Research of the corrosion aggressiveness of strippers of native and foreign production used for removal of paint coatings
Fomina M.A., Zakharov К.Е., Volkov I.A., Ivanov A.L. Research of the corrosion aggressiveness of strippers of native and foreign production used for removal of paint coatings // Proceedings of VIAM. 2021. No. 12. DOI: 10.18577/2307-6046-2021-0-12-73-85. URL: https://www.viam-works.ru/en/journal/2021/12/9
Keywords
painting removers, corrosion aggressiveness, metal materials, aluminum alloys, accelerated tests, paint coatings, pitting, low-cycle fatigue.
Abstract
In this work was explored the removal possibility of strippers by acid, alkaline and organic bases, was explored the corrosion effect of strippers for typical metal materials for aircrafts the aluminium alloys 1163-T, B95-T2, the steel 30HGSA. The fact of the corrosive effect of strippers for metal materials was experimentally substantiated. The negative impact of the several strippers (in the case of their mixing) for the surface of the fragments of the aluminum alloy cladding, and, accordingly, on the resource characteristics (low-cycle fatigue), is studied, using the example of the B95-T2 alloy.
Reference list
- Kablov E.N. Aviation materials science: results and prospects. Vestnik RAN, 2002, vol. 72, no. 1, pp. 3–12.
- Kablov E.N. Materials and chemical technologies for aviation technology. Vestnik RAN, 2012, vol. 82, no. 6, pp. 520–530.
- Kablov E.N. Corrosion or life. Nauka i zhizn, 2012, no. 11, pp. 16–21.
- Nefedov N.I., Semenova L.V., Kuznecova V.A., Vereninova N.P. Paint coatings for protection of metallic and polymer composite materials against aging, corrosion and biodeterioration. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 393–404. DOI: 10.18577/2071-9140-2017-0-S-393-404.
- Kravchenko D.V., Kozlov I.A., Nikiforov A.A. Methods for preparing the surface of aluminum alloys for electroplating (review). Trudy VIAM, 2021, no. 6 (100), paper no. 09. Available at: http://www.viam-works.ru (accessed: August 16, 2021). DOI: 10.18577/2307-6046-2021-0-6-82-99.
- Kovrizhkina N.A., Kuznetsova V.A., Kozlov I.A., Vdovin A.I., Silaeva A.A.. Influence of silicate fillers on operational properties of coatings based on protective polymeric pastes with the lowered content of strontium chromate. Trudy VIAM, 2020, no. 4-5 (88), paper no. 09. Available at: http://www.viam-works.ru (accessed: August 16, 2021). DOI: 10.18577/2307-6046-2020-0-45-80-88.
- Kravchenko N.G., Kozlov I.A., Shchekin V.K., Efimova E.A. Cleaning chemical compositions for aircraft engines (review). Trudy VIAM, 2021, no. 1 (95), paper no. 11. Available at: http://www.viam-works.ru (accessed: August 16, 2021). DOI: 10.18577/2307-6046-2021-0-1-105-113.
- Kuznetsova V.A., Deev I.S., Semenova L.V. Influence of modification of epoxy film-forming compositions on their phase microstructure and adgesion to aluminium alloy. Aviacionnye materialy i tehnologii, 2016, no. 1 (40), pp. 72–78. DOI: 10.18577/2071-9140-2016-0-1-72-78.
- Semenova L.V., Novikova T.A., Nefedov N.I. Study of removing ability of removers for paint systems removal. Aviacionnye materialy i tehnologii, 2017, no. 1 (46), pp. 32–37. DOI: 10.18577 / 2071-9140-2017-0-1-32-37.
- Wolf K., Krincher R., Ermalovich J. Laser Strip: A Portable Hand-held Laser Stripping Device for Reducing VOC, Toxic and Particulate Emissions. Report under Innovative Clean Air Technologies grant number 06-010 from the California Air Resources Boar Institute for Research and Technical Assistance. IRTA, California, 2009, pp. 4–11.
- Merati A., Yanishevsky M., Bombardier Y. Effect of Alternative Paint Stripping Processes on the Fatigue Performance of Aluminum Alloys-Atmospheric Plasma De-painting. Springer, 2019, pp. 589–599.
- Ospennikova O.G., Kozlova A.A., Kozlov I.A. Laser technology to remove paint coatings in the process of repair and maintenance of aircraft (review). Trudy VIAM, 2021, no. 4 (98), paper no. 09. Available at: http://www.viam-works.ru (accessed: August 16, 2021). DOI: 10/18577/2307-6046-2021-0-4-110-123.
- Composition for removing paint and varnish coatings from external metal surfaces: US Pat. 2686928C1 Rus. Federation, no. 2018133349; filed 20.09.18; publ. 06.05.19.
- Uang S.N., Shih T.S., Chang C.H. et al. Exposure assessment of organic solvents for aircraft paint stripping and spraying workers. Science of the Total Environment, 2006, no. 356, pp. 38–44.
- Demin S.A., Petrova A.P., Kozlov I.A., Nikiforov N.N. Heat-resistant composite coating for corrosion protection of steel parts. Modern achievements in the field of creating promising light alloys and coatings for aviation and space technology. Sat. report All-Russian scientific and technical conference. Moscow: VIAM, 2021, pp. 9–11.
- Vinogradov S.S., Nikiforov A.A., Demin S.A., Chesnokov D.V. Protection against corrosion of carbon steel. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 242–263. DOI: 10.18577/2071-9140-2017-0-S-242-263.
- Kablov E.N., Startsev O.V., Medvedev I.M. Review of international experience on corrosion and corrosion protection. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
- Itsko E.F. Removal of paint and varnish coatings. Leningrad: Khimiya, 1991, 96 p.
- Newman P. Peroxide-Activated paint removers in Aerospace application. Metal Finishing, 2004, no. 3, pp. 6–11.
- Kablov E.N. Materials for aerospace technology. Vse materialy. Entsiklopedicheskiy spravochnik, 2007, no. 5, pp. 7–27.
- Tkachenko E.A., Senatorova O.G., Milevskaya T.V., Ivanov A.L. Influence of grain size on the complex of properties of cladding clad cold-rolled sheets from base alloys 1163 and V95pch. Tsvetnyye metally, 2013, no. 9, pp. 57–63.
- Lutsenko A.N., Grinevich A.V., Skripachev S.Yu., Bakanov A.V. On the issue of determining the design characteristics of aviation metallic materials taking into account the effect of a corrosive environment. Voprosy materialovedeniya, 2017, no. 4, pp. 169–182. DOI: 10.22349/1994-6716-2017-92-4-169-182.
- Nesterenko B.G. Experimental study of the degradation of strength the accuracy of aircraft structures. Nauchnyy vestnik Moskovskogo gosudarstvennogo universiteta grazhdanskoy aviatsii, 2010, no. 153, pp. 146–149.