Model for prediction of high temperature durability of castable nickel-base superalloys

Petrushin N.V., Elyutin E.S.
Petrushin N.V., Elyutin E.S. Model for prediction of high temperature durability of castable nickel-base superalloys // Proceedings of VIAM. 2021. No. 4. DOI: 10.18577/2307-6046-2021-0-4-16-31. URL: https://www.viam-works.ru/en/journal/2021/4/2
Keywords
castable nickel-base superalloys, durability in the long-term strength test, solidus temperature, lattice spacing
Abstract

The relationship between the long-term strength and the structural-phase and physico-chemical parameters of castable polycrystalline nickel-based superalloys is considered. A regression model for prediction of the durability at a temperature of 1100 °C and a stress of 80 MPa of the considered class of alloys is proposed. The model takes into account the amount of the γ'-phase, the γ'-solvus and solidus temperatures, γ/γ'-misfit, the lattice spacing of the γ- and γ'-phases, and the atomic mass of the alloy. The reliability of the durability prediction is confirmed by comparison with the experimental results on the long-term strength at temperatures 1000, 1050 and 1100 °C of a number of industrial and experimental castable polycrystalline nickel-based superalloys.

Reference list
  1. Inozemtsev A.A., Koryakovtsev A.S., Lesnikov V.P., Kuznetsov V.P. The role of materials and protective coatings in ensuring the reliability and efficiency of GTD. Transnamer works scientific school. conf. “Scientific ideas S.T. Kischina and modern materials science”. Moscow: VIAM, 2006, pp. 84–87.
  2. Cabers E.N. The materials of the new generation are the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  3. Pollock T.M. Alloy Design for Aircraft Engines. Nature Materials. 2016, vol. 15, pp. 809–815.
  4. Ospennikova O.G. Implementation results of the strategic directions on creation of new generation of heat-resisting cast and wrought alloys and steels for 2012–2016. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 17–23. DOI: 10.18577/2071-9140-2017-0-S-17-23.
  5. Bondarenko Yu.A. Trends in the development of high-temperature metal materials and technologies in the production of modern aircraft gas turbine engines. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 3–11. DOI: 10.18577/2071-9140-2019-0-2-3-11.
  6. Ohno T., Watanabe R., Tanaka K. Development of a Nickel-Base Single Crystal Superalloy Contai Ning Molybdenum by An Alloy Designing Method. Journal of the Iron and Steel Institute of Japan, 1988, vol. 74, is. 11, pp. 133–140. DOI: 10.2355/tetsutohagane1955.74.11_2193.
  7. Harada H., Ohno K., Yamagata T. et al. Phase Calculation and Its Use in Aloy Design Program for Nickel-Base Superaloys. Superalloys 1988. Pennsylvania: The Metallurgical Society, 1988, pp. 733–741.
  8. Shalin R.E., Svetlov I.L., Kachanov E.B., Tolorai V.N., Gavrilin O.S. Single crystals of nickel heat-resistant alloys. Moscow: Mashinostroyenie, 1997. 336 p.
  9. Reed R.C. The Superalloys. Fundamentals and Applications. Cambridge: United Kingdom at University Press, 2006. 372 p.
  10. Cabers E.N., Petrins N.V. Computer method for constructing foundry heat-resistant nickel alloys. Aviacionnye materialy i tehnologii, 2004, no. 1, pp. 3-21.
  11. Logunov A.V. Heat resistant nickel alloys for blades and gas turbine discs. Rybinsk: Gazoturbinnye tekhnologii, 2017, 854 p.
  12. Yokokawa T., Harada H., Kawagishi K. et al. Advanced Alloy Design Program and Improvement of Sixth-Generation Ni-Base Single Crystal Superalloy TMS-238. Superalloys 2020. Pennsylvania: Minerals, Metals & Materials Society, 2020, pp. 122–130.
  13. Mills K.C., Youssef Y.M., Li Z., Su Y. Calculation of Thermophysical Properties of Ni-Based SuperalOlys. ISIJ International, 2006, vol. 46, no. 5, pp. 623–632.
  14. Collins H.E., Quigg R.J., DRENSHFIELD R.L. Development of a Nickel-Base Superalloy Using Statistically Designed Experiments. Transactions of American Society for Metals, 1968, vol. 61, pp. 711–721.
  15. Rtishchev V.V. Estimated methods for predicting the phase composition, structural characteristics and limits of long-term strength of the chemical composition of heat-resistant alloys on a nickel-based basis. Heat resistant and heat-resistant steel and nickel-based alloys. Moscow: Nauka, 1984, pp. 144–150.
  16. Petrushin N.V., Visik E.M., Elyutin E.S. Improvement of the chemical composition and structure of castable nickel-base superalloy with low density. Part 1. Trudy VIAM, 2021, no. 3 (97), paper no. Available at: http://www.viam-works.ru (date of access: March 30, 2021). DOI: 10.18577/2307-6046-2021-0-3-3-15.
  17. Boxtein S.Z., Ginzburg S.S., Kishkin S.T. et al. Autoradiography of the surfaces of the section and the structural stability of alloys. Moscow: Metallurgiya, 1987, 272 p.
  18. Petrushshin N.V., Logunov A.V., Kishkin S.T. et al. Study of patterns of changes in the physicomechanical properties and structural stability of nickel heat-resistant alloys. Aviatsionnyye materialy. Moscow: VIAM, 1983. Is.: Thermophysical studies of heat-resistant alloys and heat-shielding coatings, pp. 17–30.
  19. Logunov A.V., Petrushin N.V., Kuleshova E.A., Dolzhany Yu.M. Forecasting the influence of structural factors on the mechanical properties of heat-resistant alloys. Metallovedeniye i termicheskaya obrabotka metallov, 1981, no. 6, pp. 16–20.
  20. Kishkin S.T., Logunov A.V., Petrushin N.V., Glezer G.M., Kuleshova E.A., Morozova S.G. Scientific bases for doping heat-resistant nickel alloys. Aviation materials. Moscow: VIAM, 1987, is.: Methods for the study of structural materials. pp. 6–18.
  21. Caron P. High γ' solvus new generation nickel-based superalloys for single crystal turbine blade applications. Superalloys 2000. Pennsylvania: Minerals, Metals & Materials Society, 2000, pp. 737–746.
  22. Boxtein B.S., Boxtein S.Z., Zhukhovitsky A.A. Thermodynamics and kinetics of diffusion in solids. Moscow: Metallurgiya, 1974, 280 p.
  23. Physical metal studies: at 3 vols. Ed. R.U. Kan, P.T. Haazen; trans. from English. Moscow: Metallurgiya, 1987, vol. 3: Physico-chemical properties of metals and alloys. 663 p.
  24. Superplays II. Heat resistant materials for aerospace and industrial power plants: in 2 books. Ed. Ch.T. Sims, N.S. Tornoff, U.K. Chagel; trans. from English. Moscow: Metallurgiya, 1995, book 1. 384 p.
  25. Petrushin N.V., Ignatova I.A., Logunov A.V., Samoilov A.I., Razumovsky I.M. The study of the influence of dimensional inconsistency of the parameters of crystalline lattices γ- and γ'-phases on the characteristics of the heat resistance of dispersion-hardening nickel alloys. Izvestiya AN SSSR, metals. 1981, no. 6, pp. 153–159.
  26. Boxtein S.Z., Ignatova I.A., Bolberova E.V., Kishkin S.T., Razumovsky I.M. Effect of inconsistency of phase lattices parameters on diffusion permeability of interfacial boundaries. Fizika metallov i metallovedeniye, 1985, vol. 59, is. 5, pp. 936–942.
  27. Svetlov I.L., Oldakovsky I.V., Petrins N.V., Ignatova I.A. Concentration dependence of lattice periods γ- and γ'-phases of nickel heat-resistant alloys. Metally, 1991, no. 6, pp. 150–157.
  28. Zhang J.x., Murakumo T., Harada H., Koizumi Y. Dependence of Creep Strength On The Interfacial Dislocations in A Fourth Generation SC Superaloy TMS-138. Scripta Materialia, 2003, vol. 48, pp. 287–293.
  29. Koizumi Y., Kobayashi T., Yokokawa T., Zhang J., Osawa M., Harada H., Aoki Y., Arai M. Development of Next-Generation Ni-Base Single Crystal Superalloys. Superalloys 2004, Pennsylvania : Minerals, Metals & Materials Society, 2004, pp. 35–43.
  30. Ignatova I.A., Petrins N.V., Samoilov A.I., Logunov A.V., Kozlova V.S. High-temperature study of structural factors of heat resistance of complexized nickel alloys. Aviation materials. Moscow: VIAM, 1983. is: Thermophysical studies of heat-resistant alloys and heat-shielding coatings, pp. 39–46.
  31. Biermann H., Strehler V., Mughrabi H. High Temperature Measurement of Lattice Parameters and Internal Stresses of A Creep-Deformed Monocrystalline Nickel-Base Superalloy. Metallurgical and Material Transaction, 1996, vol. 27, pp. 1003–1014.
  32. Heckl A., NEUMEIER S., Göken M., Singer R.F. The effect of Re and Ru on γ/γ' Microstructure, γ-Solid Solutions Strength and Creep Strength in Nickel-Base Superaloys. Materials Science and Engineering A, 2011, vol. A528, no. 9, pp. 3435–3444.
  33. Rtishchev V.V. Methods for predicting the structural characteristics and properties of heat-resistant alloys on a nickel basis. Metallovedeniye i termicheskaya obrabotka metallov, 1994, no. 9, pp. 13–20.
  34. Yamagata T., Harada H., Nakazawa S., Yamasaki M. Effect of TA / W Ratio in γ 'Phase on Creep Strength of Nickel-Base Single Crystal Superaloys. Transactions of the Iron and Steel Institute of Japan, 1986, vol. 26, is. 7, pp. 638–642.
  35. Harada H., Yamagata T., Yokokawa T. et al. Computer Analysis on Microstructure and Property of Nickel-Base Single Crystal Superalloys. Proceedings of the Fifth International Conference Held At University College (Swansea, 28 March – 2 April, 1993). Swansea: The Institute of Metals, 1993, pp. 255–264.
  36. Yokokawa T., Harada H., Mory Y. et al. Design of Next Generation Ni-Base Single Crystal Superalloys Containing IR: Towards 1150 °C Temperature Capability. Superalloys 2016. Pennsylvania: Minerals, Metals & Materials Society, 2016, pp. 123–130.
  37. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  38. Spool K.Ya., Sidorov V.V. High-grade foundry alloy on nickel-based brand ZhS6F. Construction and heat-resistant materials for new techniques. Moscow: Nauka, 1978, pp. 31–35.
  39. Peregienidze I.G. Planning an experiment for study of multicomponent systems. Moscow: Nauka, 1976, 390 p.
  40. Kablov E.N. Foundry heat-resistant alloys. Mechanical engineering: Encyclopedia: 40 vols: Mashinostroyeniye, 2001. T. II-3: non-ferrous metals and alloys. Composite materials, pp. 519–552.
  41. Cast blades of gas turbine engines. Alloys, technology, coatings Ed. E.N. Kablov. 2nd ed. Moscow: Nauka, 2006. 632 p.
  42. A method for determining the relative volumetric content of the strengthening γ'-phase in alloys: a.c. No. 687965 USSR; filed 16.05.77; publ. 15.03.92.
  43. Link T., Epishin A., Paulisch M., May T. TOPOGRAPHY OF SEMICOHERENT γ/γ'-Interfaces in Superalloys: Investigation of the formation Mechanism. Materials Science Engineering A, 2011, vol. A528, no. 19-20, pp. 6225–6234.
  44. Petrushin N.V., Logunov A.V., Kovalev A.I. Temperature intervals of dissolving strengthening intermetallic phases in heat-resistant alloys for GTD. Aviation materials. Moscow: VIAM, 1983, is: Thermophysical studies of heat-resistant alloys and heat-shielding coatings, pp. 30–35.
  45. Samojlov A.I., Nazarkin R.M., Moiseeva N.S. Definition miss-fit in fragmental single crystals of nickel hot strength alloys. Trudy VIAM, 2013, no. 5, paper no. 02. Available at: http://www.viam-works.ru (accessed: March 30, 2021).
  46. Arginbaeva E.G., Nazarkin R.M., Shestakov A.V., Karachevtsev F.N. Research of heat treatment influence on structural-phase parameters of intermetallic nickel based alloys. Aviacionnye materialy i tehnologii, 2017, no. 3 (48), pp. 8–13. DOI: 10.18577/2071-9140-2017-0-3-8-13.
  47. Calculation of the parameters of heat-resistant nickel alloys: Certificate of state registration of the program for computer RU 2019661855: filed 28.08.19; opubl. 10.09.19.
  48. Stepnov M.N. Statistical processing of mechanical test results. Moscow: Mashinostroyeniye, 1972, 232 p.
  49. Drayer N., Smith G. Applied Regression Analysis. Moscow: Statistika, 1973, 392 p.
  50. Foundry heat-resistant nickel-based alloy: pat. 2148100 Rus. Federation; filed 18.01.99; opubl. 27.04.00.
  51. Foundry heat-resistant alloy based on nickel: pat. 2153020 Rus. Federation; filed 27.05.99; opubl. 20.07.00.
  52. Foundry heat-powered alloy based on nickel: pat. 2434069 Rus. Federation; filed 05.10.10; opubl. 20.11.11.
  53. Foundry heat-resistant alloy on a nickel basis and a product made of it: pat. 2530932 Rus. Federation; filed 29.10.13; opubl. 20.10.14.