Temporary laminated stoppers: materials, properties, application

Postnov V.I., Postnova M.V., Barannikov A.A., Veshkin E.A
Postnov V.I., Postnova M.V., Barannikov A.A., Veshkin E.A Temporary laminated stoppers: materials, properties, application // Proceedings of VIAM. 2020. No. 4-5. DOI: 10.18577/2307-6046-2020-0-45-32-41. URL: https://www.viam-works.ru/en/journal/2020/4-5/4
Keywords
aluminum foul tape, temporary repair, vibrating loadings, the temporary laminated stopper, adhesion, aluminium tape.
Abstract

During plane operation on a glider surface often there are defects and damages which at the further operation can lead to breakage, therefore in the conditions of aerodrome carry operative out repairs of such defects, allowing to raise functionability and durability of a design. In activity comparative analysis FSL of the aluminium alloys made of different compositions and glue is presented. Their comparative adhesive characteristics are resulted.

Are resulted their comparative adhesive and прочностные characteristics, and as agency of stoppers from FSL on growth rate of fatigue cracks in aluminium sheetings of an aeronautics.

Reference list
  1. Kablov E.N. Materials of a new generation – the basis of innovation, technological leadership and national security of Russia. Intellekt & Tekhnologii, 2016, no. 2, pp. 41–46.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Podzhivotov N.Yu., Kablov E.N., Antipov V.V., Erasov V.S., Serebrennikova N.Yu., Abdulin M.R., Limonin M.V. Layered metal-polymer materials in aircraft structural elements. Perspektivnyye materialy, 2016, no. 10, pp. 5–19.
  4. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, No. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  5. Zhadova N.S., Tyumeneva T.Yu., Sharova I.A., Lukina N.F. Perspective technologies for field repair if aviation engineering. Aviacionnye materialy i tehnologii, 2013, no. 2, pp. 67–70.
  6. Kondrashov S.V., Shashkeev K.A., Petrova G.N., Mekalina I.V. Constructional polymer composites with functional properties. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 405–419. DOI: 10.18577/2071-9140-2017-0-S-405-419.
  7. Kablov E.N., Minakov V.T., Postnov V.I., Kazakov I.A., Zhelezina G.F. Temporary stoppers to increase the overhaul life of aircraft skin. Aviacionnye materialy i tehnologii, 2002, vyp.: Remontnyye tekhnologii v aviastroyenii, pp. 31–34.
  8. Zhelezina G.F., Gulyaev I.N., Kazakov I.A., Postnov V.I., Yapparov V.M., Ilyin V.A. The experience of using laminated metal-organic plastics (ALORs) for repairing the glider skin of An-124 aircraft. Aviacionnye materialy i tehnologii, 2002, vyp.: Remontnyye tekhnologii v aviastroyenii, pp. 54–57.
  9. Ilyushenkov S.F., Shmagin I.V. The use of self-adhesive aluminum foil in aircraft structures. Aviatsionnaya promyshlennost, 1983, no. 10, pp. 73–75.
  10. Tyumeneva T.Yu., Zhadova N.S., Lukina N.F. Development of VIAM Federal State Unitary Enterprise in the field of adhesives of industrial rubber assignment and being self-glued materials. Trudy VIAM, 2014, no. 7, paper no. 04. Available at: http://www.viam-works.ru (accessed: December 02, 2019). DOI: 10.18577/2307-6046-2014-0-7-4-4.
  11. The adhesive composition and self-adhesive material containing it: pat. 2266941 Rus. Federation, no. 2003134176/04; filed 26.11.03; publ. 27.12.05.
  12. Lukina N.F., Petrova A.P., Muhametov R.R., Kogtjonkov A.S. New developments in the field of adhesive aviation materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 452–459. DOI: 10.18577/2071-9140-2017-0-S-452-459.
  13. Kolobova Z.N., Pavlovskaya T.G., Anikhovskaya L.I., Karimova S.A. Development of surface preparation methods for the repair of glued structures made of aluminum alloys. Aviacionnye materialy i tehnologii, 2002, vyp.: Remontnyye tekhnologii v aviastroyenii, pp. 73–76.
  14. Lukina N.F., Petrova A.P., Kotova E.V. Heat-resistent adhesives used in aviation and space technique. Trudy VIAM, 2014, no. 3, paper no. 06. Available at: http://www.viam-works.ru (accessed: December 02, 2019). DOI: 10.18577/2307-6046-2014-0-3-6-6.