laser. Photonics, 2010, no. 2, pp. 12–14.
  67. Zhanga Z., Zhang J., Wang Y. et al. Removal of paint layer by layer using a 20 kHz 140 ns quasicontinuous wave laser. Optik, 2018, vol. 174, pp. 46–55.
  68. Brygo F., Dutouquet Ch., Le Guern F. et al. Laser fluence, repetition rate and pulse duration effects on paint ablation. Applied Surface Science, 2006, vol. 252, is. 6, pp. 2131–2138.
  69. Losev V.F., Tsipilev V.P. Laser technologies and equipment: textbook. Tomsk: Publ. House Tomsk Polytech. University, 2008, 148 p.
  70. Delaporte Ph., Gastaud M., Marine W. et al. Dry excimer laser cleaning applied to nuclear decontamination. Applied Surface Science, 2003, vol. 208-209, pp. 298–305.
  71. Vinokhodov A.Yu. Electric-discharge laser and plasma sources of UV and VUV radiation with a high pulse repetition rate: thesis, Cand. Sc. (Phys.-Math.) . Troitsk: RFNC "VNIIEF", 2004, 301 p.
  72. Galantucci L. M., Gravina A., Chita G., Cinquepalmi M. An experimental study of paint-stripping using excimer laser. Polymer and Polymer Composites, 1997, vol. 5, no. 2, pp. 87–94.
  73. Kumar M., Bhargava P., Biswas A.K. et al. Epoxy-paint stripping using TEA CO2 laser: Determination of threshold fluence and the process parameters. Optics & Laser Technology, 2013, vol. 46. P. 29–36.
  74. Beck M., Berger P., Hugel H. The effect of plasma formation on beam focusing in deep penetration welding with CO2 laser. Journal of Physics D: Applied Physics, 1995, vol. 28, pp. 2430-2442.
  75. Panchenko Yu.N., Losev V.F., Puchikin A.V., Yao Jun. TEA CO2 lasers with high output radiation intensity. Izvestiya vysshikh uchebnykh zavedeniy, Fizika, 2013, vol. 56, no. 11, pp. 33–36.
  76. Zhu G., Wang S., Cheng W. et al. Corrosion and wear performance of aircraft skin after laser cleaning. Optics & Laser Technology. 2020, vol. 132, pp. 64-75.
  77. Razab M.K.A.A., Jaafar M.S., Abdullah N.H. et al. Influence of elemental compositions in laser cleaning for automotive coating systems. Journal of Russian laser research, 2016, vol. 37, no. 2, pp. 197–206.
  78. Coutouly J.-F., Deprez P., Breaban F., Longuemard J.-P. Optimization of a paint coating ablation process by CO2 TEA laser: Thermal field modeling and real-time monitoring of the process. Journal of Materials Processing Technology, 2009, vol. 209, is. 17, pp. 5730-5735.
  79. Plankovsky S.I., Tsegelnik E.V., Melnichuk P.I., Lebed V.I. Computational and experimental algorithm for assigning modes of laser removal of paint and varnish coatings. Voprosy proyektirovaniya i proizvodstva konstruktsiy letatelnykh apparatov, 2017, is. 4 (92), pp. 34–41.
  80. Plankovsky S.I., Tsegelnik E.V., Melnichuk P.I., Golovin I.I. On the question of the appointment of modes of laser cleaning of elements of aircraft structures made of aluminum alloys from paint and varnish coatings. Voprosy proyektirovaniya i proizvodstva konstruktsiy letatelnykh apparatov, 2015. is. 4 (84), pp. 105–111.
  81. Plankovsky S.I., Tsegelnik E.V., Melnichuk P.I., Chashchin N.A. Experimental and computational method for determining the limitations of the modes of laser cleaning of parts made of aluminum alloys. Voprosy proyektirovaniya i proizvodstva konstruktsiy letatelnykh apparatov, 2017, is. 3 (91), pp. 61–70.
  82. Han J., Cui X., Wang S. et al. Laser effects based optimal laser parameter identifications for paint removal from metal substrate at 1064 nm: A multi-pulse model. Journal of Modern Optics, 2017, vol. 64, no. 19, p. 1947–1959.
  83. Tsegelnik E.V. Promising directions of application of laser technologies in the aviation industry. Otkrytye informatsionnyye i kompyuternye integrirovannye tekhnologii, 2015, is. 70, pp. 121–129.
  84. Weissling D.H., Wiedmann S.L., Solomon D.P. A Large-Scale Robotic System for Depainting Advanced Fighter Aircraft. SAE International Journal of Aerospace, 2011, vol. 4. Is. 2, pp. 1125–1132.
  85. Blinkov V.V. Application of laser technologies in the aviation industry. LazerInform, 2009, no. 23 (422), pp. 5–9.
  86. Tsegelnik E.V., Melnichuk P.I. Modern approaches to the automation of the processes of laser cleaning of elements of aircraft structures from paint and varnish coatings. AVIA-2015: materials of the XII Intern. scientific and technical conf. Kiev: Nat. Aviation University, 2015, pp. 16.35–16.38.
  87. Tochenov L.A. State and prospects of mechanization of technological processes for cleaning aircraft. Moscow: TsSTI Civil Aviation, 1985, 54 p.
  88. Kremeres D., Radziemski L. Laser-spark emission spectroscopy. Moscow: Tekhnosfera, 2009, 360 p.
  89. Veiko V.P., Volkov S.A., Mutin T.Yu., Smirnov V.N. On the possibility of spectroscopic control of the laser cleaning process. Priborostroenie, 2011, no. 2, pp. 65–68.
  90. Hsu S.-C., Lin J. Removal mechanisms of micro-scale particles by surface wave in laser cleaning. Optics & Laser Technology, 2006, vol. 38, is. 7, pp. 544–551.