Measurement of thermophysical properties rigid fiber insulation

Zuev A.V., Zarichnyak Yu.P., Barinov D.Y.
Zuev A.V., Zarichnyak Yu.P., Barinov D.Y. Measurement of thermophysical properties rigid fiber insulation // Proceedings of VIAM. 2021. No. 2. DOI: 10.18577/2307-6046-2021-0-2-88-98. URL: https://www.viam-works.ru/en/journal/2021/2/10
Keywords
fiber thermal insulation, measurements, thermal conductivity, thermophysical properties, heat protection material, fly vehicle.
Abstract

Describes a mathematical model for processing the results of measurements of thermal conductivity of highly porous fibrous materials of thermal protection. The results and some methodological features of measuring the thermal conductivity of rigid thermal insulation based on refractory oxide fibers are presented. The possibility of measurements taking into account the anisotropy of properties is investigated. The stiffness of the thermal insulation at the fiber contacts is provided by the binder. Thermal conductivity was measured by the stationary method on cylindrical samples in a wide temperature range from 20 to 1700 °C in various gaseous media.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Armor for «Buran». Materials and technologies of VIAM for the ISS «Energia-Buran». Ed. E.N. Kablov. Moscow: Nauka i zhizn, 2013, 128 p.
  3. Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
  4. Zhitnyuk S.V. Oxygen-free ceramic materials for the space technics (review). Trudy VIAM, 2018, no. 8 (68), paper no. 8. Available at: http://www.viam-works.ru (accessed: December 2, 2020). DOI: 10.18577/2307-6046-2018-0-8-81-88.
  5. Polezhaev Yu.V., Yurevich F.B. Thermal protection. Moscow: Energiya, 1976б 392 p.
  6. Ivakhnenko Yu.A., Baruzdin B.V., Varrik N.M., Maksimov V.G. High-temperature fibrous sealing materials. Aviacionnye materialy i tehnologii, 2017, No. S, pp. 272–289. DOI: 10.18577/2071-9140-2017-0-S-272-289.
  7. Istomin A.V., Kolyshev S.G. Electrostatic method of forming ultrathin fibers of refractory oxides. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 40–46. DOI: 10.18577/2071-9140-2019-0-2-40-46.
  8. Zuev A.V., Prosuntsov P.V. Model of the structure of fibrous thermal insulation materials for the analysis of combined heat transfer processes. Inzhenerno-fizicheskii zhurnal, 2014, vol. 87, no. 6, pp. 1319–1330.
  9. Zuev A.V., Prosuntsov P.V., Mayorova I.A. Computational and experimental study of heat transfer processes in highly porous fibrous materials. Teplovye protsessy v tekhnike, 2014, vol. 6, no. 9, pp. 410–420.
  10. Zuev A.V., Zarichnyak Yu.P., Razmakhov M.G. Prerequisites for the selection of the structure model of highly porous fibrous materials to take into account the influence of technological factors and the calculation of heat transfer. Trudy VIAM, 2019, no. 12 (84), paper no. 12. Available at: http://www.viam-works.ru (accessed: December 2, 2020). DOI: 0.18577/2307-6046-2019-0-12-109-118.
  11. Alifanov O.M., Budnik S.A., Mikhailov V.V., Nenarokomov A.V. Experimental-computing complex for the study of thermophysical properties of heat engineering materials. Teplovye protsessy v tekhnike, 2010, vol. 1, no. 2, pp. 49–60.
  12. Majorova I.A. Mathematical modeling of heat transfer and optimization of multilayer thermal protective system. Aviacionnye materialy i tehnologii, 2013, no. 2, pp. 16–18.
  13. Alifanov O.M., Cherepanov V.V. Prediction of physical properties and identification of models of light highly porous heat-shielding materials. Vestnik MAI, 2010, vol. 16, no. 4, pp. 48–57.
  14. Royzen L.I. An approximate method for solving problems of heat conduction of multilayer bodies. Teplofizika vysokikh temperatur, 1981, vol. 19, no.4, pp. 821–831.
  15. Tikhonov A.N., Samarsky A.A. Equations of mathematical physics. Ed. 5th. Moscow: Nauka, 1977, 736 p.