Investigation of the radio technical characteristics of two-matrix composites based on templates produced by 3D-printing

Sorokin A.E., Beljaev А.А., Kraev I.D., Larionov S.A.
Sorokin A.E., Beljaev А.А., Kraev I.D., Larionov S.A. Investigation of the radio technical characteristics of two-matrix composites based on templates produced by 3D-printing // Proceedings of VIAM. 2021. No. 10. DOI: 10.18577/2307-6046-2021-0-10-45-57. URL: https://www.viam-works.ru/en/journal/2021/10/5
Keywords
carbon nanotubes, template, two-matrix composite, radio-technical properties, thermoplastic, filler, radiotechnical material.
Abstract

In this work, we studied the radio technical characteristics of two-matrix composites made by combining thermoplastic, modified carbon nanotubes (CNTs), templates with a network and figured structure, and polymer compositions based on epoxy resin containing iron powders and CNTs. It has been established that the implemented approach makes it possible to flexibly regulate the radio-technical properties of a two-matrix composite material by varying the structure and size of the cells of the thermoplastic template and the type of filler for the polymer composition based on epoxy resin. 

Reference list
  1. Kablov E.N. Materials and chemical technologies for aviation equipment. Vestnik Rossiyskoy akademii nauk, 2012, vol. 82, no. 6, pp. 520–530.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N. The formation of domestic cosmic materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
  4. Vorshevsky A.A., Grishakov E.S. Ensuring electromagnetic compatibility of marine equipment in the event of electrostatic discharges. Vestnik Astrakhanskogo gosudarstvennogo tekhnicheskogo universiteta, ser.: Marine equipment and technology, 2020, no. 1, pp. 106–114.
  5. Safina R.M., Schkinders M.S. Increasing the noise immunity of the control and access control system when exposed to electrostatic discharge. Zhurnal radioelektroniki, 2020, no. 8, p. 15.
  6. Bodylov A.S., Ryabishin L.A. Electromagnetic compatibility of controlled static converters with a supply network. Materials of the III Volga Sc. Conf. "Instrument-making and automated electric drive in the fuel and energy complex and housing and communal services". Kazan: Publ. house Kazan State Energ. University, 2017, vol. 2, pp. 98–102
  7. Kondrashov S.V., Gunyaeva A.G., Shashkeev K.A., Barinov D.Ya., Soldatov M.A., Shevchenko V.G., Muzafarov A.M. Electrically-conductive hybrid polymer composite materials on the basis of noncovalent functional carbon nanotubes. Trudy VIAM, 2016, no. 2 (38), paper no. 10. Available at: http://www.viam-works.ru (accessed: August 31, 2021). DOI: 10.18577/2307-6046-2016-0-2-10-10.
  8. Bannyj V.A., Ignatenko V.A. The use of polymer radio-absorbing materials in solving the problem of electromagnetic security. Problemy zdorovya i ekologii, 2016. № 3 (49), pp. 9–13.
  9. Devin K.L., Agafonova A.S., Sokolov I.I. Prospects for the use of radio-absorbing materials to ensure electromagnetic compatibility of avionics. Trudy VIAM, 2020, no. 8 (90), paper no. 09. Available at: http://www.viam-works.ru (accessed: December 6, 2020). DOI: 10.18577/2307-6046-2020-0-8-94-100.
  10. Savitsky A.I., Kulikovich D.B., Petrova E.S., Bannik V.A., Gramameva L.I. Study of the possibilities of optical location of radio absorbing materials with a fiber-porous structure. Fundamentalnye problemy radioelektronnogo priborostroeniya, 2017, vol. 17, no. 1, pp. 208–211.
  11. Kraev I.D., Popkov O.V., Shuldeshov E.M., Sorokin A.E., Yurkov G.Yu. Prospects for the use of organosilicon elastomers in the development of modern polymer materials and coatings for various purposes. Trudy VIAM, 2017, no. 12 (60), paper no. 5. Available at: http://www.viam-works.ru (accessed: December 6, 2020). DOI: 10.18577/2307-6046-2017-0-12-5-5.
  12. Shcherbinin S.V., Volchkov S.O., Svalov A.V., Vaskovsky V.O., Kurland G.V. Measuring the parameters of ferromagnetic microwaves in the frequency range from 0.1 to 20 GHz. Materialovedenie, 2019, no. 7, pp. 12–18.
  13. The absorber of electromagnetic waves of the Gigahertz range: pat. 2657018 Rus. Federation, no. 2017126740; filed 26.07.17; publ. 08.06.18.
  14. Bespalova E.E., Kondrashov E.K. Features of updating of a composition of a fireproof material for anechoic chambers when changed of parameters radio absorbing filler. Aviacionnye materialy i tehnologii, 2014, no. 2, pp. 48–52. DOI: 10.18577/2071-9140-2014-0-2-48-52.
  15. Antipova E.A., Bothanogova E.D., Agafonova A.S., Belyaev A.A. Construction radio absorbing material of a three-layer structure with a matching layer. Kompozitnyy mir, 2014. № 3 (54), pp. 32–35.
  16. Ivanova L.N., Borovik I.A., Kohnik D.D., Polikikova A.A., Chistyev V.A., Semenenko V.N. Radio-absorbing coating with high mechanical strength for an antenna platform. Elektronika i mikroelektronika SVCh, 2017. № 1 (1), pp. 55–62.
  17. Roldugin V.I., Rudoy V.M. Absorption of electromagnetic radiation by nanoparticle in a nanocomposite: output for the approximation of Maxwell-harnetta. Kolloidny zhurnal, 2017, vol. 79, no. 6, pp. 778–784.
  18. Prokhorov MA The use of carbon nanomodifiers in composites. Politekhnicheskiy molodezhny zhurnal, 2017. № 7 (12), p. 15.
  19. Kondrashov S.V., Shashkeev K.A., Petrova G.N., Mekalina I.V. Constructional polymer composites with functional properties. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 405–419. DOI: 10.18577/2071-9140-2017-0-S-405-419.
  20. Kondrashov S.V., Shashkeev K.A., Popkov O.V., Solovyanchik L.V. Prospective producing methods for functional structural materials based on CNT-filled nanocomposites (review). Trudy VIAM, 2016, no. 3 (39), paper no. 07. Available at: http://www.viam-works.ru (accessed: May 25, 2021). DOI: 10.18577/2307-6046-2016-0-3-7-7.
  21. Ivahnenko Yu.A., Varrik N.M., Maksimov V.G. The high-temperature radiolucent ceramic composite materials for the radomes and other products of aviation engineering (review). Trudy VIAM, 2016, no. 5, paper no. 05. Available at: http://www.viam-works.ru (accessed: May 25, 2021). DOI: 10.18577/2307-6046-2016-0-5-5-5.
  22. Gorenshev V.N., Kolesov V.V., Fionov A.S., Erichman N.S. Multilayer coatings with variable electrodynamic characteristics based on filled polymer matrices. Zhurnal radioelektroniki, 2016. № 11, pp. 1-16.
  23. Thomassin J.-M., Jerome C., Pardoen T. et al. Polymer/carbon based composites as electromagnetic interference (EMI) shielding materials. Material Science and Engineering. R, 2013, vol. 74, pp. 211–232.
  24. Sandler J.K.W., Kirk J.E., Kinloch I.A. et al. Ultra-low electrical percolation threshold in carbon-nanotube epoxy composites. Polymer, 2003, vol. 44, no. 19, pp. 5893–5899.
  25. Silva V.A., Folgueras L., Candido G.M. et al. Nanostructured Composites Based on Carbon Nanotubes and Epoxy Resin for Use as Radar Absorbing Materials. Materials Research, 2013, vol. 16, no. 6, pp. 1299–1308.
  26. Teber A., Cil K., Yilmaz T. et al. Manganese and Zinc Spinel Ferrites Blended with Multi-Walled Carbon Nanotubes as Microwave Absorbing Materials. Aerospace, 2017, vol. 4, pp. 2–19.
  27. Wang Z., Wu L., Zhou J. et al. Magnetite Nanocrystals on Multiwalled Carbon Nanotubes as a Synergistic Microwave Absorber. Journal of Physical Chemistry, 2013, vol. 117, pp. 5446−5452.
  28. Jia X., Wang J., Zhu X. et al. Synthesis of lightweight and flexible composite aerogel of mesoporous iron oxide threaded by carbon nanotubes for microwave absorption. Journal Alloys and Compounds, 2017, vol. 697, pp. 138–146.
  29. Du Y., Liu W., Qiang R. et al. Shell Thickness-Dependent Microwave Absorption of Core–Shell Fe3O4C Composites. ACS Applied Materials and Interfaces, 2014, vol. 6, pp. 12997–13006.
  30. Andreev A.S., Kazakova М.A., Ishchenko A.V. et al. Magnetic and dielectric properties of carbon nanotubes with embedded cobalt nanoparticles. Carbon, 2017, vol. 114, pp. 39–49.
  31. Subramanian M.A., Li D., Duan N. et al. High Dielectric Constant in ACu3Ti4O12 and ACu3Ti3FeO12 Phases. Journal of Solid State Chemistry, 2000, vol. 151, pp. 323–325.
  32. Kadkhodayan H., Seyed Dorraji M.S., Rasoulifard M.H., Amani-Ghadim A.R. Enhanced microwave absorption property of Fe3O4/CaCu3−xMgxTi4−ySnyO12(0 ≤ x, y ≤ 1)/graphene oxide nanocomposites in epoxy vinyl ester resin. Journal of Material Science, 2017, vol. 28, pp. 12535–12544.
  33. Park S.H., Theilmann P., Yang K. et al. The influence of coiled nanostructure on the enhancement of dielectric constants and electromagnetic shielding efficiency in polymer composites. Applied Physical Letters, 2010, vol. 96, pp. 043115.
  34. Chen H.-T., Padilla W.J., Zide J.M.O. et al. Active terahertz metamaterial devices. Nature, 2006, vol. 444, pp. 597–600.
  35. Wang J., Zhou H., Zhuang J., Liu Q. Influence of spatial configurations on electromagnetic interference shielding of ordered mesoporous carbon/ordered mesoporous silica/silica composites. Scientific Reports, 2013, vol. 3, pp. 32–52.
  36. Krasilnikova O.K., Pogosyan A.S., Serebryakov N. V. et al. Receiving carbon nanomaterials with use of porous aluminum oxide as templata. Fizikokhimiya poverkhnosti zachshita materialov, 2008, no. 44, pp 389–394.
  37. Chizari K., Arjmand M., Liu Z. et al. Three-Dimensional Printing of Highly Conductive Polymer Nanocomposites for EMI Shielding Applications. Material Today Communication, 2017, vol. 11, pp. 112–118.
  38. Postiglione G., Natale G., Griffini G. et al. Conductive 3D microstructures by direct 3D printing of polymer/carbon nanotube nanocomposites via liquid deposition modeling. Composites. Part A, 2015, vol. 76, p. 110–114.
  39. Kennedy Z.C., Christ J.F., Evans K.A. 3D-Printed Poly(vinylidene fluoride) / Carbon Nanotube Composites as a Tuneable, Low-Cost Chemical Vapour Sensing Platform. Nanoscale, 2017, vol. 9, pp. 5458–5467.
  40. Gnanasekaran K., Heijmans T., Van Bennekom S. et al. 3D printing of CNT- and graphene-based conductive polymer nanocomposites by fused deposition modeling. Applied Materials Today, 2017, vol. 9. Р. 21–28.
  41. Gao P., Hunter A., Benavides S. et al. Template Synthesis of Nanostructured Polymeric Membranes by Inkjet Printing. ACS Applied Materials and Interfaces, 2016, vol. 8, pp. 3386–3395.
  42. Sun J., Dawood A., Otter W.J. et al. Microwave characterization of low-loss FDM 3-D printed ABS whis dielectric-filled metal-pipe rectangular waveguide spectroscopy. IEEE ACCESS, 2019, vol. 7. Р. 95455–95486.