Abstract
In this work, a review of the cemented carbides alloys of the WC–Co system is carried out. The cemented carbides of the WC–Co system are mass used in various industries, for example, as tools. The characteristic of materials is given depending on the size of structural components. The features of obtaining starting materials for obtaining a powder mixture are considered. Attention is paid to the features of compaction of powder mixtures and their subsequent sintering. The main problems arising in the preparation of fine-grained hard alloys are considered.
Reference list
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N., Svetlov I.L., Neiman A.V., Min P.G., Karachevtsev F.N., Karpov M.I. High temperature composites based on the Nb – Si system reinforced with niobium silicides. Inorganic Materials: Applied Research, 2017, vol. 8, no. 4, pp. 609–617.
- Kablov E.N., Bondarenko Yu.A., Echin A.B. Development of technology of cast superalloys directional solidification with variable controlled temperature gradient. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 24–38. DOI: 10.18577/2071-9140-2017-0-S-24-38.
- Ospennikova O.G., Podieiachev V.N., Stoliankov Yu.V. Tugoplavkie splavy dlia novoi tekhniki [Refractory alloys for innovative equipment] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2016. №10. St. 05. Available at: http://www.viam-works.ru (accessed: October 14, 2019). DOI:10.18577/2307-6046-2016-0-10-5-5.
- Batiyenkov R.V., Bolshakova A.N., Efimochkin I.Yu. The problem of low-temperature plasticity of molybdenum and alloys based on it (review). Trudy VIAM, 2018, no. 3 (63), paper no. 02. Available at: http://www.viam-works.ru (accessed: October 14, 2019). DOI: 10.18577/2307-6046-2018-0-3-12-17.
- Batiyenkov R.V., Efimochkin I.Yu., Osin I.V., Khudnev A.A. Investigation of the mechanical properties of powder materials of the Mо–W system obtained by spark plasma sintering. Trudy VIAM, 2019, no. 2 (74), paper no. 07. URL: http://www.viam-works.ru (accessed: October 14, 2019). DOI: 10.18577/2307-6046-2019-0-2-68-76.
- Tretyakov V.I. Ceramic metal alloys. Moscow: Metallurgizdat, 1962. 609 p.
- Kiffer R., Benezovsky F. Hard alloys. Per. with Germ. Moscow: Metallurgy, 1971.3 92 p.
- García J., Ciprés V.C., Blomqvist A., Kaplan B. Cemented carbide microstructures: a review. International Journal of Refractory Metals & Hard Materials, 2019, vol. 80, pp. 40–68.
- Kramer G.S. The strength of hard alloys. Moscow: Metallurgy, 1971. 24 p.
- Falkovsky V.A., Borovsky V.G. Hard alloys based on tungsten carbide with a nanogranular and ultrathin structure. Tsvetnyye metally, 2010, no. 5, pp. 106–112.
- Kirsanov S.V. Modern problems of instrumental support of engineering industries. Available at: portal.tpu.ru/SHARED/k/KIRSSANOV/met_work/Tab2/Tab2/Sovrprobl.pdf (accessed: October 1, 2019).
- Panov V.S., Chuvilin A.M., Falkovsky V.A. Technology and properties of sintered hard alloys and products from them. Moscow: MISIS, 2004. 446 p.
- Gusev A., Kurlov A. Hard alloys today and tomorrow. Metals of Eurasia, 2005, no. 2, pp. 42–45.
- Falkovsky V.A., Klyachko L.N. Hard alloys. Moscow: Ruda i metally, 2005. 416 p.
- Falkovsky V.A. Innovations in technology of hard alloys: nano- and ultrafine structures: textbook. M: CPI MGATKhT, 2008. 69 p.
- Falkovsky V.A., Falkovsky F.I., Panov V.S. Nano- and ultrafine hard alloys. Tsvetnyye metally, 2007, no. 10, pp. 85–91.
- Zlobin G.P. Shaping of products from hard alloy powders. Moscow: Metallurgy, 1980. 224 p.