Application of new technologies in the production of helicopter main rotor blades
Barannikov A.A., Postnova M.V., Krasheninnikova E.V., Vasyukov A.N. Application of new technologies in the production of helicopter main rotor blades // Proceedings of VIAM. 2021. No. 11. DOI: 10.18577/2307-6046-2021-0-11-91-102. URL: https://www.viam-works.ru/en/journal/2021/11/9
Keywords
fiberglass, kevlar, flaking resistance, helicopter main rotor blade, adhesive joint, atmospheric pressure plasma.
Abstract
The paper considers the use of atmospheric pressure plasma (APP) treatment as a method for surface preparation of fiberglass of the VPS-53K brand in the manufacture of the main rotor blades of a helicopter of the «Mi» family. It was found that APP treatment increases the strength of the «spar–sheathing» adhesive bond (fiberglass grade VPS-53K), and also that there is a decrease in the bond strength in the presence of a temporary gap (one month) between the processing of the APP sheathing and the gluing operation, which requires additional research.
Reference list
- Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. Reports of the XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2016, pp. 25–26.
- Doroshenko N.I., Chursova L.V. Evolution of materials for blades of helicopters. Aviacionnye materialy i tehnologii, 2012, no. 2, pp. 16–18.
- Davydova I.F., Kablov E.N., Kavun N.S. Heat-resistant non-combustible polyimide glass fiber laminates for aircraft and rocket technology. Vse materialy. Entsiklopedicheskiy spravochnik, 2009, no. 7, pp. 2–11.
- Popov Y.O., Kolokolceva T.V., Gusev Y.A., Gromova A.A. Development of the constructive and technological solution for a sheet fibreglass for tail section skins of helicopter rotor blades. Trudy VIAM, 2016, no. 1 (37), paper no. 05. Available at: http://www.viam-works.ru (accessed: November 12, 2020). DOI: 10.18577/2307-6046-2016-0-1-42-49.
- Zhelezina G.F., Voinov S.I., Pletin I.I., Veshkin E.A., Satdinov R.A. Development and production of structural organoplastics for aviation technology. Izvestiya Samarskogo nauchnogo tsentra RAN, 2012, vol. 14, no. 4–2, pp. 411–416.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Popov Yu.O., Kolokoltseva T.V., Khrulkov A.V. The new generation of materials and technologies for helicopter blade spars. Aviacionnye materialy i tehnologii, 2014, no. S2, pp. 5–9. DOI: 10.18577/2071-9140-2014-0-S2-5-9.
- Grebenikov A.G., Dyachenko Yu.V., Kollerov V.V. et al. Design and technological features of the bearing surfaces of a helicopter made of polymer composite materials. Otkrytye informatsionnye i kompyuternyye integrirovannye tekhnologii, 2019, no. 84, pp. 4–49.
- Zavalov O.A., Basharov E.A. Methodical instructions for the laboratory work "Design of rotor blades and tail rotor blades". Available at: http://elibrary.mai.ru/MegaPro/Download/ ToView/15843?idb=NewMAI2014 (accessed: July 12, 2021).
- Slyusar B.N., Fleck M.B., Goldberg E.S. et al. Helicopter technology. Technology for the production of helicopter blades and aircraft structures from polymer composite materials. Rostov-on-Don: Publishing house of the SSC RAS, 2013, 230 p.
- Topolev V.V. Design and operation of the Mi-171 helicopter. Available at: http://78.29.20.90/dw/lib/exe/fetch.php/ps:dikihvf:discip:mi-171_bortmexaniki_.pdf (accessed: July 12, 2021).
- Doroshenko N.I. Application of PCM in the design of helicopter propeller blades. Available at: https://conf.viam.ru/sites/default/files/uploads/proceedings/1234.pdf (accessed: July 12, 2021).
- Zavalov O.A. Helicopter main and tail rotor design. Available at: http://www.kaf102.mai.ru/bibl_files/L_20.pdf (accessed: July 12, 2021).
- Sokhan O. N., Skulkov D. D. Hubs and blades of helicopter main and tail rotor blades: method. instructions for laboratory work. Available at: https://kaf102.mai.ru/bibl_files/L_06.pdf (accessed: July 12, 2021).
- Ivchin V.A., Samsonov K.Yu. Results of the first stage of flight tests of the helicopter – flying laboratory MI-171A2. Nauchnyy vestnik MGTU GA, 2014, no. 200, pp. 63–69.
- Zhelezina G.F. Features of destruction organoplastikov at shock influences. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 272–277.
- Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Climatic aging of composite materials for aviation purposes. I. Mechanisms of aging. Deformatsiya i razrusheniye materialov, 2010, no. 11, pp. 19–27.
- Startsev V.O., Molokov M.V., Postnov V.I., Starostina I.V. Assessment of the influence of climatic impact on the properties of fiberglass grade VPS-53K. Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk, 2017, vol. 19, no. 4 (2), pp. 220–228.
- Postnov V.I., Pletin I.I., Veshkin E.A., Starostina I.V., Strelnikov S.V. Technological features of the production of thin-sheet skins of helicopter blades from structural fiberglass VPS-53K. Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk, 2016, vol. 18, no. 4 (3), pp. 619–627.
- Lukina N.F., Dementeva L.A., Petrova A.P., Anihovskaya L.I. Gluing materials in the design of blades of helicopters. Trudy VIAM, 2016, no. 7, paper no. 07. Available at: http://www.viam-works.ru (accessed: July 12, 2021). DOI: 10.18577/2307-6046-2016-0-7-7-7.
- Barannikov A.A., Postnov V.I., Veshkin E.A., Strelnikov S.V. The role of fiberglass surface preparation for gluing. Klei. Germetiki. Tekhnologii, 2019, no. 6, pp. 19–27. DOI: 10.31044/1813-7008-2019-0-6-19-27.
- Barannikov A.A., Veshkin E.A., Postnov V.I., Semenichev V.V. Structural studies of adhesive joints of VPS-53K fiberglass sheets treated with atmospheric pressure plasma. Klei. Germetiki. Tekhnologii, 2020, no. 3, pp. 27–33. DOI: 10.31044/1813-7008-2020-0-3-27-33.
- Barannikov A.A., Рostnov V.I., Veshkin E.A., Starostina I.V. Link between the energy characteristics of the surface of fiberglass of the VPS-53К brand and the strength of the adhesive joint based on it. Trudy VIAM, 2020, no. 10 (92), paper no. 05. Available at: http://www.viam-works.ru (accessed: November 12, 2020). DOI: 10.18577/2307-6046-2020-0-10-40-50.
- Tracey A.C. Effect of Atmospheric Pressure Plasma Treatment on Surface Characteristics and Adhesive Bond Quality of Peel Ply Prepared Composites. Available at: https://digital.lib.washington.edu/researchworks/handle/1773/27522 (accessed: November 12, 2020).
- Takeda T., Yasuoka T., Hoshi H. et al. Effectiveness of flame-based surface treatment for adhesive bonding of carbon fiber reinforced epoxy matrix composites. Composites. Part A: Applied Science and Manufacturing, 2019, vol. 119, pp. 30–37.
- Zaldivar R.J., Nokes J., Steckel G.L. et al. The Effect of Atmospheric Plasma Treatment on the Chemistry, Morphology and Resultant Bonding Behavior of a Pan-Based Carbon Fiber-Reinforced Epoxy Composite. Journal of Composite Materials, 2009, vol. 44, is. 2, pp. 137–156. DOI: 10.1177/0021998309345343.
- Dighton C., Rezai A., Ogin S.L., Watts J.F. Atmospheric plasma treatment of CFRP composites to enhance structural bonding investigated using surface analytical techniques. International Journal of Adhesion and Adhesives. 2019, vol. 91, pp. 142–149. DOI: 10.1016/j.ijadhadh.2019.03.010.
- Zaldivar R.J., Steckel G.L, Morgan B.A. et al. Bonding Optimization on Composite Surfaces using Atmospheric Plasma Treatment. Journal of Adhesion Science and Technology, 2012, vol. 26, is. 1–3, pp. 381–401.
- Hansen W. Plasma for Aviation and Aerospace Industries. Available at: https://www.plasmatreat.com/ downloads/english/15-04_IST_aerospace.pdf (accessed: July 12, 2021).
- Langer M., Otto D. Methods for studying the surface characteristics of polymers after plasma treatment. Comparative analysis. Analiz i kontrol: tekhnologii, pribory, resheniya, 2018, no. 2 (39). S. 2-7.
- Williams T., Yu H., Hicks R. Atmospheric pressure plasma activation of polymers and composites for adhesive bonding: A Critical Review. Reviews of Adhesion and Adhesives, 2013, vol. 1, no. 1, pp. 46–87. DOI: 10.7569/RAA.2013.097302.
- Serrano J.S. Surface modifications of composite materials by atmospheric pressure plasma treatment: PhD-Thesis. Madrid: Universidad Rey Juan Carlos, 2011. 302 p. Available at: https://eciencia.urjc.es/bitstream/10115/11379/1/Thesis_June%202011%20JSS-SLU-AUF_v5.pdf (accessed: July 12, 2021).
- Gleich H. Zusammenhang zwischen Oberflächenenergie und Adhäsionsvermögen von Polymer werkstoffen am Beispiel von PP und PBT und deren Beeinflussung durch die Niederdruck-Plasmatechnologie: Dissertation. Universtät Duisburg-Essen, 2004. 103 p. Available at: https://duepublico2.unidue.de/servlets/MCRFileNodeServlet/duepublico_derivate_00005593/gleichdiss.pdf (accessed: April 4, 2021).
- Rodríguez B.N. Pre-Treatment for adhesive bonding of aerospace composite components: PhM-Thesis. London: Brunel University, 2016. 133 p. Available at: https://bura.brunel.ac.uk/bitstream/ 2438/14669/1/FulltextThesis.pdf (accessed: April 4, 2021).
- Al-Maliki H.L.R. Adhesive and tribological behaviour of cold atmospheric plasma-treated polymer surfaces: PhD Dissertation. Gödöllő: Szent István University, 2018. 115 p. Available at: https://szie.hu/sites/default/files/hayder_lateef_dissertation.pdf (accessed: April 4, 2021).
- Lisco F., Shaw A., Wright A. et al. Atmospheric-pressure plasma surface activation for solution processed photovoltaic devices. Solar Energy, 2017, vol. 146, pp. 287–297.
- Kostova K.G., Nishimea T.M.C., Castroa A.H.R. et al. Surface modification of polymeric materials by cold atmospheric plasma jet. Applied Surface Science, 2014, vol. 314, pp. 367–375.
- Akiyama H., Hasegawa K., Sekigawa T., Yamazaki N. Atmospheric pressure plasma treatment for composites bonding. Mitsubishi Heavy Industries Technical Review, 2018, vol. 55, no. 2, pp. 1–5.
- Lucchetta G. Experimental analysis of atmospheric plasma treatment and resin optimization for adhesive bonding of carbon fiber/epoxy composites. Available at: http://tesi.cab.unipd.it/48832/1/Tesi_ANTONELLO_Julien.pdf (accessed: 04.04.2021).
- Konokotin S. P., Yatsyuk I. V., Dobrynin D. A., Azarovsky E. N. Influence of yttrium on the quality of cast billets from alloys based on aluminum. Trudy VIAM, 2020, no. 3 (87), paper no. 03. Available at: http://www.viam-works.ru (accessed: April 13, 2021). DOI: 10.18577/2307-6046-2020-0-3-49-57.