Research of the biological and corrosion resistance of samples of aluminum alloy after natural tests in the Gelenjik bay

Part 2
Varchenko E.A., Kirichok P.F.
Varchenko E.A., Kirichok P.F. Research of the biological and corrosion resistance of samples of aluminum alloy after natural tests in the Gelenjik bay. Part 2 // Proceedings of VIAM. 2020. No. 9. DOI: 10.18577/2307-6046-2020-0-9-105-114. URL: https://www.viam-works.ru/en/journal/2020/9/12
Keywords
biocorrosion, corrosion in sea water, Gelendzhik bay, full-scale climatic tests.
Abstract

Sea water – one of the most common and corrosive environments, being a finely balanced salt solution containing, among other things, organics, living organisms and dissolved gases, which leads to the multifactorial nature of this exposure condition.

This work is devoted to assessing the productivity of marine biota in 6 monitoring points of the Gelendzhik bay and coastal high seas with a quantitative assessment of fouling and mechanical properties of samples of aluminum alloy AMg6 with and without biofouling during the summer exposure.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Startsev O.V., Medvedev I.M. Review of international experience on corrosion and corrosion protection. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  3. Abramova M.G., Lutsenko A.N., Varchenko E.A. Concerning the aspects of validation of climate resistance of airborne materials at all life cycle stages (review). Aviacionnye materialy i tehnologii, 2019, no. 4 (58), pp. 86–94. DOI: 10.18577/2071-9140-2020-0-1-86-94.
  4. Varchenko E.A., Kurs M.G. Natural tests of metal materials in sea water: key approaches to estimation of resistance to corrosion and biodeterioration. Trudy VIAM, 2017, no. 11 (59), paper no. 12. Available at: http://www.viam-works.ru (accessed: December 15, 2019). DOI: 10.18577/2307-6046-2017-0-11-12-12.
  5. Yakovlev A.D. Chemistry and technology of paints and varnishes: a textbook for universities. Leningrad: Khimiya, 1989, pp. 162–163.
  6. Beetle N.P. The course of the theory of corrosion and protection of metals. Leningrad: Metallurgy, 1976, pp. 400–401.
  7. ALMET marine. Available at: http://www.almet-marine.com/ (accessed: December 20, 2019).
  8. Varchenko E.A., Kurs M.G. Influence of cor-rosion environmental parameters on properties of constructional metal materials while testing in sea water (review). Trudy VIAM, 2019, no. 5 (77), paper no. 10. Available at: http://www.viam-works.ru (accessed: December 16, 2019). DOI: 10.18577/2307-6046-2019-0-5-85-93.
  9. Sorokin A.I. Investigation of the process of destruction of an aluminum alloy from contact corrosion in a high-speed flow of sea water. Visnik SevNTU, 2012,ser.: mekhanika, energy, ecology, is. 132, pp. 135–141.
  10. Ovchinnikov I.M,. Titov V.B., Krivosheya V.G. New data on the temporal variability of currents based on the results of long-term measurements from a stabilized buoy on the Black Sea shelf. Doklady AN SSSR, 1986, vol. 286, no. 5, pp. 1250–1254.
  11. Bukharev G.M., Laptev A.B., Yakovenko T.V., Bobyreva T.V. The role of assessing the biological factor in ensuring the safe operation of complex technical systems during the life cycle. Problems of assessing the climatic resistance of materials and complex technical systems: collection of articles. report II All-Russia. scientific and technical conf. Climate-2017. Moscow: VIAM, 2017, pp. 21–30.
  12. Kablov E.N. Materials are the basis of any business. Delovaya slava Rossii, 2013, no. 2, pp. 4-9.
  13. Kablov E.N., Startsev O.V. The basic and applied research in the field of corrosion and ageing of materials in natural environments (review). Aviacionnye materialy i tehnologii, 2015, no. 4 (37), pp. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
  14. Huppatz W., Meissner H. Effect of the temperature and salt content of sea water on the corrosion behavior of aluminum. Werkstoffe und Corrosion, 1987, vol. 38, pp. 709–710.
  15. Kablov E.N. Marketing of materials science, aircraft construction and industry: present and future. Direktor po marketingu i sbytu, 2017, no. 5-6, pp. 40–44.
  16. Aluminum alloy of the Al–Mg–Si system: pat. 2672977 Rus. Federation; filed 01.11.17; publ. 21.11.18.
  17. Kablov E.N. New generation materials – the basis for innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  18. Akhiyarov R.Zh., Laptev A.B., Movenko D.A., Belova N.A. Investigation of abnormally low corrosion resistance of pipe steel of heat exchangers for oil refining. Neftyanoe khozyaistvo, 2016, no. 1, pp. 118–121.
  19. Adler Yu.P., Markova E.V., Granovsky Yu.V. Planning an experiment to find optimal conditions. Moscow: Nauka, 1976, 279 p.
  20. Laptev A.B., Nikolaev E.V., Skirta A.A., Laptev D.A. A method for assessing the state of materials in the process of climatic aging. Aviakosmicheskoe priborostroenie, 2016, no. 11, pp. 20–29.
  21. Turova T.P., Sokolova D.Sh., Nazina T.N., Gruzdev D.S., Laptev A.B. Phylogenetic diversity of microbial communities from the surface of polyethylene terephthalate materials when exposed to aqueous media. Microbiology, 2020, vol. 89, no. 1, pp. 99–110. DOI: 10.31857/S0026365620010152.
  22. Tourova T., Sokolova D., Nazina T., Grouzdev D., Kurshev E., Laptev A. Biodiversity of Microorganisms Colonizing the Surface of Polystyrene Samples Exposed to Different Aqueous Environments. Sustainability, 2020, vol. 12, no. 9, pp. 3624–3642.