Processing of wastes high-temperature heat-protective material
UDC
629.7.023.226
DOI
10.18577/2307-6046-2021-0-1-97-104
Article PDF (Russian)
(703.61 KB)
How to cite
Istomin A.V., Kolyshev S.G. Processing of wastes high-temperature heat-protective material // Proceedings of VIAM. 2021. No. 1. DOI: 10.18577/2307-6046-2021-0-1-97-104. URL: https://www.viam-works.ru/en/journal/2021/1/10
Keywords
production waste, secondary raw material, zirconium oxide, high-temperature fibers, heat treatment, heat-protective materials.
Abstract
The assessment of waste generated during the production of high-temperature fiber insulation. A method of waste processing with a minimum number of technological stages is presented. The structure and mechanical characteristics of the obtained material are estimated. Full-scale tests of the material under the influence of high-enthalpy flame flow of propane-oxygen burner were carried out. The resulting material is suitable for the production of furnace linings, heat-resistant substrates and containers, flame screens.
Reference list
- Kablov E.N. Russia needs new generation materials. Redkiye zemli, 2014, no. 3, pp. 8–13.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Trends and guidelines for innovative development in Russia: collection scientific-information materials. 3rd ed. Moscow: VIAM, 2015. 720 p.
- Shchetanov B.V., Balinova Yu.A., Lyulyukina G.Yu., Soloveva E.P. Structure and properties of continuous polycrystalline fibers α-Al2O3. Aviacionnye materialy i tehnologii, 2012, no. 1, pp. 13–17.
- Ivahnenko Yu.A., Babashov V.G., Zimichev A.M., Tinyakova E.V. High-temperature heatinsulating and heat-protective materials on the basis of fibers of high-melting connections. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 380–386.
- Ivakhnenko Yu.A., Baruzdin B.V., Varrik N.M., Maksimov V.G. High-temperature fibrous sealing materials. Aviacionnye materialy i tehnologii, 2017, No. S, pp. 272–289. DOI: 10.18577/2071-9140-2017-0-S-272-289.
- Grashhenkov D.V., Chursova L.V. Strategy of development of composite and functional materials. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 231–242.
- Istomin A.V., Kolyshev S.G. Electrostatic method of forming ultrathin fibers of refractory oxides. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 40–46. DOI: 10.18577/2071-9140-2019-0-2-40-46.
- Istomin A.V., Bespalov A.S., Babashov V.G. Adding increased resistance to heat and sound insulation of material based on mixture of inorganic and plant fibers. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 74–78. DOI: 10.18577/2071-9140-2018-0-4-74-78.
- Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.S., Sevastianov V.G. High-temperature structural composite materials based on glass and ceramics for advanced aircraft products. Steklo i keramika, 2012, no. 4, pp. 7 – 11.
- Buznik V.M., Kablov E.N., Koshurina A.A. Materials for complex technical devices for arctic applications. Scientific and technical problems of Arctic development. Moscow: Nauka, 2015, pp. 275–285.
- Bespalov A.S., Nefedov N.I., Deev I.S., Kurshev E.V., Lonsky S.L., Buznik V.M. Features of hydrophobization of high-porous ceramic materials using fluoroligomers. Trudy VIAM, 2019, no. 5 (77), paper no. 05. Available at: http://www.viam-works.ru (accessed: September 9, 2020). DOI: 10.18577/2307-6046-2019-0-5-41-51.
- Balinova Yu.A., Shheglova T.M., Lyulyukina G.Yu., Timoshin A.S. Features of formation α-Al2O3 in polycrystalline fibers containing 99% alumina doped with Fe2O3, MgO, SiO2. Trudy VIAM, 2014, no. 3, paper no. 03. Available at: http://www.viam-works.ru (accessed: September 9, 2020). DOI: 10.18577/2307-6046-2014-0-3-3-3.
- Drummers D.A., Serdyukova A.F. Utilization of industrial waste. Molodoy ucheniy, 2017, no. 25, pp. 101-104.
- Potapova E.V. The problem of recycling plastic waste. Izvestiya Baykalskogo gosudarstvennogo universiteta, 2018, vol. 28, no. 4, pp. 535–544.
- Kirin B.S., Klokova A.N. Modern technologies of separation of plastic waste. Uspekhi v khimii i khimicheskoy tekhnologii, 2014, vol. 28, no. 3, pp. 31–33.
- A method of obtaining high-temperature fiber based on aluminum oxide: pat. 2395475 Rus. Federation, no. 2008121990/03; filed 02.06.08; publ. 27.07.10. 18.
- Lukin E.S., Popov N.A., Zdvizhkova N.I. et al. Features of obtaining dense ceramics containing zirconium dioxide. Ogneupory, 1991, no. 9, pp. 5–7.
- Hannink R.H.J., Kelly P.M., Muddle B.C. Transformation toughening in zirconia-containing ceramics. Journal of American Ceramic Society, 2000, vol. 83, no. 3, pp. 461–487.
- Bokhimi X., Garcia-Ruiz A., Xiao T.D. et al. Transformation of yttrium-doped hydrated zirconium into tetragonal and cubic nanocrystalline zirconia. Journal of Solid State Chemistry, 199, vol. 142, pp. 409–418.
- Popov V.V., Petrunin V.F. Investigation of the processes of formation and stability of metastable phases in nanocrystalline ZrO2. Ogneupory i tekhnicheskaya keramika, 2007, no. 8, pp. 8–13.