Impact assessment of gas permeability of three-layered core panel on heat release

Barbotko S.L., Volnyj O.S., Bochenkov M.M.
Barbotko S.L., Volnyj O.S., Bochenkov M.M. Impact assessment of gas permeability of three-layered core panel on heat release // Proceedings of VIAM. 2020. No. 3. DOI: 10.18577/2307-6046-2020-0-3-102-110. URL: https://www.viam-works.ru/en/journal/2020/3/11
Keywords
fire safety, heat release, core panel, gas permeability, fire testing.
Abstract

This is a study of the effect of the gas permeability of the skin and honeycomb core of three-layer panels on the value of the heat release characteristics during combustion (the maximum heat release rate and the total amount of heat released during the first 2 minutes of the test). The study demonstrates that the presence of perforations of the skin or honeycomb can lead to a significant decrease in the recorded heat release characteristics due to a smoother exit of combustible thermal decomposition products from the internal volume of the three-layer panel.

Reference list
  1. Postnov V.I., Petukhov V.I., Strelnikov S.V., Makrushin K.V., Pletin I.I., Kavun N.S., Zastrogina O.B., Shvets N.I. Ways to improve manufacturability and structural properties of aircraft interior panels. Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk, 2008, vol. 1, special issue: A Quarter-Century of Surveys and Experiments on the Creation of Unique Technologies and Materials for Aircraft Engineering STCU – FSUE VIAM, pp. 59–64.
  2. Veshkin E.A., Postnov V.I., Zastrogina O.B., Satdinov R.A. Technology for accelerated molding of three-layer honeycomb panels for aircraft interior. Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk, 2013, vol. 15, no. 4-4, pp. 799–805.
  3. Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  4. The airworthiness standards of civilian light aircraft: AP-23: approved by the resolution of the 34th session of the Council on Aviation and Airspace Use 06.12.2013. 4th ed. Moscow: Aviaizdat, 2014, 208 p.
  5. Airworthiness standards for transport category aircraft: AP-25: approved. Resolution of the 35th session of the Council on Aviation and Airspace Use 23.10.2015. 3rd ed. Moscow: Aviaizdat, 2015, 290 p.
  6. Airworthiness standards of rotorcraft of the normal category: AP-27: approved. By the resolution of the 34th session of the Council on Aviation and Airspace Use 06.12.2013. 2nd ed. Moscow: Aviaizdat, 2014, 128 p.
  7. Airworthiness standards of rotorcraft of the transport category: AP-29: approved. By the resolution of the 36th session of the Council on Aviation and Airspace Use 03.15.2018. 3rd ed. Moscow: Aviaizdat, 2018, 136 p.
  8. Airworthiness standards for very light aircraft: AP-OLS. Moscow: Aviaizdat, 2006, 104 p.
  9. Transport Category Airplanes: Airworthiness Standards. Federal Regulations. Part 25. Available at: http://www.ecfr.gov/cgi-bin/text-idxSID=d7f8803c7bd1d50b6d68749e0b42d848&node=14:1.0.1.3.11&rgn=div5 (accessed: October 10, 2019).
  10. Certification Specifications and Acceptable Means of Compliance for Large Aeroplanes: CS-25. 2020. 1116 p. Available at: https://www.easa.europa.eu/document-library/certification-specifications/cs-25-amendment-24 (accessed: October 10, 2019).
  11. Barbotko S.L., Volny O.S., Kirienko O.A., Shurkova E.N. Fire safety assessment of aviation polymer materials: state analysis, test methods, development prospects, methodological features / gen. ed. E.N. Kablov. Moscow: VIAM, 2018, 442 p.
  12. Berlin A.A. Combustion of polymers and low combustibility polymeric materials. Sorosovskiy obrazovatelny zhurnal, 1996, no. 9, pp. 57–63.
  13. Barbotko S.L. Heat emission during combustion of polymer materials for aviation purposes: thesis abstract. Cand. Sc. (Tech.). Moscow, 1999, 23 p.
  14. Barbotko S.L., Vorobyov V.N. Influence of air flow in OSU calorimeter on test results. Proceeding of the Third Triennial International Aircraft Fire & Cabin Safety Conference (Atlantic City, New Jersey, USA. October 22–25, 2001). Available at: http://www.fire.tc.faa.gov (accessed: October 10, 2019).
  15. Zhelezina G.F., Bader E.Ya., Raskutin A.E., Migunov V.P., Stolyankov Yu.V. Materials for sound-absorbing structures. Vse materialy. Entsiklopedicheskiy spravochnik, 2012, no. 4, pp. 12–16.
  16. A method of manufacturing a relief aggregate: pat. 2307032 Rus. Federation; filed 27.12.05; publ. 27.09.07.
  17. Barbotko S.L. Ways of providing fire safety of aviation materials. Russian Journal of General Chemistry, 2011, vol. 81, no. 5, pp. 1068–1074.
  18. Kurnosov A.O., Sokolov I.I., Melnikov D.A., Topunova T.E. Fireproof fiberglass for interior of passenger aircraft (review). Trudy VIAM, 2015, no. 11, paper no. 07. Available at: http://www.viam-works.ru (accessed: October 10, 2019). DOI: 10.18577/2307-6046-2015-0-11-7-7.
  19. Petrova G.N., Beider E.Ya., Perfilova D.N., Rumyantseva T.V. Fire safety of injection molding thermoplastics and TPE materials. Trudy VIAM, 2013, no. 11, paper no. 02. Available at: http://www.viam-works.ru (accessed: October 10, 2019).
  20. Shurkova E.N., Volny O.S., Izotova T.F., Barbotko S.L. Research of possibility of decrease in heat release when burning composite material by change of its structure. Aviacionnye materialy i tehnologii, 2012, no. 1, pp. 27–30.
  21. Lyon R.E., Gandhi S., Crowley S. Fire Properties of Heat-Resistant Polymers: Technical Report DOT/FAA/TC-TN18/32. 2019. 33 p. Available at: http://www.fire.tc.faa.gov (accessed: October 10, 2019).
  22. Quintiere J.G., Walters R.N., Crowley S. Flammability Properties of Aircraft Carbon-Fiber Structural Composite: Technical Report DOT/FAA/AR-07/57. 2007. 43 p. Available at: http://www.fire.tc.faa.gov (accessed: October 10, 2019).
  23. Lyon R.E., Janssens M.L. Polymer Flammability: Technical Report DOT/FAA/AR-05/14. 2005. 82 p. Available at: http://www.fire.tc.faa.gov (accessed: October 10, 2019).
  24. Zhang H. Fire-Safe Polymers and Polymer Composites: Technical Report DOT/FAA/AR-04/11. 2004. 209 p. Available at: http://www.fire.tc.faa.gov (accessed: October 10, 2019).
  25. Flammability Testing of Interior Materials: Policy Statement No. PS-ANM-25.853-01-R2. 2013. 28 p. Available at: http://www.faa.gov (accessed: October 10, 2019).
  26. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  27. Kablov E.N. At the crossroads of science, education and industry. Ekspert, 2015, no. 15 (941), pp. 49–53.
  28. Kablov E.N. What to make the future of? Materials of a new generation, technologies for their creation and processing - the basis of innovation. Krylya Rodiny, 2016, no. 5, pp. 8–18.