Ceramics based on organosilicon polymers-precursors: methods of preparation and properties (review)

Shestakov A.M.
Shestakov A.M. Ceramics based on organosilicon polymers-precursors: methods of preparation and properties (review) // Proceedings of VIAM. 2020. No. 11. DOI: 10.18577/2307-6046-2020-0-11-76-92. URL: https://www.viam-works.ru/en/journal/2020/11/9
Keywords
silicon carbide, silicon carbonitride, ceramics, organosilicon polymers, fillers, silicon nitride, curing, pyrolysis, thermal oxidative stability, shaping.
Abstract

The main types of preceramic organosilicon polymers, general methods of their synthesis and physical, and chemical properties are considered. Methods of shaping, curing and pyrolysis of polymers and the influence of process parameters on the composition, structure and properties of ceramics are described. Separately, the work considers modifying fillers for preceramic polymers, the goals and methods of their introduction into the polymer, the features of processing the compositions and the properties of the products obtained.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. E. N. Kablov Composites: Today and Tomorrow. Metally evrazii, 2015, no. 1, pp. 36–39.
  3. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  4. Grashchenkov D.V., Evdokimov S.A., Zhestkov B.E., Solntsev S.St., Shtapov V.V. Research of thermochemical influence of the air plasma flow on high-temperature ceramic composite material. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 31–40. DOI: 10.18577/2071-9140-2017-0-2-31-40.
  5. Kablov E.N., Nikiforov A.A., Demin S.A., Chesnokov D.V., Vinogradov S.S. Promising coatings for corrosion protection of carbon steels. Stal, 2016, no. 6, pp. 70–81.
  6. Grashchenkov D.V., Efimochkin I.Yu., Bolshakova A.N. High-temperature metal-matrix composite materials reinforced with particles and fibers of refractory compounds. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 318–328. DOI: 10.18577/2071-9140-2017-0-S-318-328.
  7. Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.S., Sevastianov V.G. High-temperature structural composite materials based on glass and ceramics for advanced aircraft products. Steklo i keramika, 2012, no. 4, pp. 7–11.
  8. Sorokin O.Yu., Grashhenkov D.V., Solntsev S.St., Evdokimov S.A. Ceramic composite materials with high oxidation resistance for the novel aircrafts (review). Trudy VIAM, 2014, no. 6, paper no. 8. Available at: http://www.viam-works.ru (accessed: January 24, 2020). DOI: 10.18577/2307-6046-2014-0-6-8-8.
  9. Minakov V.T., Solntsev S.S. Ceramic-matrix composites. Vse materialy. Entsiklopedicheskiy spravochnik, 2007, no. 2, pp. 5–9.
  10. Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.St. Promising high-temperature ceramic composite materials. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, No. 1, pp. 20–24.
  11. Sorokin O.Yu. On the issue of the mechanism of interaction between carbon materials and Si melt (review). Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 65–70. DOI: 10.18577/2071-9140-2015-0-1-65-70.
  12. Fu Sh., Zhu M., Zhu Y. Organosilicon polymer-derived ceramics: An overview. Journal of Advanced Ceramics, 2019, vol. 8, no. 4, pp. 457–478.
  13. Zhao Zh., Li K., Li W. et al. Preparation, ablation behavior and mechanism of C/C–ZrC–SiC and C/C–SiC composites. Ceramics International, 2018, vol. 44, no. 7, pp. 7481–7490.
  14. Colombo P., Riedel R., Soraru G.D., Kleebe H.K. Historical Review of the Development of Polymer Derived Ceramics (PDCs). Polymer Derived Ceramics: From Nanostructure to Applications. Pennsylvania: DEStech Publications Inc. Lancaster, 2010, pp. 1–13.
  15. Du B., Hong Ch., Zhang X. et al. Preparation and mechanical behaviors of SiOC-modified carbon-bonded carbon fiber composite with in situ growth of three-dimensional SiC nanowires. Journal of the European Ceramic Society, 2018, vol. 38, no. 5, pp. 2272–2278.
  16. Zhang L., Pei L., Li H. et al. Preparation and characterization of Na and F co-doped hydroxyapatite coating reinforced by carbon nanotubes and SiC nanoparticles. Materials Letters, 2018, vol. 218, pp. 161–164.
  17. Wang Z.-C., Aldinger F., Riedel R. Novel Silicon–Boron–Carbon–Nitrogen Materials Thermally Stable up to 2200 °C. Journal of the American Ceramic Society, 2001, vol. 84, no. 10, pp. 2179–2183.
  18. Colombo P., Mera G., Riedel R., Soraru G.D. Polymer-Derived Ceramics: 40 Years of Research and Innovation in Advanced Ceramics. Journal of the American Ceramic Society, 2010, vol. 93, no. 7, pp. 1805–1837.
  19. Blum Y.D., MacQueen D.B., Kleebe H.-J. Synthesis and Characterization of Carbon-Enriched Silicon Oxycarbides. Journal of the European Ceramic Society, 2005, vol. 25, no. 2–3. P. 143–149.
  20. Kleebe H.-J., Gregori G., Babonneau F. et al. Evolution of C-Rich SiCO Ceramics. Part I. Characterization by Integral Spectroscopic Techniques: Solid-State NMR and Raman Spectroscopy. International Journal of Materials Research, 2006, vol. 97, no. 6, pp. 699–709.
  21. Gregori G., Kleebe H.-J., Blum Y.D., Babonneau F. Evolution of C-Rich SiCO Ceramics. Part II. Characterization by High Lateral Resolution Techniques: Electron Energy-Loss Spectroscopy, High-Resolution TEM and Energy-Filtered TEM. International Journal of Materials Research, 2006, vol. 97, no. 6, pp. 710–720.
  22. Kleebe H.-J., Blum Y.D. SiOC Ceramic with High Excess Free Carbon. Journal of the European Ceramic Society, 2008, vol. 28, no. 5, pp. 1037–1042.
  23. Kipping F.S., Sands J.E. XCIII-Organic Derivatives of Silicon. Part XXV. Saturated and Unsaturated Silicohydrocarbons, Si4Ph8. Journal of the Chemical Society Transactions, 1921, vol. 119, pp. 830–847.
  24. Kipping F.S. CCCVIII-Organic Derivatives of Silicon. Part XXX. Complex Silicohydrocarbons [SiPh2]n. Journal of the Chemical Society Transactions, 1924, vol. 125, pp. 2291–2297.
  25. Aitken C.T., Harrod J.F., Samuel E. Polymerization of Primary Silanes to Linear Polysilanes Catalyzed by Titanocene Derivatives. Journal of Organometallic Chemistry, 1985, vol. 279, no. 1–2, pp. C11–C13.
  26. Aitken C.T., Harrod J.F., Samuel E. Identification of Some Intermediates in the Titanocene-Catalyzed Dehydrogenative Coupling of Primary Organosilanes. Journal of the American Chemical Society, 1986, vol. 108, no. 14, pp. 4059–4066.
  27. Shiina K., Kumada M. Thermal Rearrangement of Hexamethyldisilane to Trimethyl(dimethylsilylmethyl)silane. Journal of Organic Chemistry, 1958, vol. 23, no. 1, pp. 139–139.
  28. Storozhenko P.A., Shcherbakova G.I., Tsirlin A.M. et al. Synthesis of nanozirconium oligocarbosilanes. Neorganicheskiye materialy, 2006, vol. 42, no. 10, pp. 1269–1277.
  29. Shcherbakova G.I., Storozhenko P.A., Sidorov D.V. et al. Features of the molecular structure of pre-ceramic nanozirconium oligocarbosilanes. Neorganicheskiye materialy, 2011, vol. 47, no. 5, pp. 605–613
  30. Shcherbakova G.I., Blokhina M.Kh., Storozhenko P.A. et al. Preceramic nanogaphnium oligocarbosilanes. Neorganicheskiye materialy, 2014, vol. 50, no. 4, pp. 457–464.
  31. Chojnowski J., Cypryk M., Kurjata J. Organic Polysilanes Interrupted by Heteroatoms. Progress in Polymer Science, 2003, vol. 28, no. 5, pp. 691–728.
  32. Kurjata J., Chojnowski J. Equilibria and Kinetics of the Cationic Ring-Opening Polymerization of Permethylated 1,4-dioxa-2,3,5,6-tetrasilacyclohexane. Comparison with Cyclosiloxanes. Macromolecular Chemistry and Physics, 1993, vol. 194, no. 12, pp. 3271–3286.
  33. Chi F.K. Carbon-Containing Monolithic Glasses via the Sol-Gel Process. Proceedings of the 7th Annual Conference on Composites and Advanced Ceramic Materials: Ceramic Engineering and Science Proceedings, 1983, vol. 4, pp. 704–717.
  34. Babonneau F., Thorne K., Mackenzie J.D. Dimethyldiethoxysilane/Tetraethoxysilane Copolymers: Precursors for the Silicon–Carbon–Oxygen System. Chemistry of Materials, 1989, vol. 1, no. 5, pp. 554–558.
  35. Zhang H., Pantano C.G. Synthesis and Characterization of Silicon Oxycarbide Glasses. Journal of the American Ceramic Society, 1990, vol. 73, no. 4, pp. 958–963.
  36. Kroke E., Li Y.-L., Konetschny C. et al. Silazane Derived Ceramics and Related Materials. Materials Science and Engineering: Reports, 2000, vol. 26, no. 4–6, pp. 97–199.
  37. Krüger C.R., Rochow E.G. Polyorganosilazanes. Journal of Polymer Science, part A: General Papers. 1964, vol. 2, no. 7, pp. 3179–3189.
  38. Production of Shaped Articles of Homogeneous Mixtures of Silicon Carbide and Nitride: pat. US3853567A; filed 02.04.73; publ. 12.12.74.
  39. Seyferth D., Stewart R.M. Synthesis and Polymerization of Cyclotetrasilazanes. Applied Organometallic Chemistry, 1997, vol. 11, no. 10–11, pp. 813–832.
  40. Blum Y., Laine R.M. Catalytic Methods for the Synthesis of Oligosilazanes. Organometallics, 1986, vol. 5, no. 10, pp. 2081–2086.
  41. Laine R.M. Transition Metal Catalysed Synthesis of Oligo- and Polysilazanes. Platinum Metals Review, 1988, vol. 32, no. 2, pp. 64–71.
  42. Seyferth D., Strohmann C., Dando N.R., Perrotta A.J. Poly(ureidosilazanes): Preceramic Polymeric Precursors for Silicon Carbonitride and Silicon Nitride. Synthesis, Characterization, and Pyrolytic Conversion to Si3N4/SiC Ceramics. Chemistry of Materials, 1995, vol. 7, no. 11, pp. 2058–2066.
  43. Method for manufacturing a hafnium-containing silazane polymer and a method for manufacturing a ceramic from said polymer: pat. US 5296418; filed 23.10.92; publ. 22.03.94.
  44. Kotrelev G.V., Petrov V.S., Zhdanov A.A. et al. Influence of titanium and zirconium atoms in the chain of oligomethylsilazanes on the process of their thermal destruction under dynamic heating in vacuum. Vysokomolekulyarnyye soyedineniya, ser. A, 2000. T. 42, no. 2, pp. 312–319.
  45. Ryzhova O.G., Polivanov A.N., Timofeev I.A. Polyorganosilazanes: present and future. Vse materialy. Entsiklopedicheskiy spravochnik, 2010, no. 10, pp. 47–55.
  46. The method of obtaining oligoborsilazanes: pat. RU2546664; filed 30.12.13; publ. 10.04.15.
  47. Seyferth D., Plenio H. Borasilazane Polymeric Precursors for Borosilicon Nitride. Journal of the American Ceramic Society, 1990, vol. 73, no. 7, pp. 2131–2133.
  48. Su K., Remsen E.E., Zank G.A., Sneddon L.G. Synthesis, Characterization, and Ceramic Conversion Reactions of Borazine-Modified Hydridopolysilazanes: New Polymeric Precursors to Silicon Nitride Carbide Boride (SiNCB) Ceramic Composites. Chemistry of Materials, 1993, vol. 5. No. 4, pp. 547–556.
  49. Baldus H.-P., Passing G., Sporn D., Thierauf A. Si-B-(N,C) A New Ceramic Material for High Performance Applications. Ceramic Transactions. High-Temperature Ceramic-Matrix Composites II. Eds. A.G. Evans, R. Naslain. Westerville: American Ceramic Society, 1995, vol. 58. P. 75–84.
  50. Riedel R., Kienzle A., Dressler W. et al. A Silicoboron Carbonitride Ceramic Stable to 2000 °C. Nature, 1996, vol. 382, pp. 796–798.
  51. Srivastava D., Duesler E.N., Paine R.T. Synthesis of Silylborazines and Their Utilization as Precursors to Silicon-Containing Boron Nitride. European Journal of Inorganic Chemistry, 1998, vol. 1998, no. 6, pp. 855–859.
  52. Schmidt W.R., Narsavage-Heald D.M., Jones D.M. et al. Poly(borosilazane) Precursors to Ceramic Nanocomposites. Chemistry of Materials, 1999, vol. 11, no. 6, pp. 1455–1464.
  53. Weinmann M., Schuhmacher J., Kummer H. et al. Synthesis and Thermal Behavior of Novel Si–B–C–N Ceramic Precursors. Chemistry of Materials, 2000, vol. 12, no. 3, pp. 623–632.
  54. Isocyanate- and isothiocyanate-modified polysilazane ceramic precursors: pat. US4929704А; filed 20.12.88; publ. 29.05.90.
  55. Gordetsov A.S., Kozyukov V.P., Vostokov I.A. et al. Synthesis and properties of silicon-, germanium-, tin- and lead-containing carbodiimides and cyanamides. Uspekhi khimii, 1982. T. 51, no. 5, pp. 848–878.
  56. Pump J., Rochow E.G. Silylcarbodiimide. IV. Sila-Polycarbodiimide. Zeitschrift für Anorganische und Allgemeine Chemie, 1964, vol. 330, no. 1–2, pp. 101–106.
  57. Klebe J.F., Murray J.G. Organosiliconcarbodiimide Polymers and Process for Their Preparation: pat. US3352799А; filed 22.06.66; publ. 14.11.67.
  58. Birkofer L., Ritter A., Richter P. N,N′-bis-trimethylsilyl-carbodiimide. Tetrahedron Letters, 1962, vol. 3, no. 5, pp. 195–198.
  59. Haag P., Lechler R., Weidlein J. Substitution Reactions of Bis(trimethylelement)Carbodiimides of Silicon and Germanium with Metal Chloride and Dimethylmetal Chlorides of Sb, Al, Ga, and In. Zeitschrift für Anorganische und Allgemeine Chemie, 1994, vol. 620, no. 1, pp. 112–116.
  60. Mera G., Riedel R., Poli F., Müller K. Carbon-Rich SiCN Ceramics Derived from Phenyl-Containing Poly(silylcarbodiimides). Journal of the European Ceramic Society, 2009, vol. 29, no. 13, pp. 2873–2883.
  61. Kolesnikova A.B., Mitrofanov M.Yu., Gruzinova E.A., Muzafarov A.M. Synthesis and modification of polysilylcarbodiimides. Vysokomolekulyarnyye soyedineniya, ser. A. 2007. T. 49, no. 9, pp. 1628–1634.
  62. Shvets N.I., Minakov V.T., Papkov V.S. et al. Research of thermochemical transformations of polycarbosilane precursors into a ceramic matrix. Zhurnal prikladnoy khimii, 2014, vol. 87, no. 6, pp. 793–799.
  63. Shestakov A.M., Shvets N.I., Rosenenkova V.A., Khaskov M.A. Ceramic-forming compositions based on polycarbosilane and modified polyorganosilazanes. Zhurnal prikladnoy khimii, 2017, vol. 90, no. 8, pp. 1066–1073.
  64. Ceramic-forming composition, ceramic composite material based on it and method of its production: pat. RU2190582; filed 09.01.01; publ. 10.10.02.
  65. Zaitsev B.A., Khramova G.I., Tsygankova T.S. et al. Dependence of physical, mechanical and thermal properties of unfilled polymers and reinforced plastics on the composition of rolivsans. Plasticheskiye massy, 2003, no. 10, pp. 23–25.
  66. Minakov V.T., Shvets N.I., Zaitsev B.A. et al. Investigation of the effect of Rolivsan on the process of obtaining a ceramic matrix from a polycarbosilane precursor. Zhurnal prikladnoy khimii, 2016, vol. 89, no.2, pp. 161–167.
  67. Shestakov A.M., Minakov V.T., Shvets N.I. et al. Ceramic-forming polymeric precursors based on polycarbosilane and diallylbisphenol A. Zhurnal prikladnoy khimii, 2014, vol. 87, no. 11, pp. 1626–1635.
  68. Shestakov A.M., Shvets N.I., Khaskov M.A. et al. Compositions based on polycarbosilane and bismaleimide – precursors of ceramic-matrix composite materials. Zhurnal prikladnoy khimii, 2015, vol. 88, no. 9, pp. 1339–1347.
  69. Shestakov A.M., Khaskov M.A., Sorokin O.Yu. Organosilicon polymer compounds based inorganic fibers for high-temperature composite materials (review). Trudy VIAM, 2019, no. 1 (73), paper no. 09. Available at: http://viam-works.ru (accessed: September 17, 2020). DOI: 10.18577/2307-6046-2019-0-1-74-91.
  70. Schwartz K.B., Rowcliffe D.J. Modeling Density Contributions in Preceramic Polymer/Ceramic Powder Systems. Journal of the American Ceramic Society, 1986, vol. 69, no. 5, pp. C106–C108.
  71. Balog M., Kečkéš J., Schöberl T. et al. Nano/Macro-Hardness and Fracture Resistance of Si3N4/SiC Composites with up to 13 wt. % of SiC Nano-Particles. Journal of the European Ceramic Society, 2007, vol. 27, no. 5, pp. 2145–2152.
  72. Schwab S.T., Blanchard C.R., Graef R.C. The Influence of Preceramic Binders on the Microstructural Development of Silicon Nitride. Journal of Materials Science, 1994, vol. 29, no. 23. P. 6320–6328.
  73. Zhu S., Fahrenholtz W.G., Hilmas G.E. Enhanced Densification and Mechanical Properties of ZrB2–SiC Processed by a Preceramic Polymer Coating Route. Scripta Materialia, 2008, vol. 59, no. 1, pp. 123–126.
  74. Greil P., Seibold M. Modelling of Dimensional Changes During Polymer-Ceramic Conversion for Bulk Component Fabrication. Journal of Materials Science,1992, vol. 27, no. 4, pp. 1053–1060.
  75. Greil P. Active-Filler-Controlled Pyrolysis of Preceramic Polymers. Journal of the American Ceramic Society, 1995, vol. 78, no. 4, pp. 835–848.
  76. Greil P. Net Shape Manufacturing of Polymer Derived Ceramics. Journal of the European Ceramic Society, 1998, vol. 18, no. 13, pp. 1905–1914.
  77. Katsuda Y., Gerstel P., Narayanan J. et al. Reinforcement of Precursor-Derived Si–C–N Ceramics with Carbon Nanotubes. Journal of the European Ceramic Society, 2006, vol. 26, no. 15. P. 3399–3405.
  78. Li Y., Fernandez-Recio L., Gerstel P. et al. Chemical Modification of Single-Walled Carbon Nanotubes for the Reinforcement of Precursor-Derived Ceramics. Chemistry of Materials, 2008, vol. 20, no. 17, pp. 5593–5599.
  79. Kim Y.-W., Kim S.-H., Kim H.-D., Park C.B. Processing of Closed-Cell Silicon Oxycarbide foams from a Preceramic Polymer. Journal of Materials Science, 2004, vol. 39, no. 18, pp. 5647–5652.
  80. Sorarù G.D., Kleebe H.-J., Ceccato R., Pederiva L. Development of Mullite-SiC Nanocomposites by Pyrolysis of Filled Polymethylsiloxane Gels. Journal of the European Ceramic Society, 2000, vol. 20, no. 14–15, pp. 2509–2517.
  81. Duperrier S., Gervais C., Bernard S. et al. Design of a Series of Preceramic B-Tri(methylamino)borazine-Based Polymers as Fiber Precursors: Architecture, Thermal Beha- vior, and Melt-Spinnability. Macromolecules, 2007, vol. 40, no. 4, pp. 1018–1027.
  82. Kim Y.-W., Park C.B. Processing of Microcellular Preceramics Using Carbon Dioxide. Composites Science and Technology, 2003, vol. 63, no. 16, pp. 2371–2377.
  83. Zhu Y., Huang Z., Dong S. et al. Manufacturing 2D Carbon-Fiber-Reinforced SiC Matrix Composites by Slurry Infiltration and PIP Process. Ceramics International, 2008, vol. 34, no. 5. P. 1201–1205.
  84. Harshe R., Balan C., Riedel R. Amorphous Si(Al)OC Ceramic from Polysiloxanes: Bulk Ceramic Processing, Crystallization Behavior and Applications. Journal of the European Ceramic Society, 2004, vol. 24, no. 12, pp. 3471–3482.
  85. Janakiraman N., Aldinger F. Fabrication and Characterization of Fully Dense Si–C–N Ceramics from a Poly(ureamethylvinyl)Silazane Precursor. Journal of the European Ceramic Society, 2009, vol. 29, no. 1, pp. 163–173.
  86. Shah S.R., Raj R. Mechanical Properties of a Fully Dense Polymer Derived Ceramic Made by a Novel Pressure Casting Process. Acta Materialia, 2002, vol. 50, no. 16, pp. 4093–4103.
  87. Friedel T., Travitzky N., Niebling F. et al. Fabrication of Polymer Derived Ceramic Parts by Selective Laser Curing. Journal of the European Ceramic Society, 2005, vol. 25, no. 2–3, p. 193–197.
  88. Hasegawa Y. Si–C Fiber Prepared from Polycarbosilane Cured without Oxygen. Journal of Inorganic and Organometallic Polymers and Materials, 1992, vol. 2, no. 1, pp. 161–169.
  89. Perale G., Giordano C., Daniele F. et al. A Novel Process for the Manufacture of Ceramic Micro- electrodes for Biomedical Applications. International Journal of Applied Ceramic Technology, 2008, vol. 5, no. 1, pp. 37–43.