Alternatives to chromate pigments (review)

Kovrizhkina N.A., Kuznetsova V.A., Silaeva A.A., Emelyanov V.V.
Kovrizhkina N.A., Kuznetsova V.A., Silaeva A.A., Emelyanov V.V. Alternatives to chromate pigments (review) // Proceedings of VIAM. 2020. No. 12. DOI: 10.18577/2307-6046-2020-0-12-96-107. URL: https://www.viam-works.ru/en/journal/2020/12/10
Keywords
coating materials, anticorrosive pigments, corrosion inhibitors, chromate replacement, the transitional metals, conductive polymers, core pigments, non-chromate pigments.
Abstract

The review of the researches concerning search of alternative to chromate pigments is provided. Among possible alternatives various connections are considered: cerium salts (in a mix with other non-chromate pigments), compounds of phosphorus, including organic (oxyaminophosphates and oxyethylidenediphosphonates), conductive polymers (polyaniline and polipirrol) and core pigments on their basis, compounds of transitional metals (vanadium, tungsten, molybdenum, manganese, etc.). It is shown that correctly picked up mix of pigments of inhibitive type is capable to provide the level of protective properties which is not conceding to coverings, containing chromate pigments.

Reference list
  1. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  2. Kablov E.N. Corrosion or life. Nauka i zhizn, 2012, no. 11, pp. 16–21.
  3. Zheleznyak V.G. Modern paint and varnish materials for use in aviation equipment products. Trudy VIAM, 2019, no. 5 (77), paper no. 07. Available at: http://www.viam-works.ru. (accessed: October 17, 2020). DOI: 10.18577/2307-6046-2019-0-5-62-67.
  4. Twite R.L., Bierwagen G.P. Review of alternatives to chromate for corrosion protection of aluminum aerospace alloys. Progress in Organic Coatings, 1998, no. 33, pp. 91–100.
  5. Kablov E.N. Innovative development is the most important priority of the state. Metally Evrazii, 2010, no. 2, pp. 6–11.
  6. Merkulova Yu.I., Kuznetsova V.A., Novikova T.A. Investigation of properties of coating system based on fluorine polyurethane enamel and primer with low toxical pigment content. Trudy VIAM, 2019, no. 5 (77), paper no. 08. Available at: http://www.viam-works.ru. (accessed: October 2, 2020). DOI: 10.18577/2307-6046-2019-0-5-68-75.
  7. Kablov E.N., Startsev O.V., Medvedev I.M., Shelemba I.S. Fiber optic sensors for monitoring corrosion processes in units of aviation engineering (review). Aviacionnye materialy i tehnologii, 2017, no. 3 (48), pp. 26–34. DOI: 10.18577/2071-9140-2017-0-3-26-34.
  8. Kuznetsova V.A., Semenova L.V., Shapovalov G.G. Development trends in the field of anticorrosive polymeric systems for corrosion protection of fixing connections of contact couples of combined structures (review). Aviacionnye materialy i tehnologii, 2017, no. 1 (46), pp. 25–31. DOI: 10.18577/2071-9140-2017-0-1-25-31.
  9. Drinberg A.S., Itsko E.F., Kalinskaya T.V. Anti-corrosion primers. Saint Petersburg: NIPROINS LKM and P s OP, 2006, 168 p.
  10. Kalininskaya T.V., Drinberg A.S. Colored pigments. Moscow: LKM-press, 2013, 360 p.
  11. Chromate-free protective coatings: pat. EP 0792922B1; filed 26.02.97; publ. 03.09.97.
  12. Chromate free waterborne epoxy corrosion resistant primer: pat. EP 1433821B1; filed 24.11.03; publ. 30.06.04.
  13. Rosenfeld I.L., Rubinstein F.I. Anti-corrosion primers and inhibited paints. Moscow: Khimiya, 1980, 200 p.
  14. Anticorrosive pigment: pat. 2330054 Rus. Federation, no. 2007117422/04; filed 04.05.07; publ. 27.07.08.
  15. Ashuiko V.A., Ivanova N.P., Salychits O.I. Properties of anticorrosive phosphate-containing pigments for paint and varnish coatings of metals. Energy and material-saving environmentally friendly technologies: abstracts of the X Intern. conf. Grodno, 2013, pp. 117–118.
  16. Anticorrosive pigment: pat. 2151157 Rus. Federation, no. 99115751/12; filed 19.07.99; publ. 20.06.00.
  17. Deya´ C., Romagnoli R., del Amo B. A new pigment for smart anticorrosive coatings. Journal of Coatings Technology and Research, 2007, no. 4 (2), pp. 167–175.
  18. Kuznetsova O.S. The use of calcium phosphonate for pigmentation of anticorrosive coatings. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2012, no. 8, pp. 38–39.
  19. Sheremetyeva I.M., Vakhin A.V., Svetlakov A.P. Anticorrosive properties of core phosphonate pigments. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2011, no. 11, pp. 142–145.
  20. Skorokhodova O.N., Kazakova E.E. New pigments and fillers for the production of paintwork materials. Paint and varnish industry. 2017, no. 6, pp. 20–23.
  21. MacQueen R.C., Miron R.R., Granata R.D. Method for corrosion inhibitor mechanism studies in epoxy coater aluminum. Lakokrasochnaya promyshlennost, 1996, no. 68 (857), pp. 75–82.
  22. Emirova I.V., Alekseev A.A. New anticorrosive pigments. Izvestiya vuzov. Khimiya i khimicheskaya tekhnologiya, 2009, vol. 52, no. 6, pp. 113–114.
  23. Liu J., Yang S.C. Novel colloidal polyaniline fibrils made by template guided chemical polymerization. Journal of the Chemical Society, Chemical Communications, 1991, is. 21, pp. 1529–1531.
  24. Kurbatov V.G., Ilyin A.A., Indeikin E.A. Anticorrosive pigments and fillers with polyaniline sheath. Lakokrasochnye materialy i ikh primeneniye, 2012, no. 11, pp. 49–52.
  25. Kurbatov V.G., Kochkina N.V., Indeikin E.A. The use of shell pigments in the composition of polymeric anticorrosive materials. Uspekhi v khimii i khimicheskoy tekhnologii, 2014, vol. XXVIII, no. 3, pp. 92–96.
  26. Sitnov S.A., Vakhin A.V., Khuziakhmetov R.Kh., Stepin S.N. Properties of mechanochemically obtained core phosphonate pigments. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2012, no. 14, pp. 71–73.
  27. Anticorrosive pigment: pat. 2237073 Rus. Federation, no. 2003123808/15; filed 29.07.03; publ. 27.09.04.
  28. Salychits O.I., Orekhova S.E., Ashuiko V.A. Pigments with anticorrosive properties based on transition metal compounds. Trudy BGT, 2012, no. 3, pp. 16–18.
  29. Orekhova S.E., Ashuiko V.A., Kurilo I.I., Salychits O.I. Synthesis and properties of pigments for paints and varnishes with anticorrosive properties. Energy and material-saving environmentally friendly technologies: abstracts of the IX Intern. conf. Grodno, 2011, pp. 42–43.
  30. Akulich N.E., Zharsky I.M., Ivanova N.P., Kurilo I.I. Anticorrosive properties of pigments based on bismuth and calcium vanadates. Vesti Natsionalnoy akademii nauk Belarusi, Chemical Science Series, 2016, no. 2, pp. 5–9.
  31. Shutova A.L., Globa A.I., Prokopchuk N.R. et al. Features of the use of new pigments in alkyd anticorrosive primers. Trudy BGTU, 2014, no. 4, pp. 43–47.
  32. Ziganshina M.R., Stepin S.N. Anticorrosive properties of coatings pigmented with manganese compounds obtained by the ceramic method. Lakokrasochnyye materialy i ikh primeneniye, 2017, no. 3, pp. 34–40.
  33. Ziganshina M.R., Stepin S.N., Akhmadieva A.A. et al. Assessment of anticorrosive properties of «manganese blue». Lakokrasochnyye materialy i ikh primeneniye, 2007, no. 9, pp. 19–22.
  34. Slobodchikova I.V. Obtaining an epoxy primer using a manganese-containing pigment. Best research work–2017: collection of articles of winners of the VII Int. scientific-practical competition. Penza: Science and Education, 2017, pp. 18–23.
  35. Karandashov S.A., Dzhanbekova A.V., Knyazeva N.A. Development of anti-corrosion primers. Globus, 2016, vol. 1, no.10 (14), pp. 8–11.
  36. Afanasyev O. L. Inhibitory properties of polymer coatings containing barium manganate: thesis, Cand. Sc (Tech.). Kazan: Kazan State Technol. Univ., 2010, 16 p.
  37. Sorokov A.V. Anticorrosive properties of synthetic manganese and phosphonate-containing pigments and primers based on them: hesis, Cand. Sc (Tech.). Kazan: Kazan State Technol. Univ., 2003, 118 p.
  38. Ziganshina M.R., Vakhin A.V. Physical and mechanical properties of epoxy coatings filled with manganese-containing piments. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2014, no. 5, pp. 42–43.
  39. Ziganshina M.R., Usmanova E.D. Manganese pigments for polymer compositions for decorative purposes. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2013, no. 10, pp. 138–140.
  40. Ziganshina M.R., Bayburina E.A., Azizova E.T. Performance properties of epoxy coatings based on E-40 resin filled with manganese-containing pigment. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2015, no. 1, pp. 141–142.
  41. Nurislamova E.A., Baranov A.O., Gaptravanova A.V. Low-toxic anticorrosive pigment. World Science: problems and innovations: collection of articles of XVI Inter. scientific-practical conf.: 3 parts. Penza: Science and Education, 2017, part 1, pp. 69–72.
  42. Gataullina E. D. Anticorrosive properties of calcium phosphate (V) manganate (IV) and the development of primers based on it: thesis abstract, Cand. Sc (Tech.). Kazan: Kazan State Technol. Univ., 2008, 20 p.