Abstract
A review of scientific and technical literature in the field of hybrid metal composite materials (MMС) based on aluminum alloys is presented. The most widespread at present matrix aluminum alloys and reinforcing components for the manufacture of hybrid MMCs are considered. The main methods of manufacturing MMCs are shown, as well as the effect of matrix aluminum alloys and reinforcing components on the mechanical, thermophysical and tribological properties of hybrid MMCs. A comparison of the characteristics of hybrid MCMs with matrix alloys and MCMs of similar systems is given.
Reference list
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing – the basis of innovations. Krylya Rodiny, 2016, no. 5, pp. 8–18.
- Kablov E.N., Valueva M.I., I.V. Zelenina, Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials. Trudy VIAM, 2020, no. 1, paper no. 07. Available at: http://www.viam-works.ru (accessed: June 2, 2020). DOI: 10.18577/2307-6046-2020-0-1-68-77.
- Imametdinov E.S., Valueva M.I. Сomposites for piston engines (rеview). Aviacionnye materialy i tehnologii, 2020, no. 3 (60), pp. 19–28. DOI: 10.18577/2071-9140-2020-0-3-19-28.
- Karashaev M.M., Bazyleva O.A., Shesta- kov A.V., Ovsepyan S.V. Technological princi-ples for the development of metal composite materials reinforced with oxide and intermetallic particles. Aviacionnye materialy i tehnologii, 2020, no. 3 (60), pp. 29–36. DOI:10.18577/2071-9140-2020-0-3-29-36.
- Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
- Chawla N., Chawla K.K. Metal Matrix Composites. New York: Springer Sience+Business Media, Inc., 2006, pp. 351–379.
- Almangour B. Additive Manufacturing of Emerging Materials. Springer, 2019, 355 p.
- Debroy H.L., Wei J.S., Zuback T. et al. Additive manufacturing of metallic components – Process, structure and properties. Progress in Materials Science, 2018, vol. 92, pp. 112–224.
- Venugopal S., Karikalan L. Microstructure and physical properties of hybrid metal matrix composites AA6061–TiO2–SiC via stir casting techniques. Materials Today: Proceedings, 2020, pp. 2–6. DOI:10.1016/j.matpr.2020.06.462.
- Gowrishankar M.C., Hiremath P., Shettar M. et al. Experimental validity on the casting characteristics of stir cast aluminium composites. Journal of Materials Research and Technology, 2020, vol. 9, is. 3, pp. 3340–3347. DOI: 10.1016/j.jmrt.2020.01.028.
- Oh K.H., Han K.S. Short-fiber/particle hybrid reinforcement: effects on fracture toughness and fatigue crack growth of metal matrix composites. Composites Science and Technology, 2007, vol. 67, is. 7–8, pp. 1719–1726. DOI: 10.1016/j.compscitech.2006.06.020.
- Hu J., Wu G., Zhang Q., Gou H. Mechanical properties and damping capacity of SiCp/TiNif/Al composite with different volume fraction of SiC particle. Composites. Part B: Engineering, 2014, vol. 66, pp. 400–406. DOI: 10.1016/j.compositesb.2014.06.013.
- Lu T.W., Chen W.P., Wang P. et al. Enhanced mechanical properties and thermo-physical properties of 7075Al hybrid composites reinforced by the mixture of Cr particles and SiCp. Journal of Alloys and Compounds, 2018, vol. 735, pp. 1137–1144. DOI: 10.1016/j.jallcom.2017.11.227.
- Liu Y.X., Yang C., Chen W.P. et al. Effects of particle size and properties on the microstructures, mechanical properties, and fracture mechanisms of 7075Al hybrid composites prepared by squeeze casting. Journal of Materials Science, 2014, vol. 49, pp. 7855–7863. DOI: 10.1007/s10853-014-8496-5.
- Chen W., Liu Y., Yang C. et al. (SiCp+Ti)/7075Al hybrid composites with high strength and large plasticity fabricated by squeeze casting. Materials Science and Engineering: A, 2014, vol. 609, pp. 250–254. DOI: 10.1016/j.msea.2014.05.008.
- Shalaby E.A.M., Churyumov A.Y., Solonin A.N., Lotfy A. Preparation and characterization of hybrid A359/(SiC+Si3N4) composites synthesized by stir/squeeze casting techniques. Materials Science and Engineering: A, 2016, vol. 674, pp. 18–24. DOI: 10.1016/j.msea.2016.07.058.
- Ko B.C., Yoo Y.C. The effect of aging treatment on the microstructure and mechanical properties of AA2124 hybrid composites reinforced with both SiC whiskers and SiC particles. Composites Science and Technology, 1999, vol. 59. is. 5. pp. 775–779. DOI: 10.1016/S0266-3538(98)00118-3.
- Pandian V., Kannan S. Processing and preparation of aerospace-grade aluminium hybrid metal matrix composite in a modified stir casting furnace integrated with mechanical supersonic vibration squeeze infiltration method. Materials Today Communications, 2020, vol. 24. DOI: 10.1016/j.mtcomm.2020.101732.
- Ahamad N., Mohammada A., Guptab P. Wear characteristics of Al matrix reinforced with Al2O3-carbon hybrid metal matrix composites. Materials Today: Proceedings, 2020, vol. 33, no. 1, p. 2–6. DOI: 10.1016/j.matpr.2020.05.739.
- Sharma S.S., Jagannath K., Prabhu P.R. et al. Metallography & Bulk Hardness of Artificially Aged Al6061–B4C–SiC Stir Cast Hybrid Composites. Materials Science Forum Submitted, 2016, vol. 880, pp. 140–143. DOI: 10.4028/www.scientific.net/MSF.880.140.
- Kumar J., Singh D., Kalsi N.S. et al. Comparative study on the mechanical, tribological, morphological and structural properties of vortex casting processed, Al–SiC–Cr hybrid metal matrix composites for high strength wear-resistant applications: Fabrication and characterizations. Journal of Materials Research and Technology, 2020, vol. 9, is. 6, pp. 13607–13615. DOI: 10.1016/j.jmrt.2020.10.001.
- Shabani M., Mazahery A. Prediction of wear properties in A356 matrix composite reinforced with B4C particulates. Synthetic Metals, 2011, vol. 161, pp. 1226–1231. DOI: 10.1016/j.synthmet.2011.04.009.
- Bayhan M., Önel K. Optimization of reinforcement content and sliding distance for AlSi7Mg/SiCp composites using response surface methodology. Materials & Design, 2010, vol. 31, is. 6, pp. 3015–3022. DOI: 10.1016/j.matdes.2009.12.049.
- Liu Y.B., Lim S.C., Ray S., Rohatgic P.K. Friction and wear of aluminium-graphite composites: the smearing process of graphite during sliding. Wear, 1992, vol. 159, is. 2, pp. 201–205. DOI: 10.1016/0043-1648(92)90303-P.
- Suresha S., Sridhara B.K. Wear characteristics of hybrid aluminium matrix composites reinforced with graphite and silicon carbide particulates. Composites Science and Technology, 2010, vol. 70, is. 11, pp. 1652–1659. DOI: 10.1016/j.compscitech.2010.06.013.
- Mahdavi S., Akhlaghi F. Effect of SiC content on the processing, compaction behavior, and properties of Al6061/SiC/Gr hybrid composites. Journal of Materials Science, 2011, vol. 46, pp. 1502–1511. DOI: 10.1007/s10853-010-4954-x.