Operability of glued joints on epoxy film adhesives at simultaneous influence of loadings and climatic factors

Petrova A.P., Lukina N.F., Isaev A.Yu.
Petrova A.P., Lukina N.F., Isaev A.Yu. Operability of glued joints on epoxy film adhesives at simultaneous influence of loadings and climatic factors // Proceedings of VIAM. 2019. No. 9. DOI: 10.18577/2307-6046-2019-0-9-57-63. URL: https://www.viam-works.ru/en/journal/2019/9/6
Keywords
tape adhesive, epoxy adhesive, ageing, environmental resistance, the level of loading, the strength of adhesive joints
Abstract

Reviewed the performance of adhesive joints made of epoxy film adhesives VK-31, VK-41 and MC-51, while the impact of conditions of warm humid climate of Black sea coast and loads of 0.2–0.5 of the original strength of the adhesive joints. It is shown that the level of remaining strength after exposure to the above conditions affects not only the initial strength of the adhesive joints, but also the temperature at which the curing of the adhesive. Adhesive bonding for all three adhesives showed a high level of retained strength after exposure to climatic conditions of warm moist climate of Black sea coast and loads.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Kablov E.N. Kontrol' kachestva materialov – garantiya bezopasnosti ekspluatatsii aviatsionnoy tekhniki [Quality control of materials - a guarantee of the safety of the operation of aircraft] // Aviacionnyye materialy i tehnologii. 2001. №1. S. 3–8.
  4. Sorokin A.E., Bejder E.Ya., Perfilova D.N. Vliyanie klimaticheskih faktorov na svojstva ugleplastika na polifenilensulfidnom svyazuyushhem [Effect of climatic factors on properties of carbon fiber reinforced plastic based on polyphenylenesulfide resin] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №1. St. 10. Available at: http://www.viam-works.ru (accessed: Augusta 12, 2019). DOI: 10.18577/2307-6046-2015-0-1-10-10.
  5. Laptev A.B., Barbotko S.L., Nikolaev E.V. Osnovnye napravleniya issledovanij sokhranyaemosti svojstv materialov pod vozdejstviem klimaticheskikh i ekspluatatsionnykh faktorov [The main research areas of the persistence properties of materials under the influence of climatic and operational factors] // Aviacionnye materialy i tehnologii. 2017. №S. S. 547–561. DOI: 10.18577/2071-9140-2017-0-S-547-561.
  6. Petrova A.P., Lukina N.F., Sharova I.A. Otsenka prochnosti kleyevykh soyedineniy, vypolnennykh epoksidnymi kleyami, pri vozdeystvii razlichnykh faktorov [Strength assessment of adhesive joints made with epoxy adhesives under the influence of various factors] // Vse materialy. Entsiklopedicheskiy spravochnik. 2013. №8. S. 28–34.
  7. Sorokin A.E., Bejder E.Ya., Izotova T.F., Nikolaev E.V., Shvedkova A.K. Issledovanie svojstv ugleplastika na polifenilensulfidnom svyazuyushhem posle uskorennyh i naturnyh klimaticheskih ispytanij [Investigation of carbon fiber reinforced plastic on polyphenylenesulfide resin after accelerated and natural climatic test] // Aviacionnye materialy i tehnologii. 2016. №3 (42). S. 66–72. DOI: 10.18577/2071-9140-2016-0-3-66-72.
  8. Kochergin Yu.S., Grigorenko T.I. Dinamicheskiye mekhanicheskiye svoystva epoksidnykh kleyevykh kompozitsiy, napolnennykh molotym karbonatom kaltsiya [Dynamic mechanical properties of epoxy adhesive compositions filled with ground calcium carbonate] // Klei. Germetiki. Tekhnologii. 2018. №2. S. 35–44.
  9. Lukina N.F., Petrova A.P., Muhametov R.R., Kogtjonkov A.S. Novye razrabotki v oblasti kleyashhih materialov aviacionnogo naznacheniya [New developments in the field of adhesive aviation materials] // Aviacionnye materialy i tehnologii. 2017. №S. S. 452–459. DOI: 10.18577/2071-9140-2017-0-S-452-459.
  10. Dementyeva L.A., Petrova A.P., Lukina N.F. Primeneniye i naznacheniye epoksidnogo plenochnogo kleya VK-31 [Application and purpose of epoxy film adhesive VK-31] // Vse materialy. Entsiklopedicheskiy spravochnik. 2015. №1. S. 25–29.
  11. Dementeva L.A., Bocharova L.I., Lukina N.F., Petrova A.P. Vysokoprochnyye plenochnyye klei VK-51 i VK-51A [High-strength film adhesives VK-51 and VK-51A] // Klei. Germetiki. Tekhnologii. 2015. №4. S. 17–19.
  12. Lukina N.F., Dementeva L.A., Petrova A.P., Serezhenkov A.A. Konstrukcionnye i termostojkie klei [Constructional and heat-resistant glues] // Aviacionnye materialy i tehnologii. 2012. №S. S. 328–335.
  13. Kablov E.N., Chursova L.V., Lukina N.F., Kutsevich K.E., Rubtsova E.V., Petrova A.P. Issledovaniye epoksidno-polisulfonovykh polimernykh sistem kak osnovy vysokoprochnykh kleyev aviatsionnogo naznacheniya [The study of epoxy-polysulfone polymer systems as the basis of high-strength adhesives for aviation purposes] // Klei. Germetiki. Tekhnologii. 2017. №3. S. 7–12.
  14. Sharova I.A. Epoksidnyye klei kholodnogo otverzhdeniya dlya skleivaniya i remonta detaley aviatsionnoy tekhniki: avtoref. diss. … kand. tekhn. nauk [Cold cured epoxy adhesives for gluing and repairing aircraft parts: thesis abstract, Cand. Sc. (Tech.)]. M.: VIAM, 2015. 26 s.
  15. Tyumeneva T.Yu., Lukina N.F. Razrabotki v oblasti elastomernykh kleyev aviatsionnogo naznacheniya [Development in the field of elastomeric adhesives for aviation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №8 (44). St. 9. Available at: http://viam-works.ru (accessed: August 12, 2019). DOI: 10.18577/2307-6046-2016-0-8-9-9.
  16. Sytov V.A., Verstakov A.E., Voronin A.E., Sytov V.V. Sovremennyye sinteticheskiye klei na osnove epoksikauchukovykh kompozitsiy [Modern synthetic adhesives based on epoxy rubber compositions] // Klei. Germetiki. Tekhnologii. 2012. №9. S. 6–9.
  17. Sytov V.A., Sytov V.V., Vettegren V.I. Temperaturnaya zavisimost prochnosti kleyevykh soyedineniy stali na osnove epoksikauchukovykh kleyev [Temperature dependence of the strength of adhesive joints of steel based on epoxy rubber adhesives] // Tez. dokl. Mezhdunar. nauch.-tekhnich. konf. «Sovremennyye dostizheniya v oblasti kleyev i germetikov. Materialy, syre, tekhnologii» (Dzerzhinsk, 17–19 sent. 2013 g.). Dzerzhinsk, 2013. S. 50–52.
  18. Lukina N.F., Dementeva L.A., Petrova A.P., Anihovskaya L.I. Kleyashhie materialy v konstrukcii lopastej vertoletov [Gluing materials in the design of blades of helicopters] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №7. St. 07. Available at: http://www.viam-works.ru (accessed: : August 12, 2019). DOI: 10.18577/2307-6046-2016-0-7-7-7.
  19. Konoplin A.Yu., Nelyub V.A. Prochnost kleyevykh soyedineniy, izgotovlennykh pri otritsatelnykh znacheniyakh temperatur [Strength of adhesive joints made at negative temperatures] // Klei. Germetiki. Tekhnologii. 2018. №9. S. 20–23.
  20. Tkachuk A.I., Gurevich YA.M., Guseva M.A., Mishurov K.S. Tekhnologicheskiye i ekspluatatsionnyye kharakteristiki i oblasti primeneniya epoksidnogo svyazuyushchego VSE-1212, pererabatyvayemogo po prepregovoy tekhnologii [Technological and operational characteristics and applications of the epoxy binder VSE-1212, processed by prepreg technology] // Klei. Germetiki. Tekhnologii. 2018. №4. S. 29–34.
  21. Nelyub V.A. Otsenka adgezionnoy prochnosti metodom pull-out v sisteme svyazuyushcheye–elementarnaya nit v zavisimosti ot tipa obrabotki niti [Evaluation of adhesive strength by the pull-out method in a binder – filament system depending on the type of processing of the thread] // Klei. Germetiki. Tekhnologii. 2018. №3. S. 28–32.
  22. Tkachuk A.I., Terekhov I.V., Kudryavtseva A.N., Grigoreva K.N. Ispolzovaniye reologicheskikh metodov issledovaniya pri otverzhdenii epoksidnykh svyazuyushchikh [The use of rheological research methods in the curing of epoxy binders] // Klei. Germetiki. Tekhnologii. 2018. №2. S. 15–20.
  23. Tsverava V.G., Rusin M.Yu., Nepovinnykh V.I., Khimitsayev A.S. Analiz vliyaniya uskorennogo klimaticheskogo stareniya na prochnost kleyevykh soyedineniy [Analysis of the effect of accelerated climatic aging on the strength of adhesive joints] // Klei. Germetiki. Tekhnologii. 2018. №8. S. 28–31.