Investigation of the strength characteristics dispersion-strengthened metal-ceramic composite material VKM22

Pevchev D.I., Gorbovets M.A., Ryzhkov P.V., Kurbatkina E.I.
Pevchev D.I., Gorbovets M.A., Ryzhkov P.V., Kurbatkina E.I. Investigation of the strength characteristics dispersion-strengthened metal-ceramic composite material VKM22 // Proceedings of VIAM. 2021. No. 2. DOI: 10.18577/2307-6046-2021-0-2-30-38. URL: https://www.viam-works.ru/en/journal/2021/2/4
Keywords
composite material, aluminum alloy, silicon carbide, hardening particles, strength characteristics.
Abstract

In many industries, such as mechanical engineering and aerospace, traditional alloys are being replaced by metal matrix composites (MCM). Compared to unreinforced alloys, MCM is characterized by increased strength and rigidity combined with low density. To calculate the resource of nodes for the safe and reliable operation of new equipment, it is necessary to have a set of calculated values of the MCM strength characteristics, including the characteristics of short-term and long-term strength, low-cycle (LCF) and high-cycle (HCF) fatigue. The work is devoted to the study of the characteristics of short-term and long-term strength, LCF and MCF fatigue of dispersion-strengthened MKM grade VKM22.

Reference list
  1. History of aviation materials science. VIAM – 80 years: years and people. Ed. E.N. Kablov. Moscow: VIAM, 2012, 519 p.
  2. Kablov E.N. Modern materials – the basis of innovative modernization of Russia. Metally Evrazii, 2012, no. 3, pp. 10–15.
  3. Kablov E.N. New generation materials – the basis for innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  4. Kablov E.N. Composites: Today and Tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
  5. Krasnov E.I., Shteinberg A.S., Shavnev A.A., Serpova V.M., Zabin A.N. Research of layered metal composite material of Ti–TiAl3 system. Trudy VIAM, 2016, no. 7, paper no. 03. Available at: http://http www.viam-works.ru (accessed date: September 15, 2020). DOI: 10.18577 / 2307-6046-2016-0-7-3-3.
  6. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  7. Tarasov Yu.M., Antipov V.V. The VIAM new materials – for perspective aviation engineering of production of JSC «OAK». Aviacionnye materialy i tehnologii, 2012, no. 2, pp. 5–6.
  8. Kablov E.N., Shchetanov B.V., Ivahnenko Yu.A., Balinova Yu.A. Perspective reinforcing high-temperature fibers for metal and ceramic composite materials. Trudy VIAM, 2013, no. 2, paper no. 05. Available at: http://www.viam-works.ru (accessed: September 21, 2020).
  9. Kablov E.N., Shchetanov B.V., Grashhenkov D.V., Shavnev A.A., Nyafkin A.N. Metalmatrix composite materials on the basis of Al–SiC. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 373–380.
  10. Shmotin Yu.N., Starkov R.Yu., Danilov D.V., Ospennikova O.G., Lomberg B.S. New materials for the perspective engine of JSC «NPO „Saturn”». Aviacionnye materialy i tehnologii, 2012, no. 2, pp. 6–8.
  11. Berezovskij V.V., Shavnev A.A., Lomov S.B., Kurganova Yu.A. Receiving and the analysis of structure of the disperse strengthened composite materials of Al–SiC system with the different maintenance of the reinforcing phase. Aviacionnye materialy i tehnologii, 2014, no. S6, pp. 17–23. DOI: 10.185577/2071-9140-2014-0-S6-17-23.
  12. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  13. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  14. Kablov E.N., Grashchenkov D.V., Shchetanov B.V., Shavnev A.A., Nyafkin A.N. et al. Metal composite materials based on Al – SiC for power electronics. Mekhanika kompozitsionnykh materialov i konstruktsiy, 2012. T. 18, no. 3, pp. 359–368.
  15. Kablov E.N., Chibirkin V.V., Vdovin S.M. Manufacturing, properties and application of the heat-removing bases from Al–SiC MMK in power electronics and converting equipment. Aviacionnye materialy i tehnologii, 2012, no. 2, pp. 20–22.
  16. Solovyev A.E., Golynets S.A., Khvatsky K.K., Aslanyan I.R. Performing of static tensile tests on Zwick/Roell machines. Trudy VIAM, 2015, no. 8, paper no. 12. Available at: http://viam-works.ru (accessed: October 5, 2020). DOI: 10.18577/2307-6046-2015-0-8-12-12.
  17. Gorbovets M.A., Khodinev I.A., Ryzhkov P.V. Equipment for testing carrying out the strain-controlled low-cycle fatigue. Trudy VIAM, 2018, no. 9 (69), paper no. 06. Available at: http://www.viam-works.ru (accessed: October 5, 2020). DOI: 10.18577/2307-6046-2018-0-9-51-60.
  18. Beletsky V.M., Krivov G.A. Aluminum alloys (composition, properties, technology, application): reference book. Ed. I.N. Friedlander. Kiev: KOMINTECH, 2005, 365 p.
  19. Tham L.M., Gupta M., Cheng L. Effect of limited matrix-reinforcement interfacial reactions on enhancing the mechanical properties of aluminum-silicon carbide compo-sites. Acta Materialia, 2001, vol. 49, no. 16, pp. 3243–3253.
  20. Kablov E.N., Golubovsky E.R. Heat resistance of nickel alloys. Moscow: Mashinostroenie, 1998, 463 p.
  21. Grishina O.I., Shavnev A.A., Serpova V.M. Features of influence of structural parameters on mechanical properties of metallic composite material based on particle-reinforced aluminum alloys by silicon carbide. Aviacionnye materialy i tehnologii, 2014, no. S6, pp. 24–27. DOI:
  22. Pandey V., Chattopadhyay K., Srinivas N. C., Singh V. Role of Ultrasonic Shot Peening on Low Cycle Fatigue Behavior of 7075 Aluminum Alloy. International Journal of Fatigue, 2017. DOI: 10.1016/j.ijfatigue.2017.06.033.
  23. Radetskaya E.M., Makeev Yu.I. Corrosion fatigue of high-strength aluminum alloys. Aviacionnye materialy, 1987, is.: Increasing the strength and reliability of structuresuction materials, pp. 204–214.