Determination of sulfur in casting heat-resistant nickel alloys by GD-MS
UDC
669.018.44:669.245
DOI
10.18577/2307-6046-2020-0-1-118-125
Article PDF (Russian)
(625.43 KB)
How to cite
Yakimovitch P.V., Alekseev A.V. Determination of sulfur in casting heat-resistant nickel alloys by GD-MS // Proceedings of VIAM. 2020. No. 1. DOI: 10.18577/2307-6046-2020-0-1-118-125. URL: https://www.viam-works.ru/en/journal/2020/1/11
Keywords
high-resolution mass-spectrometry, GD-MS, nickel alloys, determination of sulfur, determination of harmful impurities, analysis of nickel alloys.
Abstract
In the production of heat-resistant nickel alloy foundries, it is extremely important to control the contents of harmful impurities, especially sulfur. In this work, the determination of sulfur in nickel alloys by high resolution mass spectrometry with a glow discharge, which eliminates spectral interference, is carried out. The selection of analysis conditions is given. The correctness of the results is confirmed by the analysis of certified standard samples of nickel alloys. The sulfur detection limits are 0,000003% by mass. The range of determined concentrations is 0,000016–0,0401% by mass, and the relative standard deviation does not exceed 0,05.
Reference list
- Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
- Kablov E.N., Ospennikova O.G., Svetlov I.L. Highly efficient cooling of GTE hot section blades. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 3–14. DOI: 10.18577/2071-9140-2017-0-2-3-14.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Chabina E.B. Phosphorus and sulfur segregation in model heat resistant Ni-based alloy. Trudy VIAM, 2015, no. 9, paper no. 02. Available at: http://www.viam-works.ru (accessed: July 07, 2019). DOI: 10.18577/2307-6046-2015-0-9-2-2.
- Kablov E.N., Bondarenko Yu.A., Echin A.B. Development of technology of cast superalloys directional solidification with variable controlled temperature gradient. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 24–38. DOI: 10.18577/2071-9140-2017-0-S-24-38.
- Kablov E.N., Ospennikova O.G., Vershkov A.V. Rare metals and rare-earth elements are materials for modern and future high technologies. Aviacionnye materialy i tehnologii, 2013, no. S2, pp. 3–10.
- Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G. The metallurgical fundamentals for high quality maintenance of single crystal heat-resistant nickel alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 55–71. DOI: 10.18577/2071-9140-2017-0-S-55-71.
- Sarioglu C., Stinner C., Blanchere J.R., Birks N., Pettit F.S., Meier G.H. The control of sulfur content in nickel-base, single crystal superalloys and its effect on cyclic oxidation resistance. Superalloys, 1996, pp. 71–80.
- Mc Vay R.V., William P., Meier G.H., Pettit F.S. Oxidation of Low Sulfur Single Crystal Nickel-base Superalloys. Superalloys, 1992, pp. 807–816.
- Mehanik E.A., Min P.G., Gundobin N.V., Rastegaeva G.Yu. Determination of sulfur mass fraction in heat-resistant nickel alloy and steels within the concentration range from 0,0001 to 0,0009% wt. Trudy VIAM, 2014, no. 9, paper no. 12. Available at: http://viam-works.ru (accessed: July 07, 2019). DOI: 10.18577/2307-6046-2014-0-9-12-12.
- State Standard 6689.18–92. Nickel, nickel and copper-nickel alloys. Methods for the determination of sulfur. Moscow: Gosstandart Rossii, 1992. 6 p.
- State Standard 24018.8–91. Nickel-based heat resistant alloys. Methods for the determination of sulfur. Moscow: Gosstandart SSSR, 1991. 6 p.
- ASTM E1019-11. Standard Test Method for Determination of Carbon, Sulfur, Nitrogen and Oxygen in Steel, Iron, Nickel and Cobalt Alloys by Various Combustion and Fusion Techniques. USA, 2011.
- Hu J., Wang H. Determination of Trace Elements in Super Alloy by ICP-MS. Mikrochimica Acta, 2001, vol. 137, pp. 149–155.
- Pupyshev A.A., Epova E.N. Spectral interference of polyatomic ions in inductively coupled plasma mass spectrometry. Analytics and Control, 2001, vol. 5, no. 4, pp. 335–369.
- Clough R., Evans P., Catterick T., Hywel Evans E. Measurements of Sulfur by Multicollector Inductively Coupled Plasma Mass Spectrometry. Analytical Chemistry, 2006, vol. 78, pp. 6126–6132.
- Xing Y., Xiaojia L., Haizhou W. Interference correction in analysis of stainless steel and multi-element determination by glow discharge quadrupole mass spectrometry. International Journal of Mass Spectrometry, 2007, vol. 262, pp. 25–32.
- Jakubowski N., Prohaska T., Rottmann L., Vanhaecke F. Inductively coupled plasma- and glow discharge plasma-sector field mass spectrometry. Journal Analytical Atomic Spectrometry, 2011, vol. 26, pp. 693–726.