Features of hardening of wide cladding sheets from V95p.ch. aluminum alloy on a continuous heat treatment line

Nechaykina T.A., Oglodkov M.S., Ivanov A.L., Kozlova O.Yu., Yakovlev S.I., Shlyapnikov M.A.
Nechaykina T.A., Oglodkov M.S., Ivanov A.L., Kozlova O.Yu., Yakovlev S.I., Shlyapnikov M.A. Features of hardening of wide cladding sheets from V95p.ch. aluminum alloy on a continuous heat treatment line // Proceedings of VIAM. 2021. No. 11. DOI: 10.18577/2307-6046-2021-0-11-25-33. URL: https://www.viam-works.ru/en/journal/2021/11/3
Keywords
high-strength aluminum alloy V95p.ch., alloys of the Al–Zn–Mg–Cu system, sheathing sheets, wide sheets, structure, mechanical properties, heat treatment, continuous heat treatment line.
Abstract

The features of quenching on the line of continuous heat treatment (CHT) of wide (2400 mm wide) cladding sheets made of high-strength aluminum alloy B95p.ch. are given. The investigations of the structure, corrosion resistance and mechanical properties in tension at different temperatures shown that the technology of heat treatment, including hardening on the CHT line and subsequent artificial two-stage aging according to the T2 modes of sheets, made it possible to provide a uniform characteristic structure, the surface quality and level of mechanical properties necessary for sheathing sheets along the width of the sheet and in different directions of rolling that meets the requirements of the aviation industry standard.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Fridlyander I.N., Senatorova O.G., Tkachenko E.A. High strength alloy systems Al – Zn – Mg – Cu. Mechanical engineering: encyclopedia in 40 vols. Moscow: Mechanical engineering, 2001, vol. II-3: Non-ferrous metals and alloys. Composite metallic materials, pp. 94–128.
  3. Fridlyander IN, Senatorova OG, Tkachenko EA, Molostova II. Development and application of high-strength alloys of the Al – Zn – Mg – Cu system for aerospace engineering. 75 years. Aviation materials. Moscow: VIAM, 2007, pp. 155–163.
  4. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  5. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334. DOI: 10.31857/S0869587320040052.
  6. Fridlander I.N. Aluminum alloys in aircraft in the period 1970–2015. Tekhnologiya legkikh splavov, 2002, no. 4, pp. 12–17.
  7. Kablov E.N. Aviation and Space Materials Science. Vse materialy. Entsiklopedicheskiy spravochnik, 2008, no. 3, pp. 2–14.
  8. Antipov V.V., Klochkova Yu.Yu., Romanenko V.A. Modern aluminum and aluminum-lithium alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 195–211. DOI: 10.18577/2107-9140-2017-0-S-195-211.
  9. Wen K., Fan Yu., Wang G. et al. Aging behavior and precipitate characterization of a high Zn-containing Al – Zn – Mg – Cu alloy with various tempers. Materials & Design, 2016, vol. 101, pp. 16–23.
  10. Oglodkov M.S., Shchetinina N.D., Rudchen- ko A.S., Panteleev M.D. Directions of the develop-ment of promising aluminum-lithium alloys for aero-space engineering (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 19–29. DOI: 10.18577/2071-9140-2020-0-1-19-29.
  11. Tsukrov S.L. Development of lines for continuous heat treatment of strips from aluminum alloys. Tekhnologiya legkikh splavov, 2018, no. 4, pp. 85–91.
  12. Tsukrov S.L. Development of hardening technology for semi-finished products from aluminum alloys: Advanced technologies for light and special alloys. Moscow: Fizmatlit, 2006, pp. 323–338.
  13. Fridlyander I.N. Aluminum wrought structural alloys. Moscow: Metallurgiya, 1979, 208 p.
  14. TR 50-31-70. Homogenization of aluminum alloy ingots. Moscow: VILS, 1970, 24 p.
  15. Fridlyander I.N. Metallurgy of aluminum alloys. Moscow: Nauka, 1985, 238 p.
  16. Belov N.A. Phase composition of industrial and promising aluminum alloys. Moscow: Publ. house MISIS, 2010, 511 p.
  17. Nechaikina T.A., Blinova N.E., Ivanov A.L., Kozlova O.Yu., Kozhekin A.E. Research of the effect of homogenization and quench hardening modes on the structure and mechanical properties of retail rings from alloy В95o.ch.-T2. Trudy VIAM, 2018, no. 10 (70), paper no. 04. Available at: http://www.viam-works.ru (accessed: September 30, 2021). DOI: 10.18577/2307-6046-2018-0-10-27-36.
  18. Beletskiy V.M., Krivov G.A. Aluminum alloys (composition, properties, technology, application): reference book. Ed. I.N. Friedlander. Kiev: Komintech, 2005, pp. 99–100.