Current trends in development of acoustic non-destructive testing methods in aviation industry (review)

Slavin A.V., M.A. Dalin, Dikov I.A., Boychuk A.S., Chertishchev V.Yu.
Slavin A.V., M.A. Dalin, Dikov I.A., Boychuk A.S., Chertishchev V.Yu. Current trends in development of acoustic non-destructive testing methods in aviation industry (review) // Proceedings of VIAM. 2021. No. 12. DOI: 10.18577/2307-6046-2021-0-12-96-106. URL: https://www.viam-works.ru/en/journal/2021/12/11
Keywords
nondestructive testing, ultrasonic testing, acoustic testing, automated ultrasonic testing, probability of defects detection, mathematic simulation of ultrasonic testing.
Abstract

The document includes the below main trends in development of acoustic non-destructive testing methods in aviation industry: automation and enhancement of the sensitivity the testing, development of Procedures for acoustic non-destructive testing methods for products in case of repair and use of products, probabilistic assessment of the outcomes of the ultrasonic non-destructive testing, mathematic simulation of the ultrasonic non-destructive testing, development of the ultrasonic non-destructive testing by applying state-of-the-art technologies, development of the low-frequency acoustic testing methods, development of a Procedure on training of specialists who conduct NDT. The experience of NRC «Kurchatov institute» – VIAM is pointed out to show an example on the implementation of main trends on ultrasonic testing development.

Reference list
  1. Dalin M.A., Generalov A.S., Bojchuk A.S., Lozhkova D.S. Basic development tendencies of acoustic non-destructive control methods. Aviacionnye materialy i tehnologii, 2013, no. 1, pp. 64–69.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Lozhkova D.S. Evaluation of the probability of detecting defects in automated immersion ultrasonic testing of semi-finished products from titanium alloys using mathematical modeling: thesis, Cand. Sc. (Tech.). Moscow, 2018, 197 p.
  4. Guidance circular AP-33.70-1. Methodological materials for the implementation of the requirements for the main engine parts, the resource of which is set in cycles. Moscow: Aviaizdat, 2012, 31 p.
  5. Kablov E.N., Ospennikova O.G., Kudinov I.I., Golovkov A.N., Generalov A.S., Knyazev A.V. Evaluation of the probability of detecting operational defects in aircraft parts made of heat-resistant alloys using flaw detection liquids of domestic and foreign production. Defektoskopiya, 2021, no. 1, pp. 64–71.
  6. Lozhkova D.S. Assessment of the reliability of automated ultrasonic testing of semi-finished products of the main parts of a gas turbine engine made of titanium alloy using a mathematical model. Kontrol. Diagnostics, 2017, no. 12, pp. 54–63.
  7. Chertishchev V.Yu. Development of technologies and means of acoustic impedance control of multilayer honeycomb structures made of polymer composite materials: thesis, Cand. Sc. (Tech.). Moscow, 2020, 180 p.
  8. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Kara-vaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021. no. 1 (62). paper no. 03. Available at: https://journal.viam.ru (accessed: March 11, 2021). DOI: 10.18577/2713-0193-2021-0-1-22-23.
  9. Imametdinov E.S., Valueva M.I. Сomposites for piston engines (rеview). Aviacionnye materialy i tehnologii, 2020, no. 3 (60), pp. 19–28. DOI: 10.18577/2071-9140-2020-0-3-19-28.
  10. Murashov V.V., Generalov A.S. PCM products and multilayer glued structures testing by ultrasonic reflection methods. Aviacionnye materialy i tehnologii, 2017, no. 1 (46), pp. 69–74. DOI: 10.18577/2071-9140-2017-0-1-69-74.
  11. Kablov E.N. New generation materials – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  12. Kablov E.N. Do not fall into technological slavery. Ekspert, 2017, no. 24, pp. 37–42.
  13. Chertishchev V.Yu. The estimation of the probability of defects detection by the acoustic methods, depending on their size in constructions from PCM for output control data in the form of binary. Aviaсionnye materialy i tehnologii, 2018, no. 3, pp. 65–79. DOI: 10.18577/2071-9140-2018-0-3-65-79.
  14. ASTM D5687/D5687M-95. Standard Guide for Preparation of Flat Composite Panels with Processing Guidelines for Specimen Preparation. ASTM International, 2007, 16 p.
  15. Chertishchev V.Yu., Boychuk A.S., Dikov I.A., Yakovleva S.I., Generalov A.S. Determination of the depth of occurrence of defects in multilayer structures made of PCM by acoustic methods by the magnitude of the mechanical impedance. Defektoskopiya, 2018, no. 8, pp. 21–34.
  16. Lozhkova D.S., Krasnov I.S. Experimental studies on the assessment of defectiveness of welded joints of the main parts of a gas turbine engine. Defektoskopiya, 2015, no. 2, pp. 10–16.
  17. State Standard 21120–75. Bars and billets of round and rectangular cross-section. Ultrasonic flaw detection methods. Moscow: Publishing house of standards, 1988, 7 p.
  18. ASTM B594-09. Standard Practice for Ultrasonic Inspection of Aluminum-Alloy Wrought Products for Aerospace Applications. ASTM International, 2009.10 p.
  19. SAE AMS-STD-2154. Inspection, Ultrasonic, Wrought Metals, Process for. SAE International, 1998, 41 p.
  20. SAE AMS2628. Ultrasonic immersion inspection titanium and titanium alloy billet premium grade. SAE International, 2007.28 p. DOI: 10.4271/AMS2628.