Intermetallic compound AlxTi – are promising material for high elevated temperatures (review)

Part 2. The mechanical properties of the intermetallic Al2Ti compound and the effect of alloying
Nochovnaya N.A., Ivanov V.I., Avilochev L.Yu.
Nochovnaya N.A., Ivanov V.I., Avilochev L.Yu. Intermetallic compound AlxTi – are promising material for high elevated temperatures (review). Part 2. The mechanical properties of the intermetallic Al2Ti compound and the effect of alloying // Proceedings of VIAM. 2021. No. 4. DOI: 10.18577/2307-6046-2021-0-4-32-47. URL: https://www.viam-works.ru/en/journal/2021/4/3
Keywords
intermetallic Al2Ti alloys, casting, alloying, heat treatment, phase composition, microstructure, mechanical properties, oxidation.
Abstract

Intermetallide alloys based on the Al2Ti compound are the most promising heat-resistant materials for future energy plants.The review examines the mechanical properties of the Al2Ti Intermetalide, two-phase alloys based on it and the doped niobium alloy. For use at temperatures of up to 950 °С, alloys with phase composition r-Al2Ti + γ-TiAl and platemicrostructure with additional doping of refractory elements are of interest.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E. N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7-8. S. 54–58.
  3. Kablov E.N., Bondarenko Yu.A., Kolodyazhny M.Yu., Surova V.A., Narsky A.R. Prospects for the creation of high-temperature heat-resistant alloys based on refractory matrices and natural composites. Voprosy materialovedeniya, 2020, no. 4 (104), pp. 64–78.
  4. Nochovnaya N.A., Bazyleva O.A., Kablov D.E., Panin P.V. Intermetallic alloys based on titanium and nickel. Ed. E.N. Kablov. Moscow: VIAM, 2018, 318 p.
  5. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  6. Benci J.E., Maa J.C., Feistb T.P. Evaluation of the intermetallic compound Al2Ti for elevated temperature applications. Journal of Materials Science and Engineering A, 1995, vol. 192/193. pp. 38–44.
  7. Umakoshi Y., Nakano T., Ashida K. High Temperature Deformation in Ti–62,5 at. % Al Single Crystals Containing Small Al2Ti-type Precipitates. Journal of Materials Science Forum, 1999, vol. 304–306, pp. 163–168.
  8. Blum M., Jarczyk G., Scholz H., Plier S. et al. Prototype plant for economical mass production of TiAl-vales. Journal of Materials Science and Engineering A, 2002, vol. 329–331, pp. 616–620.
  9. Zhang W.J., Reddy B.V., Deeve S.C. Physical properties of TiAl alloys. Journal of Scripta Materialia, 2001, vol. 45, no. 6, pp. 645–651.
  10. Рininsky M., Drevermann A., Schmitz G.J., Palm M. et al. Casting and properties of Al-rich Ti–Al alloys. Proceedings International Conference «Ti-2007. Science and Technology». The Japan Institute of Metals, 2007, pp. 1059–1062.
  11. Sturm D., Heilmaer M., Saage H., Pininssky M. et al. Creep strength of centrifugally cast Al-rich TiAl alloys. Journal of Materials Science and Engineering A, 2009, vol. 510–511, pp. 373–376.
  12. Ymamoto R., Mizogicni K., Wegman G., Maruyama K. Effect of discontinuour coarsening of lamellae on creep strength of fully lamellar TiAl alloys. Journal of Intermetallics, 1998, vol. 5, pp. 699–702.
  13. Sturm D., Heimaier M., Naumenko K., Rozhar S., Kruger M. Creep deformation characteristics of Al-rich Ti–Al alloys. Proceedings International Conference «Creep and Fracture of Engineering Materials and Structures» (Bed Berneck 4–9 May 2008). The Japan Institute of Metals, 2008. S0921-5093(08)01463-9.
  14. Hayes R.W., Martin P.L. Tension creep wrought single phase γ TiAl. Journal of Acta Metalugica et Materialia, 1995, vol. 43, no. 7, pp. 2761–2772.
  15. Kim S., Cho W., Hong C.P. Creep behavior of cast TiAl based intermetallics. Journal of Materials Science and Technology, 1995, vol. 11, no. 5, pp. 1147–1155.
  16. Jimenez J.A., Carsi M., Frommeyer G., Knipperscher S. et al. The effect microstructure on the creep behavior of theTi–46Al–1Mo–0,2Si alloy. Journal of Intermetallics, 2005, vol. 13, no. 11, pp. 1021–1029.
  17. Sturm D., Heilmaier M., Saage H., Agular J. et al. High temperature creep behavior of Al-rich Ti–Al alloys. Journal of Physics. 2010. Conference Series 240, no. 1, pp. 012084. DOI: 10.1088/1742-6596/240/1/012084.
  18. Sturm D., Heilmaier M., Saage H., Agular J. et al. Creep strength of binary Al62Ti38 alloy. International Journal of Materials Research, 2010, vol. 101, no. 5. Р. 676–679.
  19. Sturm D. Herstellung und Eigenschaften Al-reicher TiAl Legierungen: dis. zur Erlangung des akademischen Grades. Magdeburg: Otto-von-Guericke-Universitat Magdeburg, 2010. 118 s.
  20. Palm M., Zhangl L.C., Stein F., Sauthoff G. Phases and phase equilibria in the Al-rich part of the Al–Ti system above 900 °С. Journal of Intermetallics, 2002, vol. 10, no. 6. Р. 523–540.
  21. Karthikeyan S., Visvanathan G.B. Evaluation of the jogged-screw model of creep in equiexed γ-TiAl: identification of the key substructural parameters. Journal of Acta Materialia, 2004, vol. 52, no. 9, pp. 2577–2589.
  22. Mishin Y., Herzig C. Diffusion in the Ti–Al system. Journal of Acta Materialia, 2000, vol. 48, no. 3, pp. 589–623.
  23. Chakravadhanula V.S.K., Kelm K., Kienle L., Duppel V. et al. TEM studies of the ternary Ti36Al62Nb2 alloy. Material Research Society Symposium Proceeding, 2011, vol. 1295. DOI: 10.1557/opl.2011.181.
  24. Alekseev Е.B., Nochovnaya N.A., Novak A.V., Panin P.V. Wrought intermetallic titanium ortho alloy doped with yttrium Part 1. Research on ingot microstructure and rheological curves plotting. Trudy VIAM, 2018, no. 6 (66), paper no. 02. Available at: http://www.viam-works.ru (accessed: January 14, 2021). DOI: 10.18577/2307-6046-2018-0-6-12-21.
  25. Alexeev Е.B., Nochovnaya N.A., Novak A.V., Panin P.V. Wrought intermetallic titanium ortho alloy doped with yttrium. Part 2. Research on heat treatment effect on rolled slab microstructure and mechanical properties. Trudy VIAM, 2018, no. 12 (72), paper no. 04. Available at: http://www.viam-works.ru (accessed: January 14, 2021). DOI: 10.18577/2307-6046-2018-0-12-37-45.
  26. Novak A.V., Alekseev E.B., Ivanov V.I., Dzunovich D.A. The study of the quenching parameters influence on structure and hardness of orthorhombic titanium aluminide alloy VТI-4. Trudy VIAM, 2018, no. 2, paper no. 05. Available at: http://www.viam-works.ru (accessed: January 14, 2021). DOI: 10.18577/2307-6046-2018-0-2-5-5.