The effect of atmospheric pressure plasma on the strength of an adhesive bond based on CFPR

Barannikov A.A., Satdinov R.A., Veshkin E.A, Kurshev E.V.
Barannikov A.A., Satdinov R.A., Veshkin E.A, Kurshev E.V. The effect of atmospheric pressure plasma on the strength of an adhesive bond based on CFPR // Proceedings of VIAM. 2021. No. 12. DOI: 10.18577/2307-6046-2021-0-12-47-54. URL: https://www.viam-works.ru/en/journal/2021/12/6
Keywords
adhesion, contact angle, surface free energy, work of adhesion, carbon fiber reinforced plastic, adhesive shear.
Abstract

The article notes the results of studying the surface of VKU-30K.UMT49 carbon fiber-reinforced plastic without and with its treatment with atmospheric pressure plasma (APP), which is one of the most advanced methods of surface preparation for various adhesion processes, based on the study of the phenomenon of wetting and the theory of adhesion. The results of the effect of APP on the strength of an adhesive bond based on VKU-30K.UMT49 carbon fiber-reinforced plastic, the roughness of the surface of the carbon fiber and its microstructure, the results of the free energy of the surface and its components and the work of adhesion according to the method of Owens–Wendt–Rabel–Kaelble were obtained.

Reference list
  1. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technological development of Russia in the context of achieving national goals: problems and solutions. Innovatsii, 2020, no. 6 (260), pp. 3-16.
  2. Kablov E.N. New Generation Materials and Technologies for their Digital Processing. Herald of the Russian Academy of Sciences, 2020, vol. 90, no. 2, pp. 225-228.
  3. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7-8, pp. 54–58.
  4. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  5. Kablov E.N. New generation materials - the basis of innovation, technological leadership and national security of Russia. Intellekt & Tekhnologii, 2016, no. 2, pp. 41–46.
  6. Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing - the basis of innovation. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  7. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  8. Timoshkov P.N., Khrulkov A.V., Usacheva M.N., Purvin K.E. Technological features of the manufacture of thick-walled parts of the PCM (review). Trudy VIAM, 2019, no. 3 (75), paper no. 07. Available at: http://viam-works.ru (accessed: April 13, 2021). DOI: 10.18577/2307-6046-2019-0-3-61-67.
  9. Barannikov A.A., Postnov V.I., Veshkin E.A., Strelnikov S.V. On the role of fiberglass surface preparation for gluing. Klei. Germetiki. Tekhnologii, 2019, no. 6, pp. 19–27.
  10. Barannikov A.A., Рostnov V.I., Veshkin E.A., Starostina I.V. Link between the energy characteristics of the surface of fiberglass of the VPS-53К brand and the strength of the adhesive joint based on it. Trudy VIAM, 2020, no. 10 (92), paper no. 05. Available at: http://www.viam-works.ru (accessed: April 04, 20). DOI: 10.18577/2307-6046-2020-0-10-40-50.
  11. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  12. Williams T.S., Yu H., Hicks R.F. Atmospheric pressure plasma activation of polymers and composites for adhesive bonding: A Critical Review. Reviews of Adhesion and Adhesives, 2013, vol. 1, no. 1, pp. 46–87. DOI: 10.7569/RAA.2013.097302.
  13. Serrano J.S. Surface modifications of composite materials by atmospheric pressure plasma treatment: PhD Thesis. Madrid: Universidad Rey Juan Carlos, 2011.302 p. Available at: https://eciencia.urjc.es/bitstream/10115/11379/1/Thesis_June%202011%20JSS-SLU-AUF_v5.pdf (accessed: April 04, 2021).
  14. Gleich H. Zusammenhang zwischen Oberflächenenergie und Adhäsionsvermögen von Polymer werkstoffen am Beispiel von PP und PBT und deren Beeinflussung durch die Niederdruck-Plasmatechnologie: dis. Universtät Duisburg-Essen, 2004, 103 p. Available at: https://duepublico2.unidue.de/servlets/MCRFileNodeServlet/duepublico_derivate_00005593/gleichdiss.pdf (accessed: April 04, 2021).
  15. Rodríguez B.N. Pre-Treatment for adhesive bonding of aerospace composite components: PhM Thesis. London: Brunel University, 2016, 133 p. Available at: https://bura.brunel.ac.uk/bitstream/2438/14669/1/FulltextThesis.pdf (accessed: April 04, 2021).
  16. Al-Maliki H.L.R. Adhesive and tribological behavior of cold atmospheric-treated polymer surfaces: PhD plasma Dissertation. Gödöllő: Szent István University, 2018, 115 p. Available at: https://szie.hu/sites/default/files/hayder_lateef_dissertation.pdf (accessed: April 04, 2021).
  17. Lisco F., Shaw A., Wright A. et al. Atmospheric-pressure plasma surface activation for solution processed photovoltaic devices. Solar Energy, 2017, vol. 146, pp. 287–297.
  18. Kostova K.G., Nishimea T.M.C., Castroa A.H.R. et al. Surface modification of polymeric materials by cold atmospheric plasma jet. Applied Surface Science, 2014, vol. 314, pp. 367–375.
  19. Akiyama H., Hasegawa K., Sekigawa T., Yamazaki N. Atmospheric pressure plasma treatment for composites bonding. Mitsubishi Heavy Industries Technical Review, 2018, vol. 55, no. 2, pp. 1–5.
  20. Lucchetta G. Experimental analysis of atmospheric plasma treatment and resin optimization for adhesive bonding of carbon fiber/epoxy composites. Available at: http://tesi.cab.unipd.it/ 48832/1/Tesi_ANTONELLO_Julien.pdf (accessed: April 04, 2021).
  21. Barannikov A.A., Veshkin E.A., Postnov V.I., Semenichev V.V. Structural studies of adhesive joints of VPS-53K fiberglass sheets treated with atmospheric pressure plasma. Klei. Germetiki. Tekhnologii, 2020, no. 3, pp. 27–33. DOI: 10.31044/1813-7008-2020-0-3-27-33.
  22. Bogdanova Yu.G. Adhesion and its role in ensuring the strength of polymer composites: textbook. allowance. Moscow: Moscow State University named after M.V. Lomonosov, 2010, 68 p.
  23. Kraus E. Increasing the strength of adhesive joints of polymer materials by laser and plasma surface treatment: dis. ... Cand. tech. sciences. Kazan: KNITU, 2017, 184 p. Available at: http://www.kstu.ru/servlet/contentblob?id=146076 (accessed: April 04, 2021).
  24. Danchenko Yu.M. Regulation of free surface energy of epoxy polymer materials using mineral fillers. Polimernye materialy i tekhnologii, 2017, vol. 3, no. 2, pp. 56–63.
  25. Langer M., Otto D. Methods for studying the surface characteristics of polymers after plasma treatment. Comparative analysis. Analiz i kontrol: tekhnologii, pribory, resheniya, 2018, no. 2 (39), pp. 2–7.
  26. Operating manual OCA 15EC: Version 1.0; English; Valid as of firmware version 10.27, and SCA software version 4.4.1 Build 1046. Data Physics Instruments GmbH. Available at: https://vdocuments.site/manual-sca20-u.html (accessed: April 15, 2021).
  27. Thomsen F. Practical Contact Angle Measurement (5). Custom-made models: from contact angle to surface free energy. Available at: https://warwick.ac.uk/fac/cross_fac/sciencecity/programmes/internal/themes/am2/ booking/dropshapeanalyser/practical_contact_angle_measurement_5.pdf (accessed: April 15, 2021).
  28. Isaev A.Yu., Rubtsova E.V., Kotova E.V., Sutyagin M.N. Research of properties of glues and glue binding, made with use of modern domestic component base. Trudy VIAM, 2020, no. 3 (87), paper no. 05. Available at: http://www.viam-works.ru (accessed: April 13, 2021). DOI: 10.18577/2307-6046-2021-0-3-58-67.