Investigation of the features of the decomposition of a solid solution during aging of alloys of the Al–Mg–Si–Cu system

Sbitneva S.V., Lukinа E.A., Zaysev D.V.
Sbitneva S.V., Lukinа E.A., Zaysev D.V. Investigation of the features of the decomposition of a solid solution during aging of alloys of the Al–Mg–Si–Cu system // Proceedings of VIAM. 2021. No. 12. DOI: 10.18577/2307-6046-2021-0-12-14-20. URL: https://www.viam-works.ru/en/journal/2021/12/2
Abstract

In this work, the samples of alloy 6013 of the Al–Mg–Si–Cu system after low-temperature thermomechanical treatment (LTMT) according to the scheme: quenching → aging → deformation → aging were studied by dark-field methods of transmission electron microscopy. The analysis of the structure of precipitates of hardening phases and dislocation structure in the volume of grains after different degrees of cold hardening of LHMT is carried out. It is shown that LHMT affects the formation of the structure of hardening precipitates, contributing to both heterogeneous nucleation at dislocations and homogeneous nucleation in the bulk of grains, due to the intensification of diffusion processes.

Reference list
  1. Kablov E.N., Dynin N.V., Benarieb I., Shchetinina N.D., Samokhvalov S.V., Nerush S.V. Promising aluminum alloys for brazed structures of aviation technology. Zagotovitelnye proizvodstva v mashinostroyenii, 2021, vol. 19, no. 4, pp. 179–192.
  2. Kablov E.N., Duyunova V.A., Benarieb I., Puchkov Yu.A., Sbitneva S.V. Features of the decomposition of a supercooled solid solution during quenching of sheets from a high-tech alloy V-1341 of the Al – Mg – Si system. Tekhnologiya legkikh splavov, 2020, no. 3, pp. 20–33.
  3. Kablov E.N., Antipov V.V., Chesnokov D.V., Kutyrev A.E. Application of Al–Mg–Si–Cu system aluminum alloy combined anodic dissolution for prognosis of tensile strength loss during natural exposure testing. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 63–73. DOI: 10.18577/2071-9140-2020-0-2-63-73.
  4. Antipov V.V., Klochkova Yu.Yu., Romanenko V.A. Modern aluminum and aluminum-lithium alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 195–211. DOI: 10.18577/2107-9140-2017-0-S-195-211.
  5. Kablov E.N., Belov E.V., Trapeznikov A.V., Leo- nov A.A., Zaitsev D.V. Strengthening features and aging kinetics of high-strength cast aluminum alloy AL4MS based on Al–Si–Cu–Mg system. Aviation materials and technologies, 2021, no. 2 (63), paper no. 03. Available at: http://www.journal.viam.ru (accessed: August 06, 2021). DOI: 10.18577/2713-0193-2021-0-2-24-34.
  6. Sinyavsky V.S., Valkov V.D., Kalinin V.D. Corrosion and protection of aluminum alloys. 2nd ed., add. and rev. Moscow: Metallurgiya, 1986, 368 p.
  7. Benarieb I., Ber L.B., Antipov K.V., Sbitneva S.V. Trends in development of wrought alloys of Al–Mg–Si–(Cu) system. Part 1 (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 14–22. DOI: 10.18577/2071-9140-2019-0-3-14-22.
  8. Kolobnev N.I., Ber L.B., Tsukrov S.L. Heat treatment of wrought aluminum alloys. Moscow: APRAL, 2020, 552 p.
  9. Chuistov K.V. Aging of metal alloys. 2nd ed., add. and rev. Kiev: Akademperiodika NAS of Ukraine, 2003, 567 p.
  10. Zuo L., Ye B., Ding W. Effect of Q-Al5Cu2Mg8Si6 phase on mechanical properties of Al – Si – Cu – Mg alloy at elevated temperature. Materials Science and Engineering: A, 2017, vol. 693, pp. 26–32. DOI: 10.1016/j.msea.2017.03.087.
  11. Sunde J.K., Marioara C.D., Van Helvoort A.T.J., Holmestad R. The evolution of precipitate crystal structures in an Al – Mg – Si– (Cu) alloy studied by a combined HAADF-STEM and SPED approach. Materials Characterization, 2018, vol. 142, pp. 458–469.
  12. Gazizov M., Marioara C. D., Friis J. et al. Unique hybrid precipitate structures forming in an Al – Cu – Mg – Si alloy. Alloys of Compounds, 2020, vol. 826, pp. 1–7.
  13. Sunde J.K., Marioara C.D., Van Helvoort A.T.J., Holmestad R. The evolution of pre-cipitate crystal structures in an Al – Mg – Si– (Cu) alloy studied by a combined HAADF-STEM and SPED approach. Materials Characterization, 2018, vol. 142, pp. 458–469.
  14. Ding L., Jia Z., Nie J.-F. at al. The structural and compositional evolution of precipitats in Al – Mg – Si – Cu alloy. Acta Materialia, 2018, vol. 145, pp. 437–450.
  15. Liu S.D., Zhong Q.M., Zhang X.M., Deng Y.L. TTP diagrams for aluminum alloy 1933. Materials Science and Technology, 2010, vol. 26. DOI: 10.1179/026708309X12459430509256.