Removal of hardening coatings based on titanium nitride and zirconium nitride from the surface of parts made of titanium alloys

Dobrynin D.A., Iatsyuk I.V., Doronin O.N.
Dobrynin D.A., Iatsyuk I.V., Doronin O.N. Removal of hardening coatings based on titanium nitride and zirconium nitride from the surface of parts made of titanium alloys // Proceedings of VIAM. 2020. No. 11. DOI: 10.18577/2307-6046-2020-0-11-113-121. URL: https://www.viam-works.ru/en/journal/2020/11/12
Keywords
chemical and electrochemical removal of coatings, hardening coating, titanium nitride, zirconium nitride, titanium alloy.
Abstract

Рrovides an overview of the methods of chemical and electrochemical removal of hardening coatings based on titanium nitride (TiN) and zirconium nitride (ZrN) from the surface of parts made of various materials that can be used to remove defective and waste coatings from the surface of compressor blades and other parts of gas turbine engines (GTE) from titanium alloys. The main disadvantages of the described methods are shown in relation to the removal of hardening coatings from the surface of compressor blades and other GTE parts made of titanium alloys. Taking into account the shortcomings of the available methods, FSUE «VIAM» has developed effective methods for chemical removal of hardening coatings based on titanium nitride and zirconium nitride from the surface of parts made of titanium alloys, and recommendations are given for controlling the completeness of removal of coatings.

Reference list
  1. Kablov E.N., Muboyadzhyan S.A. Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTE. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 60–70.
  2. Kablov E.N., Muboyadzhyan S.A. Protective coatings for turbine blades of promising gas turbine engines. Gazoturbinnye tehnologii, 2001, no. 2 (12), pp. 30–32.
  3. Popova S.V., Muboyadzhyan S.A., Budinovskiy S.A., Dobrynin D.A. The feature of electrolytic plasma etching of heat resistant coatings from parts surface of high-temperature nickel alloys. Trudy VIAM, 2016, no. 2 (38), paper no. 04. Available at: http://www.viam-works.ru (accessed: October 05, 2020). DOI: 10.18577/2307-6046-2016-0-2-4-4.
  4. Kablov E.N., Muboyadzhyan S.A., Budinovskiy S.A., Lutsenko A.N. Ion-plasma protective coatings for blades of gas turbine engines. Metally, 2007, no. 5, pp. 23–34.
  5. Muboyadzhyan S.A., Budinovskij S.A. Ion-plasma technology: prospective processes, coatings, equipment. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 39–54. DOI: 10.18577/2071-9140-2017-0-S-39-54.
  6. Muboyadzhyan S.A., Kablov E.N., Budinovsky S.A. Vacuum-plasma technology for producing protective coatings from complex-alloyed alloys. Metallovedeniye i termicheskaya obrabotka metallov, 1995, no. 2, pp. 15-18.
  7. Method of removing a coating from a substrate: pat. US6905396B1; filed 20.11.03; publ. 14.07.05.
  8. Process for treating the surface of a component, made from a Ni based supperalloy, to be coated: pat. US6440238B1; filed 09.08.99; publ. 27.08.02.
  9. Composition for removing titanium nitride coatings from the surface of titanium alloy parts: pat. 2396372С1 Rus. Federation; filed 26.05.09; publ. 10.08.10.
  10. Method for removing titanium nitride film from the surface of stainless steel products: pat. 2039851С1 Rus. Federation; filed 17.08.92; publ. 20.07.95.
  11. Method for repairing parts, mainly blades, gas turbine engines: pat. 2205734С2 Rus. Federation; filed 14.03.01; publ. 10.06.03.
  12. Solution for removing coatings from titanium nitride and carbonitride: pat. 2081207С1 Rus. Federation; filed 15.06.95; publ. 10.06.97.
  13. Timergazina T.M. Research of physicochemical processes of removal of titanium nitride coating and development of recommendations for the repair technology of compressor blades of gas turbine engines: thesis, Cand. Sc. (Tech.). Ufa, Ufa Aviation Tech. University, 1997, 16 p.
  14. Method for removing coating from parts and solution for removing coating: pat. 2507311S2 Rus. Federation; filed 09.04.09; publ. 20.02.14.
  15. Method for restoring the operational properties of machine parts: pat. 2281194С1 Rus. Federation; iled 04.03.05; opubl. 10.08.06
  16. Method of electrolyte-plasma removal of coatings from titanium nitrides or nitrides of titanium compounds with metals: pat. 2467098C1 Rus. Federation; filed 25.04.11; opubl. 20.11.12.
  17. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.