Polymeric composite material on the basis of the hybrid metalcarbon reinforcing filler: properties and application

Gunyaeva A.G., Sidorina A.I., Klimenko O.N.
Gunyaeva A.G., Sidorina A.I., Klimenko O.N. Polymeric composite material on the basis of the hybrid metalcarbon reinforcing filler: properties and application // Proceedings of VIAM. 2020. No. 10. DOI: 10.18577/2307-6046-2020-0-10-30-39. URL: https://www.viam-works.ru/en/journal/2020/10/4
Keywords
polymeric composite materials, epoxy polymeric binding, hybrid metalcarbon reinforcing filler, mechanical properties, application.
Abstract

The description of hybrid metalcarbon reinforcing filler is provided, results of determination of its properties are provided. As object for research it is considered CFRP on the basis of hybrid metalcarbon reinforcing filler of the VTkU-2.280M brand and the epoxy molten binding. Experimental samples of prepregs CFRP on the basis of epoxy molten binding and two types of fillers are made: hybrid metalcarbon reinforcing filler of the VTkU-2.280M brand and carbon equal strength filler of the VTkU-2.200 brand, properties of prepregs and CFRP are investigated, the comparative analysis of the received results is carried out. Possible options of application of hybrid metalcarbon reinforcing filler and PKM on its basis are considered.

Reference list
  1. Kablov E.N. Composites: Today and Tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
  2. Sidorina A.I., Gunyaeva A.G. Woven reinforcing carbon fillers for polymer composite materials (review). Khimicheskiye volokna, 2017, no. 2, pp. 20–23.
  3. Perepelkin E.E. Reinforcing fibers and fibrous polymer composites. Saint Petersburg: Nauchnye osnovy i tekhnologii, 2009. 360 p.
  4. Gunyayeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
  5. Kurnosov A.O., Vavilova M.I., Melnikov D.A. Manufacturing technologies of glass fillers and study of effects of finishing material on physical and mechanical properties of fiberglass plastics. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 64–70. DOI: 10.18577/2071-9140-2018-0-1-64-70.
  6. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  7. Mikhailin Yu.A. Fibrous polymer composite materials in technology. Saint Petersburg: Nauchnyye osnovy i tekhnologii, 2015. 720 p.
  8. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7-8. S. 54–58.
  9. Kolpachkov E.D., Kurnosov A.O., Petrova A.P., Raskutin A.E. Hybrid composite materials for aviation based on fibrous fillers (review). Voprosy materialovedeniya, 2020, no. 1 (101), pp. 126–138.
  10. Gunyaeva A.G., Cherfas L.V., Komarova O.A., Kuprienko V.M. Carrying out tests for resistance to lightnings of the experimental and constructive and similar samples executed from carbon plastic, with covering protected from lightnings. Trudy VIAM, 2017, no. 7 (55), paper no. 10. Available at: http://www.viam-works.ru (accessed: July 09, 2020). DOI: 10.18577/2307-6046-2017-0-7-10-10.
  11. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  12. Cherfas L.V., Gunyaeva A.G., Komarova O.A., Antyufeeva N.V. The analysis of nanomodified prepreg shelf life by its reactivity at storage. Trudy VIAM, 2016, no. 1 (37), paper no. 12. Available at: http://www.viam-works.ru (accessed: July 9, 2020). DOI: 10.18577/2307-6046-2016-0-1-99-106. 09.07.2020).
  13. Aleksashin V.M., Alexandrova L.B., Matveeva N.V., Mashinskaya G.P. Application of thermal analysis to control the technological properties of thermosetting prepregs of structural composite materials. Aviatsionnaya promyshlennost, 1997, no. 5-6, pp. 38–43.
  14. Bobovich B.B. Polymeric construction materials (structure, properties, application). Moscow: FORUM: INFRA-M, 2014. 400 p.
  15. Molchanov B.I., Gudimov M.M. Properties of carbon plastics and their application. Aviatsionnaya promyshlennost, 1997, no. 3–4, pp. 58–60.
  16. Tyunina A.V. Composite materials: production, application, market trends. Polimernyye materialy, 2018, no. 2, pp. 27–29.
  17. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.