Evaluation of vibration-absorbing material based on polyurethane using possibility for a seal

Sagomonova V.A., Dolgopolov S.S., Sorokin A.E., Tselikin V.V.
Sagomonova V.A., Dolgopolov S.S., Sorokin A.E., Tselikin V.V. Evaluation of vibration-absorbing material based on polyurethane using possibility for a seal // Proceedings of VIAM. 2021. No. 10. DOI: 10.18577/2307-6046-2021-0-10-28-35. URL: https://www.viam-works.ru/en/journal/2021/10/3
Keywords
polymer composite material, thermoelastoplastic, vibration damping material, mechanical loss factor, bolt joint, cold flow, wing rib.
Abstract

The article presents the results of a study of the operational properties of the VTP-1V grade material, including cold flow. It was found that the material of the VTP-1V grade hasn’t cold flow and, according to the complex of properties studied in the work, can be recommended as an alternative to layered polymeric composite materials used in the bolted joints of the aircraft wing rib. The possibility of operating VTP-1V in an environment of aggressive liquids was assessed and it was shown that the material is resistant to the effects of TC-1 fuel, including retaining low deformability under prolonged loading.

 

 

Reference list
  1. Kablov E.N. Materials for aerospace technology. Vse materialy. Entsiklopedicheskiy spravochnik, 2007, no. 5, pp. 7–27.
  2. Kablov E.N. The sixth technological order. Nauka i zhizn, 2010, no. 4, pp. 2–7.
  3. Kablov E.N. Chemistry in Aviation Materials Science. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 3–4.
  4. Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing – the basis of innovations. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  5. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  6. Mikhailin Yu.A. Structural polymer composite materials. 2nd ed. Saint Petersburg: Nauchnye osnovy i tekhnologii, 2016, 820 p.
  7. A large reference book of a rubber worker: in 2 partss. Moscow: Tekhinform, 2012. Part 5: Rubber technology: Recipe building and testing. Trans. from English. Ed. J.S. Dick. Saint Petersburg: Scientific bases and technologies, 2010, 620 p.
  8. Eliseev O.A., Krasnov L.L., Zajceva E.I., Savenkova A.V. Development and modifying of elastomeric materials for application in all weather conditions. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 309–314.
  9. Seals and sealing technology: reference book. Ed. A.I. Golubeva, L.A. Kondakov. Moscow: Mashinostroenie, 1986, 464 p.
  10. Fedyukin D.L., Makhlis F.A. Technical and technological properties of rubbers. Moscow: Khimiya, 1985, 240 p.
  11. Naumov I.S., Petrova A.P., Chaikun A.M. Rubber for sealing purposes and reduction of their combustibility. Vse materialy. Entsiklopedicheskiy spravochnik, 2013, no. 5, pp. 28–35.
  12. Naumov I.S. Sealing rubbers of low flammability: thesis, Cand. Sc. (Tech.). M., 2016, 118 p.
  13. Alifanov E.V., Chaykun A.М., Venediktova M.A., Naumov I.S. Specialties of rubber compounds recipes based on ethylene-propylene rubbers and their application in the articles for special purpose (review). Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 51–55. DOI: 10.18577/2071-9140-2015-0-2-51-55.
  14. Semenova S.N., Chaykun A.M., Suleymanov R.R. Ethylene-propylene-diene rubber and its use in rubber materials for special purposes (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 23–30. DOI: 10.18577/2071-9140-2019-0-3-23-30.
  15. Kablov E.N., Shuldeshov E.M., Petrova A.P., Lapteva M.A., Sorokin A.E. Dependence of complex of sound-proof VZMK type material properties on concen-tration of hydrophobizing composition on the basis of organosilicon sealant. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 41–49. DOI: 10.18577/2071-9140-2020-0-2-41-49.
  16. Chaykun A.М., Naumov I.S., Venediktova M.A., Alifanov E.V.. New researches of special purpose fluorosilicone rubber. Aviacionnye materialy i tehnologii, 2016, no. 3 (42), pp. 60–65. DOI: 10.18577/2071-9140-2016-0-3-60-65.
  17. Eliseev O.A., Naumov I.S., Smirnov D.N., Bryk Ya.A. Rubbers, sealants, fireproof and heat-shielding materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 437–451. DOI: 10.18577/2071-9140-2017-0-S-437-451.
  18. Chaikun A.M., Eliseev O.A., Naumov I.S., Venediktova M.A. Features of old-resistant rubbers on the basis on different unvulcanized rubbers. Trudy VIAM, no. 12, paper no. 04. Available at: http://www.viam-works.ru (accessed: April 13, 2021).
  19. Buznik V.M. Modern materials science on the example of fluoropolymers. Ed. V.V. Kozik. Tomsk: Tomsk State University, 2012, vol. 1, 42 p.
  20. Loginov B.A. The amazing world of fluoropolymers. 2nd ed., add. Moscow: Ninth Element, 2009, 168 p.
  21. Sytyy Yu.V., Sagomonova V.A., Yurkov G.Yu., Tselikin V.V. New structural and functional PCMs based on thermoplastics and technologies for their molding. Aviatsionnaya promyshlennost, 2013, no. 2, p. 12.
  22. Sytyj Ju.V., Kisljakova V.I., Sagomonova V.A., Nikolaeva M.F. New multi-layer sealing material VTP-2P. Aviacionnye materialy i tehnologii, 2011, no. 4, pp. 32–34.
  23. Sytyy Yu.V., Kislyakova V.I., Tkachev A.A., Abakumova N.M., Rumyantseva T.V. Vibration-absorbing thermoplastic elastomer VTP-1V. Aviacionnye materialy i tehnologii, 2004, no. 3, pp. 30–31.