Application of a complex of ion-plasma technologies to protect the compressor blades of a helicopter gas-turbine engine from erosion wear and fretting

Aleksandrov D.A., Gorlov D.S., Budinovskiy S.A.
Aleksandrov D.A., Gorlov D.S., Budinovskiy S.A. Application of a complex of ion-plasma technologies to protect the compressor blades of a helicopter gas-turbine engine from erosion wear and fretting // Proceedings of VIAM. 2021. No. 2. DOI: 10.18577/2307-6046-2021-0-2-71-80. URL: https://www.viam-works.ru/en/journal/2021/2/8
Keywords
erosion-resistant coating, anti-fretting coating, ion-plasma assisted deposition, nanolayer coating, compressor blade.
Abstract

Describes the application of the technology of applying erosion-resistant and fretting-resistant ion-plasma coatings to protect compressor blades of VT8M-1 alloy from erosion wear and fretting, presents the results of tests of compressor blades for erosion resistance and vibration fatigue, samples of VT8M-1 alloy for fretting wear, multi-cycle fatigue and long-term strength, metallographic and metallophysical studies. It has been established that multilayer coatings TiN/CrN and Ti+TiN increase, respectively, the erosion resistance of the feather and the resistance to fretting wear of the locking part of titanium GTE compressor blades while maintaining their fatigue strength.

Reference list
  1. Muboyadzhyan S.A. Erosion-resistant coatings of metal nitrides and carbides and their plasma-chemical synthesis. Rossiyskiy khimicheskiy zhurnal, 2010, vol. 54, no. 1, pp. 103–109.
  2. Farafonov D.P., Leshchev N.E., Afanasiev-Khody- kin A.N., Artemenko N.I. Abrasive wear-resistant seal materials of the gas turbine engine flow section. Aviacionnye materialy i tehnologii, 2019, No. 3 (56), pp. 67–74. DOI: 10.18577/2071-9140-2019-0-3-67-74.
  3. Dzunovich D.A., Alekseyev E.B., Panin P.V., Lukina E.A., Novak A.V. Structure and properties of sheet semi-finished products from various wrought intermetallic titanium alloys. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 17–25. DOI: 10.18577/2071-9140-2018-0-2-17-25.
  4. Kablov E.N., Nochovnaya N.A., Shiryaev A.A., Davydova E.A. Investigation of structural and phase transformations in metastable β-titanium alloys and effect of cooling rate from homogenization temperature on structure and properties of VT47 alloy. Part 2. Trudy VIAM, 2020, no. 8 (90), paper no. 02. Available at: http://www.viam-works.ru (accessed: November 25, 2020). 10.18577/2307-6046-2020-0-8-11-19.
  5. Muboyadzhyan S.A., Alexandrov D.A., Gorlov D.S. Ion-plasma nanolayer erosion-resistant coatings based on metal carbides and nitrides. Metally, 2010, no. 5, pp. 39–51.
  6. Muboyadzhyan S.A., Gorlov D.S., Shchepilov A.A., Konnova V.I. Study of damping capacity of ion-plasma coatings. Aviacionnye materialy i tehnologii, 2014, no. S5, pp. 67–72. DOI: 10.18577/2071-9140-2014-0-s5-67-72.
  7. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  8. Aleksandrov D.A., Muboyadzhyan S.A., Lutsenko A.N., Zhuravleva P.L. Hardening of the surface of titanium alloys by ion implantation method and ionic modification. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 33–39. DOI: 10.18577/2071-9140-2018-0-2-33-39.
  9. Smyslov A.M., Smyslova M.K., Mukhin V.S. Ion-implantation and vacuum-plasma modification of the surface of the blades of a gas turbine engine compressor. Vestnik Rybinskoy gosudarstvennoy aviatsionnoy tekhnologicheskoy, 2017, no. 1 (40), pp. 133–138.
  10. Smyslov A.M., Bybin A.A., Nevyantseva R.R. Influence of ion implantation and plasma surface treatment on the performance characteristics of heat-resistant nickel alloy. Fizika i khimiya obrabotki materialov, 2007, no. 3, pp. 29–34.
  11. Smyslov A.M., Smyslova M.K., Dubin A.I. Investigation of the effect of complex vacuum ion-plasma treatment on the fatigue resistance of GTE blades with a concentrator. Vestnik USATU, 2016, vol. 20, no. 3 (73), pp. 38–43.
  12. Pogrebnyak A.D., Yakushchenko I.V., Sobol O.V. et al. Influence of residual pressure and ion implantation on the structure, elemental composition and properties of nitrides (TiZrAlYNb) N. Zhurnal tekhnicheskoy fiziki, 2015, vol. 85, no. 8, pp. 72–79.
  13. Karpov D.A., Litunovsky V.N. Plasma-immersion ion implantation (PII): physical foundations, use in technology. Saint Petersburg: NIIEFA, 2009, 62 p.
  14. Grigoriev S.N., Melnik Yu.A., Metel A.S. et al. Immersion ion implantation and nitriding in glow discharge plasma with electrostatic electron confinement. Uprochnyayushchie tekhnologii i pokrytiya, 2010, no. 6, pp. 43–48.
  15. Sutygina A.N., Shulepov I.A. Plasma-immersion ion implantation of aluminum into titanium VT1-0. Prospects for the development of fundamental sciences: collection of articles of XII Int. Conf. Students and Young Scientists. Tomsk: Nat. Research Tomsk Polytechnic. University, 2015, pp. 248–250.
  16. Vorobiev V.L., Bykov P.V., Bystrov S.G. et al. Change in the composition of surface layers of titanium alloy VT6 after ion-beam mixing of aluminum and heat treatment. Khimicheskaya fizika i mezoskopiya, 2013, vol. 15, no.4, pp. 576–581.
  17. Smyslov A.M., Mingazhev A.D., Smyslova M.K., Selivanov K.S., Mingazheva A.D. Nanolayer coating for turbomachine blades made of titanium alloys. Vestnik Ufimskogo gosudarstvennogo aviatsionnogo tekhnicheskogo universiteta, 2011, vol. 15, no.1 (41), pp. 109–112.
  18. Budinovskiy S.A., Kablov E.N., Muboyadzhyan S.A. Application of an analytical model for determining elastic stresses in a multilayer system when solving problems of creating high-temperature heat-resistant coatings for rotor blades of aircraft turbines. Vestnik MGTU im. N.E. Baumana, ser.: Mechanical engineering, 2011, no. SP2, pp. 26–37.
  19. Uchevatkina N.V., Ovchinnikov V.V., Zhdanovich O.A., Sbitnev A.G. Residual stresses in the surface layer of titanium alloy VT6 after ion implantation with a high dose. Zagotovitelnye proizvodstva v mashinostroyenii, 2016, no. 6, pp. 41–46.
  20. Smyslov A.M., Smyslova M.K., Dubin A.I., Sazanov V.P., Pavlov V.F. Investigation of the influence of residual stresses on the fatigue resistance of the blades of a gas turbine engine taking into account fractographic features. Izvestiya vysshikh uchebnykh zavedeniy. Povolzhskiy region. Tekhnicheskiye nauki, 2016, no. 1 (37), pp. 121–130.