Materials based phenolformaldehyde oligomers of resol and novolac tipes (review)

Part 1
Zastrogina O.B., Sinyakov S.D., Serkova E.A.
Zastrogina O.B., Sinyakov S.D., Serkova E.A. Materials based phenolformaldehyde oligomers of resol and novolac tipes (review). Part 1 // Proceedings of VIAM. 2021. No. 10. DOI: 10.18577/2307-6046-2021-0-10-58-66. URL: https://www.viam-works.ru/en/journal/2021/10/6
Keywords
phenol-formaldehyde binders, polymer composites, resole-novolac phenol-formaldehyde oligomers, adhesive compositions, fire-safe materials.
Abstract

Currently, compositions based on a mixture of phenol-formaldehyde resins of the resole and novolac types are of considerable interest. In the first part of the review examples of the use of resole-novolac phenol-formaldehyde resins in adhesive compositions, prepregs, fiberglass plastics and refractory masses are given. The advantages of using resole-novolac compositions in comparison with resole and novolac phenol-formaldehyde oligomers by increasing the physical and mechanical characteristics, fire resistance and fireproof properties are shown. 

Reference list
  1. Kablov E.N. Marketing Materials Science, Aircraft and Industry: Present and Future. Direktor po marketingu i sbytu, 2017, no. 5-6, pp. 40–44.
  2. Kablov E.N. The materials of the new generation are the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2, pp. 16–22.
  3. Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  4. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  5. Satdinov R.A., Veshkin E.A., Postnov V.I., Strelnikov S.V. РСМ low-pressure air ducts in aircraft. Trudy VIAM, 2016, no. 8, paper no. 8. Available at: http://www.viam-works.ru (accessed: July 2, 2021). DOI: 10.18577/2307-6046-2016-0-8-8-8.
  6. Sarychev I.A., Serkova E.A., Khmelnitsky V.V., Zastrogin O.B. Thermosetting binders for aircraft floor panel materials (review). Trudy VIAM, 2019, no. 7 (79), paper no. 03. Available at: http://www.viam-works.ru (accessed: July 2, 2021). DOI: 10.18577/2307-6049-2019-0-7-26-33.
  7. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  8. Polymer composite materials: properties, structure, technology: tutorial. Ed. A.A. Berlin. St. Petersburg: Professiya, 2009, 560 p.
  9. Martin R.V. Chemistry of phenolic resins. Trans. from Engl. Moscow: NIIPM, 1962, 168 p.
  10. Knop A., Shab V. Phenolic resin and materials based on them. Trans. from Engl. Moscow: Khimiya, 1983, 280 p.
  11. Encyclopedia of polymers. Ed. V.A. Kabanov. Moscow: Sovetskaya Entsyklopedia, 1977, vol. 3, pp. 710–720.
  12. Valgin V.D., Sokolov V.A., Polykin G.M., Fanar A.Ya., Gruzdev N.V., Rushkin V.M. Analysis and modeling of adiabatic curing reactions of phenolofood degree resists. Plasticheskiye massy, 1986, no. 10, pp. 5–7.
  13. Phenol Formaldehyde Resins: pat. 763697 AU, no. 200015391; filed 25.11.99; publ. 31.07.03.
  14. Moroz S.A., Proskova L.I., Lykov G.P., Chekina O.V., Radchenko S.I. Phenol formaldehyde binder for the manufacture of shell forms in the production of metal castings. Plasticheskiye massy, 1987, no. 8, pp. 44–46.
  15. Kardashov D.A., Petrova A.P. Polymeric adhesives. Creation and application. Moscow: Khimiya, 1983, 256 p.
  16. Petrova A.P. Adhesive materials: directory. Ed. E.N. Kababov, S.V. Reznichenko. Moscow: Kauchuk and Rezina, 2002, 196 p.
  17. Heat-resistant adhesive composition: pat. 2002786 Rus. Federation, no. 4948096/05; filed 24.06.91; publ. 15.11.93.
  18. Resol-type phenol resin composition and method for curing the same: pat. 7041724 US, no. 09/892457; filed 28.06.01; publ. 09.05.06.
  19. The method of obtaining resolves: pat. 2234519 Rus. Federation, no. 2000127719/04; filed 30.12.99; publ. 20.08.04.
  20. Binding: pat. 2123502 Rus. Federation, no. 97120915/04; filed 01.12.97; publ. 20.12.98.
  21. Berlin A.A., Tellyakhovsky G.I., Aseeva R.M., Belova G.V., Baver A.I. Curing resolon phenol-formaldehyde resins. Plasticheskiye massy, 1969, no. 1, pp. 23–25.
  22. Heat-resistant adhesive composition: pat. 2203917 Rus. Federation, no. 20011225969/04; filed 24.09.01; publ. 10.05.03.
  23. Heat-resistant adhesive composition: pat. 2276679 Rus. Federation, no. 2004134629/04; filed 29.11.04; publ. 20.05.06.
  24. Phenoloformaldehyde binder, prepreg on its basis and the product made of it: pat. 2333922 Rus. Federation, no. 2007107679/04; filed 01.03.07; publ. 20.09.08.
  25. Resin composition, prepreg, and phenolic resin paper base laminate: pat. 268945 CA, no. 20030106882; filed 27.03.03; publ. 21.12.06.
  26. Phenol resin composition, prepreg using the same, and phenol resin laminate with paper base: pat. 2005154592 JP, no. 20030395484; filed 26.11.03; publ. 16.06.05.
  27. Phenol resin composition and phenol resin laminated sheet using the same: pat. 2002249638 JP, no. 20010051390; filed 27.02.01; publ. 08.09.02.
  28. Phenol resin composition, prepreg and paper substrate phenolic resin laminate: pat. 2003176398 JP, no. 20010377994; filed 12.12.01; publ. 24.06.03.
  29. Plastic refractory mass: pat. 2353602 Rus. Federation, no. 2007133981/03; filed 11.09.07; publ. 27.04.09.
  30. Mix for the manufacture of foundry shell forms and rods in heated snap: pat. 1090482 USSR, no. 3566051/22-02; filed 24.03.83; publ. 05.05.84.
  31. Mix for the manufacture of casting rods and forms, mainly shell, in the heated snap: Pat. 1616754 USSR, no. 4669302/27-02; filed 01.02.89; publ. 30.1290.